Capacity Fading of Ni-Rich Li[NixCoyMn1–x–y]O2 (0.6 ≤ x ≤ 0.95) Cathodes for High-Energy-Density Lithium-Ion Batteries: Bulk or Surface Degradation?
Abstract
Ni-rich Li[Ni x Co y Mn 1– x – y ]O 2 cathodes ( x = 0.6, 0.8, 0.9, and 0.95) were tested to characterize the capacity fading mechanism of extremely rich Ni compositions. Increasing the Ni fraction in the cathode delivered a higher discharge capacity (192.9 mA h g –1 for Li[Ni 0.6 Co 0.2 Mn 0.2 ]O 2 versus 235.0 mA h g –1 for Li[Ni 0.95 Co 0.025 Mn 0.025 ]O 2 ); however, the cycling stability was substantially reduced. Li[Ni 0.6 Co 0.2 Mn 0.2 ]O 2 and Li[Ni 0.8 Co 0.1 Mn 0.1 ]O 2 retained more than 95% of their respective initial capacities after 100 cycles, while the capacity retention of Li[Ni 0.9 Co 0.05 Mn 0.05 ]O 2 and Li[Ni 0.95 Co 0.025 Mn 0.025 ]O 2 was limited to 85% during the same cycling period. The relatively inferior cycling stability of Li[Ni x Co y Mn 1– x – y ]O 2 with x > 0.8 is attributed to the phase transition near the charge-end, causing an abrupt anisotropic shrinkage (or expansion during discharge), which was suppressed for compositions of x < 0.8. Residual stress stemming from the phase transition destabilized the internal microcracks and allowed the microcracks to propagate to the surface, providing channels for electrolyte penetration and subsequent degradation of the exposed internal surfaces formed by the microcracks. Further developments in particle morphology are required to dissipate the intrinsic lattice strain, stabilize the surface, and modify the composition to attain a satisfactory long-term cycling stability, and hence battery life.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Lithium−Air Battery: Promise and Challenges
Girishkumar, G., McCloskey, B., Luntz, A. C., Swanson, S., & Wilcke, W. (2010) · The Journal of Physical Chemistry Letters · doi:10.1021/jz1005384 · Cited by 2,528
Noh, H.-J., Youn, S., Yoon, C. S., & Sun, Y.-K. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.01.063 · Cited by 2,302
Self-citationElectrochemistry and Structural Chemistry of LiNiO2 (R3m) for 4 Volt Secondary Lithium Cells
Ohzuku, T., Ueda, A., & Nagayama, M. (1993) · Journal of The Electrochemical Society · doi:10.1149/1.2220730 · Cited by 1,384
Myung, S.-T., Maglia, F., Park, K.-J., Yoon, C. S., Lamp, P., Kim, S.-J., & Sun, Y.-K. (2017) · ACS Energy Letters · doi:10.1021/acsenergylett.6b00594 · Cited by 1,382
Self-citationJung, S., Gwon, H., Hong, J., Park, K., Seo, D., Kim, H., Hyun, J., Yang, W., & Kang, K. (2014) · Advanced Energy Materials · doi:10.1002/aenm.201300787 · Cited by 1,124
Self-citationBak, S.-M., Hu, E., Zhou, Y., Yu, X., Senanayake, S. D., Cho, S.-J., Kim, K.-B., Chung, K. Y., Yang, X.-Q., & Nam, K.-W. (2014) · ACS Applied Materials & Interfaces · doi:10.1021/am506712c · Cited by 1,010
Future generations of cathode materials: an automotive industry perspective
Andre, D., Kim, S.-J., Lamp, P., Lux, S. F., Maglia, F., Paschos, O., & Stiaszny, B. (2015) · Journal of Materials Chemistry A · doi:10.1039/c5ta00361j · Cited by 806
Kondrakov, A. O., Schmidt, A., Xu, J., Geßwein, H., Mönig, R., Hartmann, P., Sommer, H., Brezesinski, T., & Janek, J. (2017) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.6b12885 · Cited by 701
Study of the Failure Mechanisms of LiNi0.8Mn0.1Co0.1O2Cathode Material for Lithium Ion Batteries
Li, J., Downie, L. E., Ma, L., Qiu, W., & Dahn, J. R. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.1011507jes · Cited by 516
