Magnesium-Based Alloys Used in Orthopedic Surgery
Open accessThe DOI matches its Crossref record; 100 of the 100 references it cites were found in a registry or an index.
Abstract
Magnesium (Mg)-based alloys have become an important category of materials that is attracting more and more attention due to their high potential use as orthopedic temporary implants. These alloys are a viable alternative to nondegradable metals implants in orthopedics. In this paper, a detailed overview covering alloy development and manufacturing techniques is described. Further, important attributes for Mg-based alloys involved in orthopedic implants fabrication, physiological and toxicological effects of each alloying element, mechanical properties, osteogenesis, and angiogenesis of Mg are presented. A section detailing the main biocompatible Mg-based alloys, with examples of mechanical properties, degradation behavior, and cytotoxicity tests related to in vitro experiments, is also provided. Special attention is given to animal testing, and the clinical translation is also reviewed, focusing on the main clinical cases that were conducted under human use approval.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Magnesium and its alloys as orthopedic biomaterials: A review
Staiger, M. P., Pietak, A. M., Huadmai, J., & Dias, G. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2005.10.003 · Cited by 4,452 · cited 2×
“Magnesium can be found in the human bone [16], ligaments and tissues [49], and along with other substances, in body fluids [50].”
BackgroundBiomaterials & scaffolds for tissue engineering
O'Brien, F. J. (2011) · Materials Today · doi:10.1016/s1369-7021(11)70058-x · Cited by 3,437 · cited 1×
“Relatively recent, some researchers proposed Mg alloys as a raw material for bone engineering scaffolds production [9,61,127,128].”
BackgroundZheng, Y. F., Gu, X. N., & Witte, F. (2014) · Materials Science and Engineering: R: Reports · doi:10.1016/j.mser.2014.01.001 · Cited by 2,436 · cited 2×
“Biodegradable metals are a new paradigm for orthopedic implants because they promote bone formation [46] and sustain the bone healing and remodeling process through a gradual load transfer between implant and tissues [47].”
BackgroundIn vivo corrosion of four magnesium alloys and the associated bone response
Witte, F., Kaese, V., Haferkamp, H., Switzer, E., Meyer-Lindenberg, A., Wirth, C. J., & Windhagen, H. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2004.09.049 · Cited by 2,395
Biomedical applications of biodegradable polymers
Ulery, B. D., Nair, L. S., & Laurencin, C. T. (2011) · Journal of Polymer Science Part B: Polymer Physics · doi:10.1002/polb.22259 · Cited by 2,206 · cited 1×
“These types of materials are not adequate for the osteointegration process and can generate inflammatory responses from the host body, thus creating the need for searching different biodegradable metals [14,15].”
BackgroundDegradable biomaterials based on magnesium corrosion
Witte, F., Hort, N., Vogt, C., Cohen, S., Kainer, K. U., Willumeit, R., & Feyerabend, F. (2008) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2009.04.001 · Cited by 1,820 · cited 2×
“Physiological and toxicological characteristics of the impurities in Mg-based alloys [59].”
BackgroundThe development of binary Mg–Ca alloys for use as biodegradable materials within bone
Li, Z., Gu, X., Lou, S., & Zheng, Y. (2008) · Biomaterials · doi:10.1016/j.biomaterials.2007.12.021 · Cited by 1,593
In vitro corrosion and biocompatibility of binary magnesium alloys
Gu, X., Zheng, Y., Cheng, Y., Zhong, S., & Xi, T. (2009) · Biomaterials · doi:10.1016/j.biomaterials.2008.10.021 · Cited by 1,343 · cited 1×
“performed cytotoxicity tests on different binary Mg-based alloys that also include analysis on Mg-Y alloys and concluded that Y exhibits some toxic effects on different cell lines [83].”
BackgroundResearch on an Mg–Zn alloy as a degradable biomaterial
Zhang, S., Zhang, X., Zhao, C., Li, J., Song, Y., Xie, C., Tao, H., Zhang, Y., He, Y., Jiang, Y., et al. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.06.028 · Cited by 1,336 · cited 3×
“In the case of the Mg-Zn binary alloy, it was concluded that cell morphologies in different extracts are normal and healthy, by comparing them with the negative control [57].”
BackgroundGu, D., Hagedorn, Y.-C., Meiners, W., Meng, G., Batista, R. J. S., Wissenbach, K., & Poprawe, R. (2012) · Acta Materialia · doi:10.1016/j.actamat.2012.04.006 · Cited by 1,089 · cited 1×
“By this technology, the final product is printed layer-by-layer, based on computer-aided tomography [39,40].”
