Instant tough bonding of hydrogels for soft machines and electronics

Open access

The DOI matches its Crossref record; 56 of the 57 references it cites were found in a registry or an index.

Abstract

A strategy for bonding water-rich hydrogels to diverse materials for electronic skins, energy storage, and soft optics is reported.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1126/sciadv.1700053

Cites

56 of 56 references verified0 citation errors · 0 not checkable

Statistics

Figures

Fig. 1 Instant tough bonding of hydrogels to a wide range of materials. (A) Schematic illustration of the bonding method. An adhesive dispersion is used to instantly tough-bond (i) heterogeneous hydrogels, (ii) hydrogels and elastomers, and (iii) rigid to flexible foils to (prestretched) hydrogels in less than a minute. (B) The bonding agent links tough hydrogels with covalent and dissipative cross-links to elastomers, and the formed interface is instant and tough yet remains stretchable. (C) Instant healing of a conductive hydrogel rod used to light up a light-emitting diode (LED) circuit. Both mechanical and electrical properties are restored after complete incision. (D) Normalized resistance versus uniaxial strain before (blue trace) and after (red trace) healing a hydrogel conductor. (E to G) Hydrogel square (colored blue for visibility) bonded to a transparent elastomer. The soft hybrid is stretched more than 1000% in area without delamination. (H to J) A conducting Cu-coated poly(ethylene terephthalate) (PET) foil is tough-bonded to a prestretched hydrogel. Upon release of the prestrain, out-of-plane wrinkles form in the foil, creating a reversibly stretchable soft-hard hybrid.
Fig. 1 Instant tough bonding of hydrogels to a wide range of materials. (A) Schematic illustration of the bonding method. An adhesive dispersion is used to instantly tough-bond (i) heterogeneous hydrogels, (ii) hydrogels and elastomers, and (iii) rigid to flexible foils to (prestretched) hydrogels in less than a minute. (B) The bonding agent links tough hydrogels with covalent and dissipative cross-links to elastomers, and the formed interface is instant and tough yet remains stretchable. (C) Instant healing of a conductive hydrogel rod used to light up a light-emitting diode (LED) circuit. Both mechanical and electrical properties are restored after complete incision. (D) Normalized resistance versus uniaxial strain before (blue trace) and after (red trace) healing a hydrogel conductor. (E to G) Hydrogel square (colored blue for visibility) bonded to a transparent elastomer. The soft hybrid is stretched more than 1000% in area without delamination. (H to J) A conducting Cu-coated poly(ethylene terephthalate) (PET) foil is tough-bonded to a prestretched hydrogel. Upon release of the prestrain, out-of-plane wrinkles form in the foil, creating a reversibly stretchable soft-hard hybrid.CC BY-NC · PubMed Central
Fig. 2 Interfacial toughness and optically transparent, stretchable bonds. (A) Illustration of the 90° peeling test, with the hydrogel instantly tough-bonded to the bulk substrate. A liner serves as stiff backing. Crack propagation in the hydrogel occurs perpendicular to the peeling direction (detail and photograph with colored hydrogel). (B) Measured interfacial toughness for PVA-isoprene (turquoise trace), PAAm/alginate–PET (light blue trace), and PHEMA-Ecoflex (purple trace) instant tough bonds. (C) Interfacial toughness of PHEMA (purple), PAAm/alginate (light blue), and PVA (turquoise) hydrogels instantly tough-bonded to plastics, elastomers, leather, bone, and chromium-coated metals (aluminum and copper) and glass. Mean values and variance for at least three individual peel tests are shown. PDMS, poly(dimethylsiloxane); PI, polyimide. (D) Transmission and absorption spectra of the acrylic elastomer VHB (yellow trace), PAAm hydrogel (blue trace), and PAAm hydrogel instantly bonded to VHB (red trace). Bonding does not deteriorate the optical properties of the soft hybrid. (E) Nearly strain-independent transmission (red trace) at 600 nm for a biaxially stretched VHB/PAAm stack up to 2000% areal expansion. Inset: Photograph of the sandwich at 1000% strain with a color wheel in the background. The dashed red line outlines the PAAm hydrogel.