Watanabe, S., Kinoshita, M., Hosokawa, T., Morigaki, K., & Nakura, K. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.02.018 · Cited by 465
Cited by
Enabling High-Voltage Lithium-Metal Batteries under Practical Conditions
Ren, X., Zou, L., Cao, X., Engelhard, M. H., Liu, W., Burton, S. D., Lee, H., Niu, C., Matthews, B. E., Zhu, Z., et al. (2019) · Joule · doi:10.1016/j.joule.2019.05.006 · Cited by 1,092
Fast Charging of Lithium‐Ion Batteries: A Review of Materials Aspects
Weiss, M., Ruess, R., Kasnatscheew, J., Levartovsky, Y., Levy, N. R., Minnmann, P., Stolz, L., Waldmann, T., Wohlfahrt‐Mehrens, M., Aurbach, D., et al. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202101126 · Cited by 1,055
Lithium–Oxygen Batteries and Related Systems: Potential, Status, and Future
Kwak, W.-J., Rosy, Sharon, D., Xia, C., Kim, H., Johnson, L. R., Bruce, P. G., Nazar, L. F., Sun, Y.-K., Frimer, A. A., et al. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00609 · Cited by 1,009
Self-citationReversible planar gliding and microcracking in a single-crystalline Ni-rich cathode
Bi, Y., Tao, J., Wu, Y., Li, L., Xu, Y., Hu, E., Wu, B., Hu, J., Wang, C., Zhang, J.-G., et al. (2020) · Science · doi:10.1126/science.abc3167 · Cited by 889
Lithium-ion batteries – Current state of the art and anticipated developments
Armand, M., Axmann, P., Bresser, D., Copley, M., Edström, K., Ekberg, C., Guyomard, D., Lestriez, B., Novák, P., Petranikova, M., et al. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.228708 · Cited by 888
Yan, P., Zheng, J., Liu, J., Wang, B., Cheng, X., Zhang, Y., Sun, X., Wang, C., & Zhang, J.-G. (2018) · Nature Energy · doi:10.1038/s41560-018-0191-3 · Cited by 826
Degradation Mechanisms and Mitigation Strategies of Nickel-Rich NMC-Based Lithium-Ion Batteries
Li, T., Yuan, X.-Z., Zhang, L., Song, D., Shi, K., & Bock, C. (2020) · Electrochemical Energy Reviews · doi:10.1007/s41918-019-00053-3 · Cited by 753
Problems and their origins of Ni-rich layered oxide cathode materials
Zhang, S. S. (2020) · Energy Storage Materials · doi:10.1016/j.ensm.2019.08.013 · Cited by 746
Jiang, M., Danilov, D. L., Eichel, R., & Notten, P. H. L. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202103005 · Cited by 720
Bulk fatigue induced by surface reconstruction in layered Ni-rich cathodes for Li-ion batteries
Xu, C., Märker, K., Lee, J., Mahadevegowda, A., Reeves, P. J., Day, S. J., Groh, M. F., Emge, S. P., Ducati, C., Layla Mehdi, B., et al. (2021) · Nature Materials · doi:10.1038/s41563-020-0767-8 · Cited by 707
Capacity Fading Mechanisms in Ni-Rich Single-Crystal NCM Cathodes
Ryu, H.-H., Namkoong, B., Kim, J.-H., Belharouak, I., Yoon, C. S., & Sun, Y.-K. (2021) · ACS Energy Letters · doi:10.1021/acsenergylett.1c01089 · Cited by 631
Self-citationYang, H., Wu, H., Ge, M., Li, L., Yuan, Y., Yao, Q., Chen, J., Xia, L., Zheng, J., Chen, Z., et al. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201808825 · Cited by 630
Qian, G., Zhang, Y., Li, L., Zhang, R., Xu, J., Cheng, Z., Xie, S., Wang, H., Rao, Q., He, Y., et al. (2020) · Energy Storage Materials · doi:10.1016/j.ensm.2020.01.027 · Cited by 564
Kim, U.-H., Park, G.-T., Son, B.-K., Nam, G. W., Liu, J., Kuo, L.-Y., Kaghazchi, P., Yoon, C. S., & Sun, Y.-K. (2020) · Nature Energy · doi:10.1038/s41560-020-00693-6 · Cited by 540
Self-citationde Biasi, L., Schwarz, B., Brezesinski, T., Hartmann, P., Janek, J., & Ehrenberg, H. (2019) · Advanced Materials · doi:10.1002/adma.201900985 · Cited by 539
