KCl Induced Corrosion of a 304-type Austenitic Stainless Steel at 600°C; The Role of Potassium
The DOI matches its Crossref record; 21 of the 21 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Potassium chloride may then condense on particles in the flue gas or on surfaces, forming a corrosive deposit. 6,11,12”
From Potassium, Chlorine, and Sulfur in Ash, Particles, Deposits, and Corrosion during Wood Combustion in a Circulating Fluidized-Bed Boiler (2007) · cites this paper as [11]
In the citing paper
“Once a deposit including alkali metals has been formed, corrosion may be enhanced 6,11,12 and the super heater tubes may have to be replaced, implying costly shutdown and repair.”
From Potassium, Chlorine, and Sulfur in Ash, Particles, Deposits, and Corrosion during Wood Combustion in a Circulating Fluidized-Bed Boiler (2007) · cites this paper as [11]
In the citing paper
“Exposures of alloy 304 and Sanicro 28 to an O2 + H2O environment in the presence of KCl (s) at 600 C showed that KCl reacts with the protective (Cr,Fe)2O3 oxide according to reaction 2, forming K2CrO4 and poorly protective Fe2O3: 11,12”
From Potassium, Chlorine, and Sulfur in Ash, Particles, Deposits, and Corrosion during Wood Combustion in a Circulating Fluidized-Bed Boiler (2007) · cites this paper as [11]
In the citing paper
“The reaction depletes the oxide in chromium and was reported to trigger rapid oxidation of the alloy, similar to the depletion caused by CrO2(OH)2 (g).”
From Potassium, Chlorine, and Sulfur in Ash, Particles, Deposits, and Corrosion during Wood Combustion in a Circulating Fluidized-Bed Boiler (2007) · cites this paper as [11]
In the citing paper
“Judging from previous laboratory investigations in similar environments, the acceleration of corrosion is attributed to the reaction of KCl (formed in the flue gas) with the protective chromium-rich oxide, forming K2CrO4.”
From Potassium, Chlorine, and Sulfur in Ash, Particles, Deposits, and Corrosion during Wood Combustion in a Circulating Fluidized-Bed Boiler (2007) · cites this paper as [11]
1 more claim about this paper
Create a free account to see every claim other papers make about this one.
Citations
Cites
Thermochemical data of pure substances
(1993) · Choice Reviews Online · doi:10.5860/choice.31-0632 · Cited by 4,494
Thermochemical Data of Pure Substances
Barin, I. (1995) · doi:10.1002/9783527619825 · Cited by 4,241
The implications of chlorine-associated corrosion on the operation of biomass-fired boilers
Nielsen, H. P., Frandsen, F. J., Dam-Johansen, K., & Baxter, L. L. (2000) · Progress in Energy and Combustion Science · doi:10.1016/s0360-1285(00)00003-4 · Cited by 785
Grabke, H. J., Reese, E., & Spiegel, M. (1995) · Corrosion Science · doi:10.1016/0010-938x(95)00011-8 · Cited by 537
Asteman, H., Svensson, J.-E., Norell, M., & Johansson, L.-G. (2000) · Oxidation of Metals · doi:10.1023/a:1004642310974 · Cited by 325
Self-citationAsteman, H., Svensson, J.-E., Johansson, L.-G., & Norell, M. (1999) · Oxidation of Metals · doi:10.1023/a:1018875024306 · Cited by 304
Self-citationDeposition and high temperature corrosion in a 10 MW straw fired boiler
Michelsen, H. P., Frandsen, F., Dam-Johansen, K., & Larsen, O. H. (1998) · Fuel Processing Technology · doi:10.1016/s0378-3820(97)00062-3 · Cited by 258
Halvarsson, M., Tang, J. E., Asteman, H., Svensson, J.-E., & Johansson, L.-G. (2006) · Corrosion Science · doi:10.1016/j.corsci.2005.08.012 · Cited by 146
Self-citationZahs, A., Spiegel, M., & Grabke, H. (1999) · Materials and Corrosion · doi:10.1002/(sici)1521-4176(199910)50:10<561::aid-maco561>3.0.co;2-l · Cited by 131