MethodAgarwal, S., Curtin, J., Duffy, B., & Jaiswal, S. (2016) · Materials Science and Engineering: C · doi:10.1016/j.msec.2016.06.020 · Cited by 955 · cited 1×
“[79] studied the angiogenesis that includes new blood vessel formation, on fetal mouse metatarsal assay.”
BackgroundZhao, D., Witte, F., Lu, F., Wang, J., Li, J., & Qin, L. (2017) · Biomaterials · doi:10.1016/j.biomaterials.2016.10.017 · Cited by 945 · cited 2×
“Magnesium can be found in the human bone [16], ligaments and tissues [49], and along with other substances, in body fluids [50].”
BackgroundMagnesium: nutrition and metabolism
Vormann, J. (2003) · Molecular Aspects of Medicine · doi:10.1016/s0098-2997(02)00089-4 · Cited by 671 · cited 1×
“Magnesium can be found in the human bone [16], ligaments and tissues [49], and along with other substances, in body fluids [50].”
BackgroundYoshizawa, S., Brown, A., Barchowsky, A., & Sfeir, C. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2014.02.002 · Cited by 577 · cited 1×
“7 macrophages, and primary human mesenchymal stem cells [56].”
BackgroundWindhagen, H., Radtke, K., Weizbauer, A., Diekmann, J., Noll, Y., Kreimeyer, U., Schavan, R., Stukenborg-Colsman, C., & Waizy, H. (2013) · BioMedical Engineering OnLine · doi:10.1186/1475-925x-12-62 · Cited by 521
The Williams Dictionary of Biomaterials
Williams, D. F. (1999) · Liverpool University Press eBooks · doi:10.5949/upo9781846314438 · Cited by 517
Wang, J., Witte, F., Xi, T., Zheng, Y., Yang, K., Yang, Y., Zhao, D., Meng, J., Li, Y., Li, W., et al. (2015) · Acta Biomaterialia · doi:10.1016/j.actbio.2015.04.011 · Cited by 493 · cited 3×
“It was underlined that the magnesium ions could have a detrimental effect on implant surrounding cells and tissues, and they may cause a systemic toxicity if they are present in a high amount [55].”
BackgroundToxicological Evaluations of Rare Earths and Their Health Impacts to Workers: A Literature Review
Rim, K. T., Koo, K. H., & Park, J. S. (2013) · Safety and Health at Work · doi:10.5491/shaw.2013.4.1.12 · Cited by 484 · cited 1×
“In addition, rare earths can cause hepatic toxicity [32].”
BackgroundLong-term clinical study and multiscale analysis of in vivo biodegradation mechanism of Mg alloy
Lee, J.-W., Han, H.-S., Han, K.-J., Park, J., Jeon, H., Ok, M.-R., Seok, H.-K., Ahn, J.-P., Lee, K. E., Lee, D.-H., et al. (2016) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.1518238113 · Cited by 480
Gu, X. N., Xie, X. H., Li, N., Zheng, Y. F., & Qin, L. (2012) · Acta Biomaterialia · doi:10.1016/j.actbio.2012.02.018 · Cited by 478
Mg bone implant: Features, developments and perspectives
Yang, Y., He, C., Dianyu, E., Yang, W., Qi, F., Xie, D., Shen, L., Peng, S., & Shuai, C. (2020) · Materials & Design · doi:10.1016/j.matdes.2019.108259 · Cited by 433 · cited 3×
“for fracture fixture [43], (d) intramedullary nail made from magnesium [43], (e) screw and wire from RESOMET® [154], (f) pin [129], and (g) scaffold [127].”
BackgroundInfluentialCurrent status and outlook on the clinical translation of biodegradable metals
Han, H.-S., Loffredo, S., Jun, I., Edwards, J., Kim, Y.-C., Seok, H.-K., Witte, F., Mantovani, D., & Glyn-Jones, S. (2019) · Materials Today · doi:10.1016/j.mattod.2018.05.018 · Cited by 423 · cited 2×
“In addition, 23 cases of osteonecrosis of femoral head flap fixation were made using pure Mg, and 53 cases of distal radius fracture fixation based on RESOMETTM (Mg-Ca alloy) were treated in 2013 [48].”