Capacity Fading of Ni-Rich NCA Cathodes: Effect of Microcracking Extent
Nam, G. W., Park, N.-Y., Park, K.-J., Yang, J., Liu, J., Yoon, C. S., & Sun, Y.-K. (2019) · ACS Energy Letters · doi:10.1021/acsenergylett.9b02302 · Cited by 505
Self-citationPark, K., Jung, H., Kuo, L., Kaghazchi, P., Yoon, C. S., & Sun, Y. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201801202 · Cited by 502
Self-citationHigh-Concentration Ether Electrolytes for Stable High-Voltage Lithium Metal Batteries
Ren, X., Zou, L., Jiao, S., Mei, D., Engelhard, M. H., Li, Q., Lee, H., Niu, C., Adams, B. D., Wang, C., et al. (2019) · ACS Energy Letters · doi:10.1021/acsenergylett.9b00381 · Cited by 502
Beyond Doping and Coating: Prospective Strategies for Stable High-Capacity Layered Ni-Rich Cathodes
Sun, H. H., Ryu, H.-H., Kim, U.-H., Weeks, J. A., Heller, A., Sun, Y.-K., & Mullins, C. B. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c00191 · Cited by 495
Self-citationIn situ inorganic conductive network formation in high-voltage single-crystal Ni-rich cathodes
Fan, X., Ou, X., Zhao, W., Liu, Y., Zhang, B., Zhang, J., Zou, L., Seidl, L., Li, Y., Hu, G., et al. (2021) · Nature Communications · doi:10.1038/s41467-021-25611-6 · Cited by 488
Transition metal-doped Ni-rich layered cathode materials for durable Li-ion batteries
Sun, H. H., Kim, U.-H., Park, J.-H., Park, S.-W., Seo, D.-H., Heller, A., Mullins, C. B., Yoon, C. S., & Sun, Y.-K. (2021) · Nature Communications · doi:10.1038/s41467-021-26815-6 · Cited by 457
Self-citationNi‐Rich/Co‐Poor Layered Cathode for Automotive Li‐Ion Batteries: Promises and Challenges
Wang, X., Ding, Y., Deng, Y., & Chen, Z. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201903864 · Cited by 427
Anion-enrichment interface enables high-voltage anode-free lithium metal batteries
Mao, M., Ji, X., Wang, Q., Lin, Z., Li, M., Liu, T., Wang, C., Hu, Y.-S., Li, H., Huang, X., et al. (2023) · Nature Communications · doi:10.1038/s41467-023-36853-x · Cited by 418
Märker, K., Reeves, P. J., Xu, C., Griffith, K. J., & Grey, C. P. (2019) · Chemistry of Materials · doi:10.1021/acs.chemmater.9b00140 · Cited by 417
Maleki Kheimeh Sari, H., & Li, X. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201901597 · Cited by 403
Quilty, C. D., Wu, D., Li, W., Bock, D. C., Wang, L., Housel, L. M., Abraham, A., Takeuchi, K. J., Marschilok, A. C., & Takeuchi, E. S. (2023) · Chemical Reviews · doi:10.1021/acs.chemrev.2c00214 · Cited by 388
Park, G.-T., Namkoong, B., Kim, S.-B., Liu, J., Yoon, C. S., & Sun, Y.-K. (2022) · Nature Energy · doi:10.1038/s41560-022-01106-6 · Cited by 385
Self-citationMao, J., Ye, C., Zhang, S., Xie, F., Zeng, R., Davey, K., Guo, Z., & Qiao, S. (2022) · Energy & Environmental Science · doi:10.1039/d2ee00162d · Cited by 365
Liu, J., Wang, J., Ni, Y., Zhang, K., Cheng, F., & Chen, J. (2021) · Materials Today · doi:10.1016/j.mattod.2020.10.028 · Cited by 349
Heterogeneous damage in Li-ion batteries: Experimental analysis and theoretical modeling
Xu, R., Yang, Y., Yin, F., Liu, P., Cloetens, P., Liu, Y., Lin, F., & Zhao, K. (2019) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2019.05.003 · Cited by 345
“The fragmentation of secondary particles, a form of intergranular crack and decohesion between primary particle, has been observed as the major aging mechanism in NMC and NCA ( Watanabe et al., 2014; Xu et al., 2017b; Ryu et al., 2018 ).”