Accelerated oxidation rate of chromium induced by sodium chloride
Shinata, Y. (1987) · Oxidation of Metals · doi:10.1007/bf00659274 · Cited by 129
Research works printed but not linked: 2
- M. Montgomery, 1999, Materials and Corrosion., 50, 579, 10.1002/(sici)1521-4176(199910)50:10<579::aid-maco579>3.0.co;2-m · DOI · Paper page
- Y. Shinata, 1987, Oxidation of Metals., 27, 315, 10.1007/bf00659274 · DOI · Paper page
Cited by
Grate-firing of biomass for heat and power production
Yin, C., Rosendahl, L. A., & Kær, S. K. (2008) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2008.05.002 · Cited by 505
Biomass combustion technology development – It is all about chemical details
Hupa, M., Karlström, O., & Vainio, E. (2017) · Proceedings of the Combustion Institute · doi:10.1016/j.proci.2016.06.152 · Cited by 251
Antunes, R. A., & de Oliveira, M. C. L. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.07.013 · Cited by 184
Kassman, H., Liske, J., Steenari, B., & Åmand, L.-E. (2011) · Fuel Processing Technology · doi:10.1016/j.fuproc.2011.06.025 · Cited by 174
Are NaCl and KCl equally corrosive on superheater materials of steam boilers?
Enestam, S. H., Bankiewicz, D., Tuiremo, J., Mäkelä, K., & Hupa, M. M. (2012) · Fuel · doi:10.1016/j.fuel.2012.07.020 · Cited by 153
Alkali Induced High Temperature Corrosion of Stainless Steel: The Influence of NaCl, KCl and CaCl2
Karlsson, S., Pettersson, J., Johansson, L. G., & Svensson, J. E. (2012) · Oxidation of Metals · doi:10.1007/s11085-012-9293-7 · Cited by 118
Self-citationPettersson, J., Folkeson, N., Johansson, L.-G., & Svensson, J.-E. (2011) · Oxidation of Metals · doi:10.1007/s11085-011-9240-z · Cited by 117
Self-citationJonsson, T., Karlsson, S., Hooshyar, H., Sattari, M., Liske, J., Svensson, J.-E., & Johansson, L.-G. (2016) · Oxidation of Metals · doi:10.1007/s11085-016-9610-7 · Cited by 103
Self-citationZhang, S., Li, H., Jiang, Z., Zhang, B., Li, Z., Wu, J., Feng, H., Zhu, H., & Duan, F. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.108295 · Cited by 97
Folkeson, N., Jonsson, T., Halvarsson, M., Johansson, L. ‐., & Svensson, J. ‐. (2011) · Materials and Corrosion · doi:10.1002/maco.201005942 · Cited by 93
Self-citationSadeghi, E., Reddy, L., Hussain, T., Markocsan, N., & Joshi, S. V. (2017) · Corrosion Science · doi:10.1016/j.corsci.2017.12.033 · Cited by 95
“After this initial step, Cl diffuses through the oxide grain boundaries towards the metal/oxide interface via electrochemical reactions [7].”
BackgroundDavidsson, K. O., Åmand, L.-E., Leckner, B., Kovacevik, B., Svane, M., Hagström, M., Pettersson, J. B. C., Pettersson, J., Asteman, H., Svensson, J.-E., et al. (2007) · Energy & Fuels · doi:10.1021/ef060306c · Cited by 92
Self-citationJafari, R., & Sadeghi, E. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.06.021 · Cited by 92
Kaolin Addition during Biomass Combustion in a 35 MW Circulating Fluidized-Bed Boiler
Davidsson, K. O., Steenari, B.-M., & Eskilsson, D. (2007) · Energy & Fuels · doi:10.1021/ef070055n · Cited by 88
High temperature interaction of Al/Si-modified Fe–Cr alloys with KCl
Li, Y. S., Niu, Y., & Spiegel, M. (2006) · Corrosion Science · doi:10.1016/j.corsci.2006.10.019 · Cited by 92
Karlsson, S., Åmand, L.-E., & Liske, J. (2015) · Fuel · doi:10.1016/j.fuel.2014.09.007 · Cited by 79
“However, during corrosion initiation little or no chlorine have been detected in the corrosion product layer, indicating that the HCl(g) formed is released to the flue gas [7,9].”