BackgroundMethodAdditively manufactured biodegradable porous magnesium
Li, Y., Zhou, J., Pavanram, P., Leeflang, M. A., Fockaert, L. I., Pouran, B., Tümer, N., Schröder, K.-U., Mol, J. M. C., Weinans, H., et al. (2018) · Acta Biomaterialia · doi:10.1016/j.actbio.2017.12.008 · Cited by 396 · cited 1×
“This is the most used technique, which helps doctors and engineers to develop custom-made Mg-based implants [41,42].”
MethodElectrodeposition of Ca–P coatings on biodegradable Mg alloy: In vitro biomineralization behavior☆
Song, Y., Zhang, S., Li, J., Zhao, C., & Zhang, X. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.12.020 · Cited by 385 · cited 2×
“One important issue is to point out that the alloying element and metallurgical processing, such as heat treatments and plastic deformation, strongly influence the biocompatibility, the mechanical properties, and the degradation rate, due to the modifications induced in the microstructure of magnesium alloys [76,77].”
BackgroundMethodZhou, H., Liang, B., Jiang, H., Deng, Z., & Yu, K. (2021) · Journal of Magnesium and Alloys · doi:10.1016/j.jma.2021.03.004 · Cited by 377 · cited 11×
“Of the plasma surface modification technologies, the most used are physical vapor deposition, ion implantation, and plasma spraying [61].”
BackgroundMethodInfluentialIn vivo study of magnesium plate and screw degradation and bone fracture healing
Chaya, A., Yoshizawa, S., Verdelis, K., Myers, N., Costello, B. J., Chou, D.-T., Pal, S., Maiti, S., Kumta, P. N., & Sfeir, C. (2015) · Acta Biomaterialia · doi:10.1016/j.actbio.2015.02.010 · Cited by 359 · cited 1×
“[26] observed an important corrosion rate in the case of a Mg plate, which was implanted in a loaded ulna fracture model.”
BackgroundZhao, D., Huang, S., Lu, F., Wang, B., Yang, L., Qin, L., Yang, K., Li, Y., Li, W., Wang, W., et al. (2016) · Biomaterials · doi:10.1016/j.biomaterials.2015.11.038 · Cited by 349 · cited 1×
“A studied pure Mg implant [63] for osteonecrosis of the femoral head proves that bone flap stability was increased, but unfortunately, two patients suffered the collapse of the femoral head, a fact that sustains that pure Mg is not suitable for load-bearing biomedical applications.”
BackgroundNeuropathology of aluminum toxicity in rats (glutamate and GABA impairment)
El-Rahman, S. (2003) · Pharmacological Research · doi:10.1016/s1043-6618(02)00336-5 · Cited by 321 · cited 1×
“Different unwanted reactions are presented, with some studies [30,31] showing that aluminum, as an alloying element (Al), could be linked to neurons and osteoblast decrease in the human body, leading to Alzheimer’s disease or dementia.”
BackgroundMg–Zr–Sr alloys as biodegradable implant materials
Li, Y., Wen, C., Mushahary, D., Sravanthi, R., Harishankar, N., Pande, G., & Hodgson, P. (2012) · Acta Biomaterialia · doi:10.1016/j.actbio.2012.04.028 · Cited by 309 · cited 5×
“The cytotoxicity and osteoinduction capacities of Mg-xZr-ySr were investigated showing, in the case of Mg-1Zr-2Sr and Mg-2Zr-5Sr, that these materials promote initial cell attachment and growth [73].”
BackgroundInfluentialPorous magnesium-based scaffolds for tissue engineering
Yazdimamaghani, M., Razavi, M., Vashaee, D., Moharamzadeh, K., Boccaccini, A. R., & Tayebi, L. (2017) · Materials Science and Engineering: C · doi:10.1016/j.msec.2016.11.027 · Cited by 298
Mei, D., Lamaka, S. V., Lu, X., & Zheludkevich, M. L. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108722 · Cited by 284 · cited 4×
“Meier and Panzica [147] described five cases of patients with acute scaphoid fractures, which were stabilized with Mg-Y-RE-Zr compression screws.”
BackgroundInfluentialMagnesium Implants: Prospects and Challenges
Chakraborty Banerjee, P., Al-Saadi, S., Choudhary, L., Harandi, S. E., & Singh, R. (2019) · Materials · doi:10.3390/ma12010136 · Cited by 280
Handbook of Bioceramics and Biocomposites
(2016) · Springer eBooks · doi:10.1007/978-3-319-12460-5 · Cited by 275
Jamesh, M., Kumar, S., & Sankara Narayanan, T. S. N. (2011) · Corrosion Science · doi:10.1016/j.corsci.2010.10.011 · Cited by 262 · cited 2×
“Different unwanted reactions are presented, with some studies [30,31] showing that aluminum, as an alloying element (Al), could be linked to neurons and osteoblast decrease in the human body, leading to Alzheimer’s disease or dementia.”