Fig. 2 Interfacial toughness and optically transparent, stretchable bonds. (A) Illustration of the 90° peeling test, with the hydrogel instantly tough-bonded to the bulk substrate. A liner serves as stiff backing. Crack propagation in the hydrogel occurs perpendicular to the peeling direction (detail and photograph with colored hydrogel). (B) Measured interfacial toughness for PVA-isoprene (turquoise trace), PAAm/alginate–PET (light blue trace), and PHEMA-Ecoflex (purple trace) instant tough bonds. (C) Interfacial toughness of PHEMA (purple), PAAm/alginate (light blue), and PVA (turquoise) hydrogels instantly tough-bonded to plastics, elastomers, leather, bone, and chromium-coated metals (aluminum and copper) and glass. Mean values and variance for at least three individual peel tests are shown. PDMS, poly(dimethylsiloxane); PI, polyimide. (D) Transmission and absorption spectra of the acrylic elastomer VHB (yellow trace), PAAm hydrogel (blue trace), and PAAm hydrogel instantly bonded to VHB (red trace). Bonding does not deteriorate the optical properties of the soft hybrid. (E) Nearly strain-independent transmission (red trace) at 600 nm for a biaxially stretched VHB/PAAm stack up to 2000% areal expansion. Inset: Photograph of the sandwich at 1000% strain with a color wheel in the background. The dashed red line outlines the PAAm hydrogel.CC BY-NC · PubMed Central
Fig. 3 Soft adaptive lens and energy harvester with instantly tough-bonded hydrogel electrodes. (A) Working principle of the tunable lens. Transparent hydrogel electrodes were used to electrically deform the lens, defined by a liquid reservoir embedded within a VHB elastomer. (B) Photograph of the soft lens without and with applied voltage, demonstrating electrical tuning of focal length. (C) Focal length and change of focal length versus voltage, illustrating a large voltage-induced focal length change of 110% at 6.5 kV. (D and E) Visualization of the voltage-controlled focal length change by showing laser light traces in a basin filled with a diluted rhodamine/water solution. (F) Illustration of mechanical into electrical energy conversion with a deformable elastomer/hydrogel capacitor. (G) Photographs of the deformable balloon-shaped elastomer/hydrogel capacitor. (H) Normalized capacitance of the deformable capacitor versus stretch ratio λ, demonstrating a λ4 behavior. (I and J) Exemplary energy harvesting cycle in pressure-volume and voltage-charge work conjugate plots. The enclosed areas in the two diagrams illustrate the mechanical energy input (497 mJ) and electrical energy output (54 mJ) of the cycle, resulting in a conversion efficiency of more than 10%.
Fig. 3 Soft adaptive lens and energy harvester with instantly tough-bonded hydrogel electrodes. (A) Working principle of the tunable lens. Transparent hydrogel electrodes were used to electrically deform the lens, defined by a liquid reservoir embedded within a VHB elastomer. (B) Photograph of the soft lens without and with applied voltage, demonstrating electrical tuning of focal length. (C) Focal length and change of focal length versus voltage, illustrating a large voltage-induced focal length change of 110% at 6.5 kV. (D and E) Visualization of the voltage-controlled focal length change by showing laser light traces in a basin filled with a diluted rhodamine/water solution. (F) Illustration of mechanical into electrical energy conversion with a deformable elastomer/hydrogel capacitor. (G) Photographs of the deformable balloon-shaped elastomer/hydrogel capacitor. (H) Normalized capacitance of the deformable capacitor versus stretch ratio λ, demonstrating a λ4 behavior. (I and J) Exemplary energy harvesting cycle in pressure-volume and voltage-charge work conjugate plots. The enclosed areas in the two diagrams illustrate the mechanical energy input (497 mJ) and electrical energy output (54 mJ) of the cycle, resulting in a conversion efficiency of more than 10%.CC BY-NC · PubMed Central