BackgroundMethodJonsson, T., Froitzheim, J., Pettersson, J., Svensson, J.-E., Johansson, L.-G., & Halvarsson, M. (2009) · Oxidation of Metals · doi:10.1007/s11085-009-9156-z · Cited by 76
Self-citationHigh temperature corrosion of superheater steels by KCl and K2CO3 under dry and wet conditions
Lehmusto, J., Yrjas, P., Skrifvars, B.-J., & Hupa, M. M. (2012) · Fuel Processing Technology · doi:10.1016/j.fuproc.2012.05.020 · Cited by 81
Influence of KCl and HCl on high temperature corrosion of HVAF-sprayed NiCrAlY and NiCrMo coatings
Sadeghi, E., Reddy, L., Hussain, T., Huhtakangas, M., Markocsan, N., & Joshi, S. V. (2018) · Materials & Design · doi:10.1016/j.matdes.2018.03.048 · Cited by 74
Skrifvars, B.-J., Westén-Karlsson, M., Hupa, M., & Salmenoja, K. (2010) · Corrosion Science · doi:10.1016/j.corsci.2009.11.026 · Cited by 70
Lindberg, D., Niemi, J., Engblom, M., Yrjas, P., Laurén, T., & Hupa, M. (2016) · Fuel Processing Technology · doi:10.1016/j.fuproc.2015.10.011 · Cited by 70
Lehmusto, J., Skrifvars, B.-J., Yrjas, P., & Hupa, M. (2013) · Fuel Processing Technology · doi:10.1016/j.fuproc.2011.12.016 · Cited by 68
Wang, X., Liu, Z., Cheng, K., & Kong, Y. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111102 · Cited by 70
Tchoffor, P. A., Davidsson, K. O., & Thunman, H. (2013) · Energy & Fuels · doi:10.1021/ef401703a · Cited by 67
Characterization of Austenitic Stainless Steels Deformed at Elevated Temperature
Calmunger, M., Chai, G., Eriksson, R., Johansson, S., & Moverare, J. J. (2017) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-017-4212-9 · Cited by 66
Steenari, B. ‐., & Fedje, K. K. (2010) · Fuel · doi:10.1016/j.fuel.2010.02.006 · Cited by 64
Studies on the corrosion behavior of Fe-20Cr alloy in NaCl solution spray at 600 °C
Cao, M., Liu, L., Yu, Z., Fan, L., Li, Y., & Wang, F. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.01.033 · Cited by 66
Pettersson, J., Svensson, J. E., & Johansson, L. G. (2009) · Oxidation of Metals · doi:10.1007/s11085-009-9153-2 · Cited by 65
Self-citationSadeghi, E., Markocsan, N., & Joshi, S. V. (2019) · Journal of Thermal Spray Technology · doi:10.1007/s11666-019-00939-0 · Cited by 60
Eklund, J., Jönsson, B., Persdotter, A., Liske, J., Svensson, J.-E., & Jonsson, T. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.09.004 · Cited by 55
Self-citationKassim, S. A., Thor, J. A., Seman, A. A., & Abdullah, T. K. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108761 · Cited by 64
Thermogravimetric studies of high temperature reactions between potassium salts and chromium
Lehmusto, J., Lindberg, D., Yrjas, P., Skrifvars, B.-J., & Hupa, M. M. (2012) · Corrosion Science · doi:10.1016/j.corsci.2012.02.013 · Cited by 53
High temperature oxidation of metallic chromium exposed to eight different metal chlorides
Lehmusto, J., Skrifvars, B.-J., Yrjas, P., & Hupa, M. M. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.06.007 · Cited by 53
Meißner, T. M., Montero, X., Fähsing, D., & Galetz, M. C. (2020) · Corrosion Science · doi:10.1016/j.corsci.2019.108343 · Cited by 51
KCl-Induced Corrosion of the FeCrAl Alloy Kanthal ® AF at 600 °C and the Effect of H2O
Israelsson, N., Hellström, K., Svensson, J.-E., & Johansson, L.-G. (2015) · Oxidation of Metals · doi:10.1007/s11085-014-9506-3 · Cited by 46
Self-citationSulfur recirculation for increased electricity production in Waste-to-Energy plants
Andersson, S., Blomqvist, E. W., Bäfver, L., Jones, F., Davidsson, K., Froitzheim, J., Karlsson, M., Larsson, E., & Liske, J. (2014) · Waste Management · doi:10.1016/j.wasman.2013.09.002 · Cited by 45
Gruber, T., Schulze, K., Scharler, R., & Obernberger, I. (2014) · Fuel · doi:10.1016/j.fuel.2014.11.071 · Cited by 46
Okoro, S. C., Montgomery, M., Frandsen, F. J., & Pantleon, K. (2014) · Energy & Fuels · doi:10.1021/ef5017335 · Cited by 44
“Moreover Cl plays a vital role in the catastrophic corrosion observed in heat exchangers (superheaters) in biomass-fired boilers, especially those utilizing straw [4,5].”