BackgroundResultIn vivo evaluation of biodegradable magnesium alloy bone implant in the first 6 months implantation
Zhang, E., Xu, L., Yu, G., Pan, F., & Yang, K. (2009) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.32132 · Cited by 256
Revolutionizing biodegradable metals
Yun, Y., Dong, Z., Lee, N., Liu, Y., Xue, D., Guo, X., Kuhlmann, J., Doepke, A., Halsall, H. B., Heineman, W., et al. (2009) · Materials Today · doi:10.1016/s1369-7021(09)70273-1 · Cited by 252
Antibacterial biodegradable Mg-Ag alloys
Institute for Material Research, H.-Z. G., Tie, D., Feyerabend, F., Müller, W.-D., Schade, R., Liefeith, K., Kainer, K., & Willumeit, R. (2013) · European Cells and Materials · doi:10.22203/ecm.v025a20 · Cited by 250
Cheng, M.-Q., Wahafu, T., Jiang, G.-F., Liu, W., Qiao, Y.-Q., Peng, X.-C., Cheng, T., Zhang, X.-L., He, G., & Liu, X.-Y. (2016) · Scientific Reports · doi:10.1038/srep24134 · Cited by 247
In vitro degradation behavior and cytocompatibility of Mg–Zn–Zr alloys
Huan, Z. G., Leeflang, M. A., Zhou, J., Fratila-Apachitei, L. E., & Duszczyk, J. (2010) · Journal of Materials Science: Materials in Medicine · doi:10.1007/s10856-010-4111-8 · Cited by 234 · cited 1×
“6Zr (ZK60) exhibit good mechanical properties as follows: for ZK60 (YS = 235 MPa, UTS = 315 MPa and elongation rate of 8%), and in the case of ZK30 (YS = 215 MPa, UTS = 300 MPa and elongation rate of 9%) [93,94].”
BackgroundZhang, X., Yuan, G., Mao, L., Niu, J., Fu, P., & Ding, W. (2011) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2011.05.026 · Cited by 228 · cited 1×
“The Mg-RE alloys exhibit a good degradation behavior [74,82].”
BackgroundJin, W., Wu, G., Feng, H., Wang, W., Zhang, X., & Chu, P. K. (2015) · Corrosion Science · doi:10.1016/j.corsci.2015.01.049 · Cited by 211 · cited 1×
“Better mechanical properties were observed after using a combination of Zn or/and Zr with RE elements, which are present in the commercial WE43 alloy [69,80].”
BackgroundLiu, D., Yang, D., Li, X., & Hu, S. (2019) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2018.08.003 · Cited by 191 · cited 1×
“The formation of an intermetallic phase in the as-cast or extruded Mg-RE alloys is due to the high maximum solubility limit of rare earth elements [81].”
BackgroundSekar, P., Narendranath, S., & Desai, V. (2021) · Journal of Magnesium and Alloys · doi:10.1016/j.jma.2020.11.001 · Cited by 176 · cited 8×
“Bioactive glass coating is a proper technology because it is usually used in tissue engineering and exhibits high bioactivity, controllable biodegradability, and good osteoconductivity [62].”
BackgroundInfluentialEffect of magnesium ion on human osteoblast activity
He, L. Y., Zhang, X. M., Liu, B., Tian, Y., & Ma, W. H. (2016) · Brazilian Journal of Medical and Biological Research · doi:10.1590/1414-431x20165257 · Cited by 166 · cited 1×
“Other studies [52] showed that Mg-ions can increase osteoblasts cells viability or have an important role in gap junction intercellular communication (GJIC) between material and osteoblast cells and signal transmission, with all of the investigations showing good biocompatibility of the magnesium implants and a sustai…”
BackgroundPurnama, A., Hermawan, H., Couet, J., & Mantovani, D. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2010.02.027 · Cited by 161 · cited 1×
“372 V, with an increased tendency to corrosion in aqueous media [16,17].”