BackgroundMethodInfluentialOxygen Release Induced Chemomechanical Breakdown of Layered Cathode Materials
Mu, L., Lin, R., Xu, R., Han, L., Xia, S., Sokaras, D., Steiner, J. D., Weng, T.-C., Nordlund, D., Doeff, M. M., et al. (2018) · Nano Letters · doi:10.1021/acs.nanolett.8b01036 · Cited by 345
Is Cobalt Needed in Ni-Rich Positive Electrode Materials for Lithium Ion Batteries?
Li, H., Cormier, M., Zhang, N., Inglis, J., Li, J., & Dahn, J. R. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.1381902jes · Cited by 343
Ren, X., Gao, P., Zou, L., Jiao, S., Cao, X., Zhang, X., Jia, H., Engelhard, M. H., Matthews, B. E., Wu, H., et al. (2020) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.2010852117 · Cited by 340
Mao, Y., Wang, X., Xia, S., Zhang, K., Wei, C., Bak, S., Shadike, Z., Liu, X., Yang, Y., Xu, R., et al. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201900247 · Cited by 339
Oxygen Loss in Layered Oxide Cathodes for Li-Ion Batteries: Mechanisms, Effects, and Mitigation
Zhang, H., Liu, H., Piper, L. F. J., Whittingham, M. S., & Zhou, G. (2022) · Chemical Reviews · doi:10.1021/acs.chemrev.1c00327 · Cited by 338
Mechanical properties of cathode materials for lithium-ion batteries
Stallard, J. C., Wheatcroft, L., Booth, S. G., Boston, R., Corr, S. A., De Volder, M. F. L., Inkson, B. J., & Fleck, N. A. (2022) · Joule · doi:10.1016/j.joule.2022.04.001 · Cited by 336
Impact of Cathode Material Particle Size on the Capacity of Bulk-Type All-Solid-State Batteries
Strauss, F., Bartsch, T., de Biasi, L., Kim, A.-Y., Janek, J., Hartmann, P., & Brezesinski, T. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b00275 · Cited by 334
Reducing cobalt from lithium-ion batteries for the electric vehicle era
Ryu, H.-H., Sun, H. H., Myung, S.-T., Yoon, C. S., & Sun, Y.-K. (2021) · Energy & Environmental Science · doi:10.1039/d0ee03581e · Cited by 331
Self-citationAdvanced Liquid Electrolytes for Rechargeable Li Metal Batteries
Jie, Y., Ren, X., Cao, R., Cai, W., & Jiao, S. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201910777 · Cited by 330
Two electrolyte decomposition pathways at nickel-rich cathode surfaces in lithium-ion batteries
Rinkel, B. L. D., Vivek, J. P., Garcia-Araez, N., & Grey, C. P. (2022) · Energy & Environmental Science · doi:10.1039/d1ee04053g · Cited by 326
Chakraborty, A., Kunnikuruvan, S., Kumar, S., Markovsky, B., Aurbach, D., Dixit, M., & Major, D. T. (2020) · Chemistry of Materials · doi:10.1021/acs.chemmater.9b04066 · Cited by 322
Kim, K., Ma, H., Park, S., & Choi, N.-S. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c00468 · Cited by 314
Xu, G., Liu, X., Daali, A., Amine, R., Chen, Z., & Amine, K. (2020) · Advanced Functional Materials · doi:10.1002/adfm.202004748 · Cited by 313
Yan, P., Zheng, J., Chen, T., Luo, L., Jiang, Y., Wang, K., Sui, M., Zhang, J.-G., Zhang, S., & Wang, C. (2018) · Nature Communications · doi:10.1038/s41467-018-04862-w · Cited by 310
Li, H., Zhou, P., Liu, F., Li, H., Cheng, F., & Chen, J. (2019) · Chemical Science · doi:10.1039/c8sc03385d · Cited by 307
An Unavoidable Challenge for Ni-Rich Positive Electrode Materials for Lithium-Ion Batteries