BackgroundPersdotter, A., Eklund, J., Liske, J., & Jonsson, T. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108961 · Cited by 44
“[11,19] studied the influence of different alkali containing species on the breakdown of the Cr-rich oxide scale (i.”
BackgroundHigh-Temperature Corrosion of HVAF-Sprayed Ni-Based Coatings for Boiler Applications
Eklund, J., Phother, J., Sadeghi, E., Joshi, S., & Liske, J. (2019) · Oxidation of Metals · doi:10.1007/s11085-019-09906-0 · Cited by 41
KCl‐induced high temperature corrosion of selected commercial alloys: Part I: chromia‐formers
Kiamehr, S., Dahl, K. V., Montgomery, M., & Somers, M. A. J. (2015) · Materials and Corrosion · doi:10.1002/maco.201408213 · Cited by 42
High temperature corrosion behavior of Ni and Co base HVOF coatings exposed to NaCl-KCl salt mixture
Abu-warda, N., Tomás, L. M., López, A. J., & Utrilla, M. V. (2021) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2021.127277 · Cited by 45
Pettersson, C., Johansson, L.-G., & Svensson, J.-E. (2008) · Oxidation of Metals · doi:10.1007/s11085-008-9118-x · Cited by 40
Self-citationPan, P., Zhou, W., Zhao, Y., Wang, Y., & Zhang, N. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109938 · Cited by 42
Karlsson, S., Jonsson, T., Hall, J., Svensson, J.-E., & Liske, J. (2014) · Energy & Fuels · doi:10.1021/ef402127h · Cited by 41
Self-citationPhother-Simon, J., Hanif, I., Liske, J., & Jonsson, T. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109315 · Cited by 37
KCl-Induced High-Temperature Corrosion Behavior of HVAF-Sprayed Ni-Based Coatings in Ambient Air
Jafari, R., Sadeghimeresht, E., Farahani, T. S., Huhtakangas, M., Markocsan, N., & Joshi, S. (2018) · Journal of Thermal Spray Technology · doi:10.1007/s11666-017-0684-9 · Cited by 37
Auinger, M., Müller‐Lorenz, E. M., & Rohwerder, M. (2014) · Corrosion Science · doi:10.1016/j.corsci.2014.06.049 · Cited by 39
A microstructural investigation into the accelerated corrosion of P91 steel during biomass co-firing
O’Hagan, C. P., O’Brien, B., Leen, S. B., & Monaghan, R. F. D. (2016) · Corrosion Science · doi:10.1016/j.corsci.2016.03.028 · Cited by 38
Effect of Water Vapor on High-Temperature Corrosion under Conditions Mimicking Biomass Firing
Okoro, S. C., Montgomery, M., Frandsen, F., & Pantleon, K. (2015) · Energy & Fuels · doi:10.1021/acs.energyfuels.5b01045 · Cited by 37
Laser Clad and HVOF-Sprayed Stellite 6 Coating in Chlorine-Rich Environment with KCl at 700 °C
Pala, Z., Bai, M., Lukáč, F., & Hussain, T. (2017) · Oxidation of Metals · doi:10.1007/s11085-017-9776-7 · Cited by 35
Wu, D., Dahl, K. V., Christiansen, T. L., Montgomery, M., & Hald, J. K. (2019) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2018.12.129 · Cited by 35
Du, Y., Wang, C., Yang, L., Zhu, S., & Wang, F. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108599 · Cited by 35
Fireside corrosion on T24 steel pipes and HVOF NiCr coatings exposed to different salt mixtures
Abu-warda, N., López, A. J., Pedraza, F., & Utrilla, M. V. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108747 · Cited by 32
“The high volatility of the iron chloride brings about its diffusion backwards (FeCl2(g)) through the non-protective Fe-rich oxide layer [34].”