BackgroundHybrid fracture fixation systems developed for orthopaedic applications: A general review
Li, T. X., Tang, N., Ngai, T., Wu, C. C., Ruan, Y. C., Huang, L., & Qin, L. (2018) · Journal of Orthopaedic Translation · doi:10.1016/j.jot.2018.06.006 · Cited by 154
Magnesium Alloys With Tunable Interfaces as Bone Implant Materials
Rahman, M., Dutta, N. K., & Choudhury, N. R. (2020) · Frontiers in Bioengineering and Biotechnology · doi:10.3389/fbioe.2020.00564 · Cited by 154
Plaaß, C., von Falck, C., Ettinger, S., Sonnow, L., Calderone, F., Weizbauer, A., Reifenrath, J., Claaßen, L., Waizy, H., Daniilidis, K., et al. (2017) · Journal of Orthopaedic Science · doi:10.1016/j.jos.2017.11.005 · Cited by 147
Jin, W., & Chu, P. K.-H. (2017) · Elsevier eBooks · doi:10.1016/b978-0-12-801238-3.10999-7 · Cited by 139
Li, G., Zhang, L., Wang, L., Yuan, G., Dai, K., Jia, P., & Hao, Y. (2017) · Acta Biomaterialia · doi:10.1016/j.actbio.2017.10.033 · Cited by 136 · cited 2×
“Femoral fracture in osteoporotic bone Intramedullary nail Mg-Nd-Zn-Zr (JDBM) integrated with the anti-catabolic drug zoledronic acid (ZA) Rat [23]”
BackgroundAbed, E., & Moreau, R. (2009) · American Journal of Physiology-Cell Physiology · doi:10.1152/ajpcell.00614.2008 · Cited by 131 · cited 1×
“[51] studied and proved that Mg ions are present in the extracellular matrix.”
BackgroundCorrosion studies and microstructure of Mg−Zn−Ca alloys for biomedical applications
Abdel-Gawad, S. A., & Shoeib, M. A. (2018) · Surfaces and Interfaces · doi:10.1016/j.surfin.2018.11.011 · Cited by 131 · cited 1×
“5 ± 1 [70] Mg–Zn -Mn 78 ± 2 175 ± 3 12 68 Hv [71] Mg- 4Zn-0.”
Chen, Y., Dou, J., Yu, H., & Chen, C. (2019) · Journal of Biomaterials Applications · doi:10.1177/0885328219834656 · Cited by 128 · cited 1×
“The Al and Zn percent in AZ31 alloy is considered to be in the safe range for in vivo applications (1% for Zn and 2–3% for Al), and it does not exhibit toxic behavior inside the human body [57,58], but Witte, Antoniac, and other authors recommend avoiding magnesium alloys that contain”
BackgroundAlkalization is responsible for antibacterial effects of corroding magnesium
Rahim, M. I., Eifler, R., Rais, B., & Mueller, P. P. (2015) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.35503 · Cited by 111 · cited 1×
“A great advantage of Mg consists of the fact that its degradation products are not toxic and they even promote new bone formation [18,19].”
BackgroundHuang, S., Wang, B., Zhang, X., Lu, F., Wang, Z., Tian, S., Li, D., Yang, J., Cao, F., Cheng, L., et al. (2020) · Biomaterials · doi:10.1016/j.biomaterials.2020.119829 · Cited by 106
Intramedullary Mg2Ag nails augment callus formation during fracture healing in mice
Jähn, K., Saito, H., Taipaleenmäki, H., Gasser, A. S., Hort, N., Feyerabend, F., Schlüter, H., Rueger, J. M., Lehmann, W., Willumeit‐Römer, R., et al. (2016) · Acta Biomaterialia · doi:10.1016/j.actbio.2016.03.041 · Cited by 105
Li, T., Sheng, Y., Huang, L., Chow, D. H. K., Chau, W. H., Tang, N., Ngai, T., Wu, C. C., Lü, J., & Qin, L. (2018) · Biomaterials · doi:10.1016/j.biomaterials.2018.07.018 · Cited by 102
Zhao, C., Pan, F., Zhang, L., Pan, H., Song, K., & Tang, A. (2016) · Materials Science and Engineering C · doi:10.1016/j.msec.2016.04.012 · Cited by 101
Kavyani, M., Ebrahimi, G. R., Ezatpour, H. R., & Jahazi, M. (2021) · Journal of Magnesium and Alloys · doi:10.1016/j.jma.2020.11.013 · Cited by 98 · cited 1×
“Calcium is considered to be a grain refining element [87], but it must be limited to 0.”
