As rapid progress has been achieved in emerging thin film solar cell technology, organic–inorganic hybrid perovskite solar cells (PVSCs) have aroused many concerns with several desired properties for photovoltaic applications, including large absorption coefficients, excellent carrier mobility, long charge carrier diffusion lengths, low‐cost, and unbelievable progress. Power conversion efficiencies increased from 3.8% in 2009 up to the current world record of 22.1%. However, poor long‐term stability of PVSCs limits the future commercial application. Here, the degradation mechanisms for unstable perovskite materials and their corresponding solar cells are discussed. The strategies for enhancing the stability of perovskite materials and PVSCs are also summarized. This review is expected to provide helpful insights for further enhancing the stability of perovskite materials and PVSCs in this exciting field.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1002/advs.201700387

Cites

199 of 199 references verified0 citation errors · 0 not checkable

Statistics

Figures

Figure 1 PVSCs power conversion efficiency chart from 2008 to 2017. The PCE highlighted with red circle is certified by an independent accredited test center.
Figure 1 PVSCs power conversion efficiency chart from 2008 to 2017. The PCE highlighted with red circle is certified by an independent accredited test center.CC BY · PubMed Central
Figure 2 a) Crystal structures of the 3D perovskite MAPbI3 and the 2D perovskite (PEA)2(MA)2[Pb3I10]. b) PXRD patterns of (PEA)2(MA)2[Pb3I10] films (1), MAPbI3 formed from PbI2 (2a), and MAPbI3 formed from PbCl2 (2b), which were exposed to 52% relative humidity. Annealing of films of 2a (15 min) and 2b (80 min) were conducted at 100 °C prior to humidity exposure. Reproduced with permission.60 Copyright 2014, Wiley‐VCH.
Figure 2 a) Crystal structures of the 3D perovskite MAPbI3 and the 2D perovskite (PEA)2(MA)2[Pb3I10]. b) PXRD patterns of (PEA)2(MA)2[Pb3I10] films (1), MAPbI3 formed from PbI2 (2a), and MAPbI3 formed from PbCl2 (2b), which were exposed to 52% relative humidity. Annealing of films of 2a (15 min) and 2b (80 min) were conducted at 100 °C prior to humidity exposure. Reproduced with permission.60 Copyright 2014, Wiley‐VCH.CC BY · PubMed Central
Figure 3 a) Unit cell structure of PEA2(MA)n −1PbnI3 n +1. b) Relative absorption intensity near the absorption onset for different n values. c) PL decay data before and after 10 d storage. d) PCE of devices based on MAPbI3 and quasi‐2D perovskites before and after 1440 h storage. Stability of e) PCE, f) J SC, g) FF, and h) V OC of perovskites with different n values. Reproduced with permission.61 Copyright 2016, American Chemical Society.
Figure 3 a) Unit cell structure of PEA2(MA)n −1PbnI3 n +1. b) Relative absorption intensity near the absorption onset for different n values. c) PL decay data before and after 10 d storage. d) PCE of devices based on MAPbI3 and quasi‐2D perovskites before and after 1440 h storage. Stability of e) PCE, f) J SC, g) FF, and h) V OC of perovskites with different n values. Reproduced with permission.61 Copyright 2016, American Chemical Society.CC BY · PubMed Central
Figure 4 XRD patterns of a) (BA)2(MA)Pb2I7, b) (BA)2(MA)2Pb3I10, and c) (BA)2(MA)3Pb4I13 perovskite films, with the illustration of their respective diffraction planes. Reproduced with permission.63 Copyright 2015, American Chemical Society.
Figure 4 XRD patterns of a) (BA)2(MA)Pb2I7, b) (BA)2(MA)2Pb3I10, and c) (BA)2(MA)3Pb4I13 perovskite films, with the illustration of their respective diffraction planes. Reproduced with permission.63 Copyright 2015, American Chemical Society.CC BY · PubMed Central
Figure 5 Schematic illustration of different preparation methods including a) one‐step method, b) fast deposition‐crystallization method, c) two‐step method, d) dual‐source thermal evaporation method, and e) vapor‐assisted solution process method procedures to deposit perovskite films.
Figure 5 Schematic illustration of different preparation methods including a) one‐step method, b) fast deposition‐crystallization method, c) two‐step method, d) dual‐source thermal evaporation method, and e) vapor‐assisted solution process method procedures to deposit perovskite films.CC BY · PubMed Central
Figure 6 Schematic diagrams of the a) DSSCs, b) mesoporous structure (mesostructure), c) HTL‐free mesoporous structure, d) n‐i‐p planar structure, and e) p‐i‐n planar structures.
Figure 6 Schematic diagrams of the a) DSSCs, b) mesoporous structure (mesostructure), c) HTL‐free mesoporous structure, d) n‐i‐p planar structure, and e) p‐i‐n planar structures.CC BY · PubMed Central
Figure 7 Scheme of the energy levels for perovskite materials and commonly used ETLs, HTLs, and the electrodes to the high performance and stability of PVSCs.
Figure 7 Scheme of the energy levels for perovskite materials and commonly used ETLs, HTLs, and the electrodes to the high performance and stability of PVSCs.CC BY · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Research works printed but not linked: 5

  1. Zhisheng Y., 2011, Acta Chim. Sin., 69, 627
  2. 10.1126/science.aad1015 · DOI · Paper page
  3. 10.1002/adma.201604186 · DOI · Paper page
  4. 10.1039/C6NR01927G · DOI · Paper page
  5. 10.1021/ja411014k · DOI · Paper page

Cited by

See all 454

Metadata

Authors
Fu, Q., Tang, X., Huang, B., Hu, T., Tan, L., Chen, L., & Chen, Y.
Affiliations
Nanchang University (CN)
Corresponding author
  • Chen, Lie
  • Chen, Yiwang
Venue
Advanced Science
Publisher
Wiley
Published
2018-02-22
Volume
5
Issue
5
Pages
1700387-1700387
ISSN
2198-3844 (ISSN-L)
OpenAlex
W2790911031
Cited by
454
References
199
Citations by year
2026: 20 · 2025: 36 · 2024: 37 · 2023: 65 · 2022: 59 · 2021: 65 · 2020: 82 · 2019: 62 · 2018: 26
FWCI
3.26
Type
journal article
Language
en
Open access
Locations
  • Advanced Science (publishedVersion, cc-by)
  • Europe PMC (PubMed Central) (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
Funders
National Natural Science Foundation of China (51663015, 51672121, 51673091, 51673092)
Topics
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Perovskite Materials and Applications
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Organic Electronics and Photovoltaics
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Silicon and Solar Cell Technologies
Keywords
perovskite solar cells, long-term stability, degradation mechanism, organic-inorganic hybrid perovskites, power conversion efficiency

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.