BackgroundHigh Temperature Corrosion Resistant and Anti-slagging Coatings for Boilers: A Review
Khantisopon, K., Singh, S., Jitputti, J., Berndt, C. C., & Ang, A. S. M. (2024) · High Temperature Corrosion of Materials · doi:10.1007/s11085-024-10251-0 · Cited by 30
Hooshyar, H., Jonsson, T., Hall, J., Svensson, J.-E., Johansson, L., & Liske, J. (2015) · Oxidation of Metals · doi:10.1007/s11085-015-9597-5 · Cited by 33
Self-citationArivarasu, M., Kannan, M. V., Ramkumar, K. D., & Arivazhagan, N. (2017) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1080/1478422x.2016.1213061 · Cited by 30
Sui, J., Lehmusto, J., Bergelin, M., & Hupa, L. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.04.010 · Cited by 26
Li, J., Liu, Z., Ma, H., Wang, X., Kong, Y., Li, Y., & Shen, Y. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111413 · Cited by 29
Continuous KCl addition in high temperature exposures of 304 L – A way to mimic a boiler environment
Phother-Simon, J., Jonsson, T., & Liske, J. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108511 · Cited by 25
Ssenteza, V., Eklund, J., Hanif, I., Liske, J., & Jonsson, T. (2023) · Corrosion Science · doi:10.1016/j.corsci.2022.110896 · Cited by 25
Guo, H., Fan, W., Liu, Y., & Long, J. (2024) · Process Safety and Environmental Protection · doi:10.1016/j.psep.2024.05.130 · Cited by 25
Wu, D., Liu, S., Yuan, Z., Cao, P., Wei, X., & Zhang, C. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109689 · Cited by 25
Eklund, J., Hanif, I., Bigdeli, S., & Jonsson, T. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110114 · Cited by 25
High Temperature Corrosion Behaviors of the Superheater Materials
Luo, W.-W., Liu, Z., Wang, Y., & Yang, R. (2012) · Procedia Engineering · doi:10.1016/j.proeng.2012.03.033 · Cited by 26
“Especially the role of potassium has been alighted with the identification of potassium chromate in the corrosion layer [11-12].”
BackgroundCalmunger, M., Eriksson, R., Chai, G., Johansson, S., & Moverare, J. J. (2015) · Corrosion Science · doi:10.1016/j.corsci.2015.08.030 · Cited by 26
Eklund, J., Persdotter, A., Hanif, I., Bigdeli, S., & Jonsson, T. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109584 · Cited by 23
Deposit Shedding in Biomass-Fired Boilers: Shear Adhesion Strength Measurements
Laxminarayan, Y., Jensen, P. A., Wu, H., Frandsen, F. J., Sander, B., & Glarborg, P. (2017) · Energy & Fuels · doi:10.1021/acs.energyfuels.7b01312 · Cited by 23
Kiamehr, S., Dahl, K. V., Montgomery, M., & Somers, M. A. J. (2015) · Materials and Corrosion · doi:10.1002/maco.201408215 · Cited by 24
Persdotter, A., Sattari, M., Larsson, E., Ogaz, M. A. O., Liske, J., & Jonsson, T. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.108234 · Cited by 26
The long-term corrosion behavior of fecral(Si) alloys after breakaway oxidation at 600 °C
Eklund, J., Persdotter, A., Ssenteza, V., & Jonsson, T. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111155 · Cited by 22