BackgroundMay, H., Katı, Y. A., Gümüşsuyu, G., Emre, T. Y., Unal, M., & Köse, Ö. (2020) · Journal of Orthopaedics and Traumatology · doi:10.1186/s10195-020-00547-7 · Cited by 95
Mohamed, A., Abdel-Aziz, A. M., & Breitinger, H. (2019) · Journal of Magnesium and Alloys · doi:10.1016/j.jma.2019.02.007 · Cited by 92
Synthesis and characterization of Mg‐Ca‐Sr alloys for biodegradable orthopedic implant applications
Berglund, I. S., Brar, H. S., Dolgova, N. V., Acharya, A. P., Keselowsky, B. G., Sarntinoranont, M., & Manuel, M. V. (2012) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.32721 · Cited by 92
Leonhardt, H., Franke, A., McLeod, N. M. H., Lauer, G., & Nowak, A. (2017) · British Journal of Oral and Maxillofacial Surgery · doi:10.1016/j.bjoms.2017.04.007 · Cited by 82
Holweg, P. L., Berger, L., Cihova, M., Donohue, N., Clement, B., Schwarze, U. Y., Sommer, N. G., Hohenberger, G. M., van den Beucken, J. J. J. P., Seibert, F. J., et al. (2020) · Acta Biomaterialia · doi:10.1016/j.actbio.2020.06.013 · Cited by 81 · cited 1×
“7 mm diameter screws Mg-Y-RE-Zr (MAGNEZIX®, Syntellix AG) Human female 48 years old (2020) [24] Osteotomized bone in sheep screw Mg-Zn-Ca (ZX00) Sheep [25]”
BackgroundKöse, Ö., Turan, A., Ünal, M., Acar, B., & Güler, F. (2018) · Archives of Orthopaedic and Trauma Surgery · doi:10.1007/s00402-018-2941-x · Cited by 80
Additive manufacturing of Mg alloys for biomedical applications: Current status and challenges
Raja, A., Gupta, P., Santra, T. S., & Jayaganthan, R. (2021) · Current Opinion in Biomedical Engineering · doi:10.1016/j.cobme.2021.100276 · Cited by 77 · cited 1×
“By this technology, the final product is printed layer-by-layer, based on computer-aided tomography [39,40].”
MethodChen, H., Yuan, B., Zhao, R., Yang, X., Xiao, Z., Antoniac, A., Biță, A.-I., Zhu, X., Antoniac, I., & Zhang, X. (2021) · Journal of Magnesium and Alloys · doi:10.1016/j.jma.2021.05.013 · Cited by 76
Self-citationIn vivo assessment of biodegradable magnesium alloy ureteral stents in a pig model
Tie, D., Liu, H. H., Guan, R., Holt-Torres, P., Liu, Y., Wang, Y., & Hort, N. (2020) · Acta Biomaterialia · doi:10.1016/j.actbio.2020.09.023 · Cited by 76 · cited 2×
“Other types of surface modifications are the chemical ones that include chemical passivation, reaction with ionic liquids, self-assembled monolayers, chemical conversion coating (phosphate or fluoride conversion coatings on Mg), and sol-gel coating technology (titania, hydroxyapatite, bioactive glass, and polymer coat…”
BackgroundKlauser, H. (2018) · Foot and Ankle Surgery · doi:10.1016/j.fas.2018.02.005 · Cited by 75
Biomaterials and their applications in medicine
Kulinets, I. (2014) · Elsevier eBooks · doi:10.1533/9780857099204.1 · Cited by 74 · cited 1×
“Biomaterials are used in different medical applications and are placed in direct or indirect contact with biological environments [1].”
BackgroundAntoniac, I., Miculescu, F., Cotruț, C. M., Ficai, A., Rau, J. V., Grosu, E., Antoniac, A., Tecu, C., & Cristescu, I. (2020) · Materials · doi:10.3390/ma13020263 · Cited by 73 · cited 1×
“Mg-Zn binary-based alloys have an α-Mg matrix and MgZn precipitates [84].”
BackgroundSelf-citationOsteosynthesis of a cranio-osteoplasty with a biodegradable magnesium plate system in miniature pigs
Naujokat, H., Seitz, J., Açil, Y., Damm, T., Möller, I., Gülses, A., & Wiltfang, J. (2017) · Acta Biomaterialia · doi:10.1016/j.actbio.2017.08.031 · Cited by 68 · cited 3×
“[20] analyzed the same type of alloy (WE43) in four-hole plates (1 mm thickness, 22 mm length) and in cortical bone screws (2 mm diameter, 5 mm length) for cranial fractures of minipig animal models.”