Li, H., Liu, A., Zhang, N., Wang, Y., Yin, S., Wu, H., & Dahn, J. R. (2019) · Chemistry of Materials · doi:10.1021/acs.chemmater.9b02372 · Cited by 304
Kim, Y., Seong, W. M., & Manthiram, A. (2021) · Energy Storage Materials · doi:10.1016/j.ensm.2020.09.020 · Cited by 299
Kim, U., Ryu, H., Kim, J., Mücke, R., Kaghazchi, P., Yoon, C. S., & Sun, Y. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803902 · Cited by 298
Self-citationDegradation Mechanism of Ni-Rich Cathode Materials: Focusing on Particle Interior
Park, N.-Y., Park, G.-T., Kim, S.-B., Jung, W., Park, B.-C., & Sun, Y.-K. (2022) · ACS Energy Letters · doi:10.1021/acsenergylett.2c01272 · Cited by 296
Self-citationLiang, Y., Liu, H., Wang, G., Wang, C., Ni, Y., Nan, C., & Fan, L. (2022) · InfoMat · doi:10.1002/inf2.12292 · Cited by 273
Ruess, R., Schweidler, S., Hemmelmann, H., Conforto, G., Bielefeld, A., Weber, D. A., Sann, J., Elm, M. T., & Janek, J. (2020) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ab9a2c · Cited by 271
Cobalt‐Free High‐Capacity Ni‐Rich Layered Li[Ni0.9Mn0.1]O2 Cathode
Aishova, A., Park, G., Yoon, C. S., & Sun, Y. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201903179 · Cited by 269
Self-citationRyu, H.-H., Park, G.-T., Yoon, C. S., & Sun, Y.-K. (2019) · Journal of Materials Chemistry A · doi:10.1039/c9ta06402h · Cited by 267
Self-citationA highly stabilized Ni-rich NCA cathode for high-energy lithium-ion batteries
Ryu, H.-H., Park, N.-Y., Seo, J. H., Yu, Y.-S., Sharma, M., Mücke, R., Kaghazchi, P., Yoon, C. S., & Sun, Y.-K. (2020) · Materials Today · doi:10.1016/j.mattod.2020.01.019 · Cited by 264
Self-citationChemomechanical interplay of layered cathode materials undergoing fast charging in lithium batteries
Xia, S., Mu, L., Xu, Z., Wang, J., Wei, C., Liu, L., Pianetta, P., Zhao, K., Yu, X., Lin, F., et al. (2018) · Nano Energy · doi:10.1016/j.nanoen.2018.09.051 · Cited by 262
Rational design of mechanically robust Ni-rich cathode materials via concentration gradient strategy
Liu, T., Yu, L., Lu, J., Zhou, T., Huang, X., Cai, Z., Dai, A., Gim, J., Ren, Y., Xiao, X., et al. (2021) · Nature Communications · doi:10.1038/s41467-021-26290-z · Cited by 260
Yang, S.-C., Hua, Y., Qiao, D., Lian, Y.-B., Pan, Y.-W., & He, Y.-L. (2019) · Electrochimica Acta · doi:10.1016/j.electacta.2019.134928 · Cited by 152
Lee, H., Lim, H.-S., Ren, X., Yu, L., Engelhard, M. H., Han, K. S., Lee, J., Kim, H.-T., Xiao, J., Liu, J., et al. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b01819 · Cited by 150
Liu, P., Xu, R., Liu, Y., Lin, F., & Zhao, K. (2020) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ab78fa · Cited by 74
Wang, J., Li, D., Zeng, W., Chen, X., Zhang, Y., Zhang, S., Li, Z., Li, C., & Mu, S. (2025) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2024.11.016 · Cited by 62
Metadata
- Authors
- Ryu, H.-H., Park, K.-J., Yoon, C. S., & Sun, Y.-K.
- Venue
- Chemistry of Materials
- Publisher
- American Chemical Society (ACS)
- Published
- 2018-02-05
- Volume
- 30
- Issue
- 3
- Pages
- 1155-1163
- ISSN
- 0897-4756 (ISSN-L)
- 1520-5002
- OpenAlex
- W2787322343
- Cited by
- 1,629
- References
- 27
- FWCI
- 48.64
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.