Gada, H., Mudgal, D., Parvez, S., & Ahmad, B. (2019) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2019.104256 · Cited by 23
Phother-Simon, J., Hanif, I., Jonsson, T., & Liske, J. (2024) · Fuel · doi:10.1016/j.fuel.2023.130012 · Cited by 21
Effect of Mo on corrosion behavior of Ni20Cr– x Mo alloys in air with NaCl–KCl–CaCl 2 vapor at 570°C
Izzuddin, H., Hayashi, S., Yoneda, S., Kogin, T., Ishikawa, E., & Noguchi, M. (2020) · Materials and Corrosion · doi:10.1002/maco.201911469 · Cited by 22
Corrosion of furnace wall materials in waste-wood fired power plant
Alipour, Y., & Henderson, P. (2014) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1179/1743278214y.0000000228 · Cited by 24
“Alkali metals such as potassium, sodium and calcium have been found to react with protective chromia scale to form non-protective chromates.(12,13) Corrosion mechanisms have usually been studied using simulated (and simplified) environments in laboratories, but in this work corrosion experiments have been performed di…”
BackgroundKassman, H. (2012) · Chalmers Publication Library (Chalmers University of Technology) · Cited by 26
Recent Development of Corrosion Factors and Coating Applications in Biomass Firing Plants
Wu, D., Yuan, Z., Liu, S., Zheng, J., Wei, X., & Zhang, C. (2020) · Coatings · doi:10.3390/coatings10101001 · Cited by 22
Critical Corrosion Phenomena on Superheaters in Biomass and Waste-Fired Boilers
Johansson, L., Svensson, J., Skog, E., Liske, J., Pettersson, C., Folkeson, N., Asteman, H., Jonsson, T., & Halvarsson, M. (2007) · Journal of Iron and Steel Research International · doi:10.1016/s1006-706x(08)60048-5 · Cited by 21
Self-citationAlipour, Y., Henderson, P., & Szakálos, P. (2013) · Materials and Corrosion · doi:10.1002/maco.201307118 · Cited by 23
KCl-Induced High Temperature Corrosion of the Austenitic Stainless Steel 304L – The Influence of SO2
Karlsson, S., Pettersson, J., Svensson, J. E., & Johansson, L. G. (2011) · Materials Science Forum · doi:10.4028/www.scientific.net/msf.696.224 · Cited by 20
Self-citationPotassium Retention in Updraft Gasification of Wood
Olwa, J., Öhman, M. C., Pettersson, E., Boström, D., Okure, M. A. E., & Kjellström, B. (2013) · Energy & Fuels · doi:10.1021/ef401179f · Cited by 20
Cantatore, V., Olivas Ogaz, M. A., Liske, J., Jonsson, T., Svensson, J.-E., Johansson, L.-G., & Panas, I. (2019) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.9b06497 · Cited by 19
Self-citationBlomberg, T., Tripathi, T. S., & Karppinen, M. J. (2019) · RSC Advances · doi:10.1039/c9ra00582j · Cited by 21
Proff, C., Jonsson, T., Pettersson, C., Svensson, J.-E., Johansson, L.-G., & Halvarsson, M. (2009) · Materials at High Temperatures · doi:10.1179/096034009x464339 · Cited by 19
“The breakdown of the protective scale was then attributed primarily to the formation of K2CrO4, depleting the protective oxide in chromium [12,13].”