BackgroundMethodInfluentialFracture Healing Using Degradable Magnesium Fixation Plates and Screws
Chaya, A. E., Yoshizawa, S., Verdelis, K., Noorani, S., Costello, B. J., & Sfeir, C. S. (2014) · Journal of Oral and Maxillofacial Surgery · doi:10.1016/j.joms.2014.09.007 · Cited by 67
Acar, B., Köse, Ö., Turan, A., Unal, M., Katı, Y. A., & Güler, F. (2018) · BioMed Research International · doi:10.1155/2018/5242806 · Cited by 65
Marukawa, E., Tamai, M., Takahashi, Y., Hatakeyama, I., Satô, M., Higuchi, Y., Kakidachi, H., Taniguchi, H., Sakamoto, T., Honda, J., et al. (2015) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.33470 · Cited by 64
Ding, Y., Lin, J., Wen, C., Zhang, D., & Li, Y. (2016) · Scientific Reports · doi:10.1038/srep31990 · Cited by 63
Yu, X., Zhao, D., Huang, S., Wang, B., Zhang, X., Wang, W., & Wei, X. (2015) · BMC Musculoskeletal Disorders · doi:10.1186/s12891-015-0790-0 · Cited by 62
Antoniac, I. V., Antoniac, A., Vasile, E., Tecu, C., Fosca, M., Yankova, V. G., & Rau, J. V. (2021) · Bioactive Materials · doi:10.1016/j.bioactmat.2021.02.030 · Cited by 59
Self-citationPolymeric nanobiocomposites for biomedical applications
Mozumder, M. S., Mairpady, A., & Mourad, A. I. (2016) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.33633 · Cited by 58 · cited 1×
“These types of materials are not adequate for the osteointegration process and can generate inflammatory responses from the host body, thus creating the need for searching different biodegradable metals [14,15].”
BackgroundNeacsu, P., Staras, A., Voicu, Ș. I., Ionaşcu, I., Soare, T., Uzun, S., Cojocaru, V. D., Pandele, A. M., Croitoru, S. M., Miculescu, F., et al. (2017) · Materials · doi:10.3390/ma10070686 · Cited by 57
Sun, Y., Helmholz, H., & Willumeit‐Römer, R. (2020) · Journal of Magnesium and Alloys · doi:10.1016/j.jma.2020.09.011 · Cited by 53 · cited 3×
“Other studies [52] showed that Mg-ions can increase osteoblasts cells viability or have an important role in gap junction intercellular communication (GJIC) between material and osteoblast cells and signal transmission, with all of the investigations showing good biocompatibility of the magnesium implants and a sustai…”
BackgroundResultKong, X., Wang, L., Li, G., Qu, X., Niu, J., Tang, T., Dai, K., Yuan, G., & Hao, Y. (2017) · Materials Science and Engineering C · doi:10.1016/j.msec.2017.12.014 · Cited by 53
Degradation behaviour of magnesium-rare earth biomedical alloys
Trivedi, P., Nune, K. C., & Misra, R. D. K. (2016) · Materials Technology · doi:10.1080/10667857.2016.1213550 · Cited by 52 · cited 1×
“The Mg-RE alloys exhibit a good degradation behavior [74,82].”
BackgroundChoo, J. T., Lai, A., Tang, C. Q. Y., & Thevendran, G. (2018) · Foot and Ankle Surgery · doi:10.1016/j.fas.2018.09.001 · Cited by 50
Telang, V. S., Pemmada, R., Thomas, V., Ramakrishna, S., Tandon, P., & Nanda, H. S. (2021) · Current Opinion in Biomedical Engineering · doi:10.1016/j.cobme.2021.100264 · Cited by 50
Antoniac, I., Filipescu, M., Barbaro, K., Bonciu, A. F., Birjega, R., Cotruț, C. M., Galvano, E., Fosca, M., Fadeeva, I. V., Vadalà, G., et al. (2020) · Advanced Materials Interfaces · doi:10.1002/admi.202000531 · Cited by 48 · cited 1×
“Casting is one of the easiest and cheapest technology, but some variations of this method are common: squeeze casting, high pressure gravity casting, sand casting, and stir casting [37].”
BackgroundSelf-citationIntercondylar eminence fracture treated by resorbable magnesium screws osteosynthesis: A case series
Gigante, A. P., Setaro, N., Rotini, M., Finzi, S. S., & Marinelli, M. (2018) · Injury · doi:10.1016/j.injury.2018.09.055 · Cited by 47
Meier, R., & Panzica, M. (2017) · Handchirurgie · Mikrochirurgie · Plastische Chirurgie · doi:10.1055/s-0042-121416 · Cited by 44
Biodegradable magnesium pins enhanced the healing of transverse patellar fracture in rabbits
Chow, D. H. K., Wang, J., Wan, P., Zheng, L., Ong, M. T., Huang, L., Tong, W., Tan, L., Yang, K., & Qin, L. (2021) · Bioactive Materials · doi:10.1016/j.bioactmat.2021.03.044 · Cited by 42
Könneker, S., Krockenberger, K., Pieh, C., von Falck, C., Brandewiede, B., Vogt, P. M., Kirschner, M. H., & Ziegler, A. (2019) · BMC Musculoskeletal Disorders · doi:10.1186/s12891-019-2723-9 · Cited by 36 · cited 1×
“Scaphoid fracture Magnesium-based headless Herbert screw Mg-Y-RE-Zr/WE43 Human (190 patients) [27]”
BackgroundChou, D., Hong, D., Öksüz, S., Schweizer, R., Roy, A., Lee, B., Shridhar, P., Gorantla, V. S., & Kumta, P. N. (2019) · Journal of Biomaterials Applications · doi:10.1177/0885328219825568 · Cited by 34
A Case of Implant Failure in Partial Wrist Fusion Applying Magnesium-Based Headless Bone Screws
Wichelhaus, A., Emmerich, J., & Mittlmeier, T. (2016) · Case Reports in Orthopedics · doi:10.1155/2016/7049130 · Cited by 34
Characteristics of the Mg-Zn-Ca-Gd Alloy after Mechanical Alloying
Lesz, S., Hrapkowicz, B., Karolus, M., & Gołombek, K. (2021) · Materials · doi:10.3390/ma14010226 · Cited by 31
Chen, L., Lin, Z., Wang, M., Huang, W., Jin, K., Zhao, D., Yin, Q., & Zhang, Y. (2019) · Journal of Orthopaedic Translation · doi:10.1016/j.jot.2019.01.004 · Cited by 31
Bohlen, J., Meyer, S., Wiese, B., Luthringer-Feyerabend, B., Willumeit‐Römer, R., & Letzig, D. (2020) · Materials · doi:10.3390/ma13020391 · Cited by 30
Magnesium Bioabsorbable Screw Fixation of Radial Styloid Fractures: Case Report
Turan, A., Katı, Y. A., Acar, B., & Köse, Ö. (2019) · Journal of Wrist Surgery · doi:10.1055/s-0039-1685489 · Cited by 27
Are Magnesium Screws Proper for Mandibular Condyle Head Osteosynthesis?
Kozakiewicz, M. (2020) · Materials · doi:10.3390/ma13112641 · Cited by 16
Biodegradable magnesium screws in elbow fracture fixation: Clinical case series
Lam, W.-H., Tso, C.-Y., Tang, N., Cheung, W., Qin, L., & Wong, R. M. Y. (2021) · Journal of Orthopaedics Trauma and Rehabilitation · doi:10.1177/2210491720986983 · Cited by 10 · cited 1×
“7 mm diameter screws Mg-Y-RE-Zr (MAGNEZIX®, Syntellix AG) Human female 48 years old (2020) [24] Osteotomized bone in sheep screw Mg-Zn-Ca (ZX00) Sheep [25]”
BackgroundShiwaku, K., Suzuki, T., Matsumura, T., Takashima, H., Otsubo, H., & Yamashita, T. (2020) · The Knee · doi:10.1016/j.knee.2020.06.012 · Cited by 8
Regenerative Engineering in the Field of Orthopedic Surgery
Laurencin, C. T., & Badon, M. A. (2019) · Elsevier eBooks · doi:10.1016/b978-0-323-55140-3.00019-9 · Cited by 2
Cited by
Review on magnesium and magnesium-based alloys as biomaterials for bone immobilization
He, M., Chen, L., Yin, M., Xu, S., & Liang, Z. (2023) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2023.02.037 · Cited by 195
Metadata
- Authors
- Antoniac, I., Miculescu, M., Mănescu (Păltânea), V., Stere, A., Quan, P. H., Păltânea, G., Robu, A., & Earar, K.
- Venue
- Materials
- Publisher
- MDPI AG
- Published
- 2022-02-02
- Volume
- 15
- Issue
- 3
- Pages
- 1148
- ISSN
- 1996-1944 (ISSN-L)
- OpenAlex
- W4210714060
- Cited by
- 163
- References
- 100
- FWCI
- 6.92
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.