BackgroundSelf-citationEffects of Cations on Corrosion of Inconel 625 in Molten Chloride Salts
Zhu, M. F., Ma, H., Wang, M., Wang, Z., & Sharif, A. A. (2015) · High Temperature Materials and Processes · doi:10.1515/htmp-2014-0225 · Cited by 21
Lehmusto, J., Lindberg, D., Yrjas, P., Skrifvars, B.-J., & Hupa, M. M. (2011) · Oxidation of Metals · doi:10.1007/s11085-011-9277-z · Cited by 19
Fan, L., Liu, L., Lv, Y. L., Wang, H., Fu, A., Yuan, J., Li, Y., Wang, F., & Yin, C. (2020) · Scientific Reports · doi:10.1038/s41598-020-73034-y · Cited by 20
Lariot-Sánchez, C., Gutierrez, A. R., Rodríguez–Machín, L., Rubio-González, A., & Quintero, P. J. I. (2022) · Oxidation of Metals · doi:10.1007/s11085-022-10102-w · Cited by 19
Okoro, S. C., Kiamehr, S., Montgomery, M., Frandsen, F., & Pantleon, K. (2016) · Materials and Corrosion · doi:10.1002/maco.201609174 · Cited by 17
Sim, J.-H., Kim, Y.-S., & Cho, I.-J. (2017) · Nuclear Engineering and Technology · doi:10.1016/j.net.2017.02.007 · Cited by 17
Superheater Corrosion In Biomass Boilers: Today's Science and Technology
USDOE Office of Energy Efficiency and Renewable Energy (EERE), & Sharp, W. (2010) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · doi:10.2172/1048711 · Cited by 24
Persdotter, A., Boll, T., & Jonsson, T. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109779 · Cited by 16
Alipour, Y., Talus, A., Henderson, P., & Norling, R. (2015) · Fuel Processing Technology · doi:10.1016/j.fuproc.2015.07.014 · Cited by 18
Khantisopon, K., Tharajak, J., Nawarat, P., Sanpo, N., & Ang, A. S. M. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110470 · Cited by 16
The effect of Cl, Br, and F on high-temperature corrosion of heat-transfer alloys
Eriksson, J.-E., Lehmusto, J., Dirbeba, M., Silvander, L., Lindberg, D., & Hupa, L. (2023) · Fuel · doi:10.1016/j.fuel.2023.128516 · Cited by 15
Hellström, K., Hall, J., Malmberg, P., Cao, Y. J., Norell, M., & Svensson, J. (2014) · Energy & Fuels · doi:10.1021/ef501269j · Cited by 16
Self-citationThe Onset of Potassium Chloride Induced High Temperature Corrosion: A Novel Experimental Approach
Sui, J., Lehmusto, J., Bergelin, M., & Hupa, M. M. (2014) · Oxidation of Metals · doi:10.1007/s11085-014-9501-8 · Cited by 15
Effect of Lead Content in Used Wood Fuel on Furnace Wall Corrosion of 16Mo3, 304L and Alloy 625
Talus, A., Norling, R., Wickström, L., & Hjörnhede, A. (2017) · Oxidation of Metals · doi:10.1007/s11085-017-9727-3 · Cited by 17
Wu, H., Yrjas, P., & Hupa, M. M. (2015) · Energy & Fuels · doi:10.1021/ef502245f · Cited by 17
A Laboratory Study of the in Situ Sulfation of Alkali Chloride Rich Deposits: Corrosion Perspective
Karlsson, S., Larsson, E., Jonsson, T., Svensson, J.-E., & Liske, J. (2016) · Energy & Fuels · doi:10.1021/acs.energyfuels.6b00372 · Cited by 16
Self-citation
Metadata
- Authors
- Pettersson, J., Asteman, H., Svensson, J. E., & Johansson, L. G.
- Affiliations
- Chalmers University of Technology (SE)
- Max-Planck-Institut für Nachhaltige Materialien (DE)
- Corresponding author
- Johansson, L. -G.
- Venue
- Oxidation of Metals
- Published
- 2005-08
- Volume
- 64
- Issue
- 1-2
- Pages
- 23-41
- ISSN
- 0030-770X (ISSN-L)
- 1573-4889
- OpenAlex
- W2042098561
- Cited by
- 182
- References
- 21
- Citations by year
- 2026: 5 · 2025: 8 · 2024: 13 · 2023: 10 · 2022: 9 · 2021: 10 · 2020: 9 · 2019: 17 · 2018: 10 · 2017: 12 · 2016: 9 · 2015: 13 · 2014: 15 · 2013: 10 · 2012: 10
- FWCI
- 4.63
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.springer.com/tdm (tdm)
- Locations
- Oxidation of Metals (publishedVersion)
- Chalmers Publication Library (Chalmers University of Technology) (submittedVersion)
- Chalmers Research (Chalmers University of Technology) (submittedVersion)
- Funders
- Chalmers Tekniska Högskola
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals
- Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
- Keywords
- high-temperature corrosion, 304 stainless steel, potassium chloride, potassium, potassium chromate, chromium depletion, spinel oxides, oxide scale growth, scale/metal interface
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.