Fig. 4 Tough, stretchable battery and self-powered stretchable circuit. (A) Scheme of a stretchable battery in top configuration, enabled by the tough hydrogel separator instantly tough-bonded to the elastomer matrix. Imperceptible 1.4-μm-thick electrodes serve as current collector. Cu-coated PET foil with Zn paste is the anode, and MnO2 paste contacted with Au-coated PET is the cathode. (B) Nyquist plot for top (red dots) and lateral (blue dots) configuration of a stretchable battery, showing reduced internal resistance due to shorter ionic paths through the separator in top configuration. (C) Voltage versus discharge current at 0% (red squares) and 50% (blue triangles) strain. Internal resistance decreases from 8.9 to 6.7 ohms with stretching due to thinning of the hydrogel separator. (D) Illustration of the self-powered stretchable LED circuit with a 6-μm PET circuit board and SMD elements. A dc-dc converter boosts the voltage of the battery to power three LEDs. (E and F) Stretchable circuit atop a hydrogel-based battery in relaxed (E) and strained and twisted state (F), without impairing function.
Fig. 4 Tough, stretchable battery and self-powered stretchable circuit. (A) Scheme of a stretchable battery in top configuration, enabled by the tough hydrogel separator instantly tough-bonded to the elastomer matrix. Imperceptible 1.4-μm-thick electrodes serve as current collector. Cu-coated PET foil with Zn paste is the anode, and MnO2 paste contacted with Au-coated PET is the cathode. (B) Nyquist plot for top (red dots) and lateral (blue dots) configuration of a stretchable battery, showing reduced internal resistance due to shorter ionic paths through the separator in top configuration. (C) Voltage versus discharge current at 0% (red squares) and 50% (blue triangles) strain. Internal resistance decreases from 8.9 to 6.7 ohms with stretching due to thinning of the hydrogel separator. (D) Illustration of the self-powered stretchable LED circuit with a 6-μm PET circuit board and SMD elements. A dc-dc converter boosts the voltage of the battery to power three LEDs. (E and F) Stretchable circuit atop a hydrogel-based battery in relaxed (E) and strained and twisted state (F), without impairing function.CC BY-NC · PubMed Central
Fig. 5 Hydrogel electronic skin. (A) Concept of a hydrogel smart skin, with a flexible unit bearing power supply, control, readout and communication units, and a stretchable transducer batch. PCB, printed circuit board. (B) Photograph of an untethered electronic hydrogel with four stretchable heating elements and adjoined temperature sensors strongly bonded to a PVA hydrogel. Battery, control, readout, and Bluetooth low energy communication electronics are hosted on a flexible circuit board. (C) Finite element (FE) simulation of the transducer batch with four heating elements enabled. (D) Corresponding infrared (IR) thermography image of the freestanding device. Dashed lines in (C) and (D) outline the heater and sensor metal traces. (E) Autonomous hydrogel electronic skin controlled and read out continuously via mobile phone, worn on a human wrist with all heaters activated. (F) Corresponding IR image after ~450 s with all heater elements activated. (G) Measured temperature evolution of the heater elements measured via IR thermography and (H) the sensor elements. Switching of the heating elements is indicated by vertical lines. Recorded temperature traces of the sensor elements (solid lines) are in excellent agreement with data taken from IR images (open squares). (I) Concept of thermally triggered drug delivery where the substance is enclosed in a lipid shell. Temperature increase melts the shell, releasing the drug into the hydrogel. (J) Thermally triggered diffusion of a green food colorant throughout the hydrogel matrix.
Fig. 5 Hydrogel electronic skin. (A) Concept of a hydrogel smart skin, with a flexible unit bearing power supply, control, readout and communication units, and a stretchable transducer batch. PCB, printed circuit board. (B) Photograph of an untethered electronic hydrogel with four stretchable heating elements and adjoined temperature sensors strongly bonded to a PVA hydrogel. Battery, control, readout, and Bluetooth low energy communication electronics are hosted on a flexible circuit board. (C) Finite element (FE) simulation of the transducer batch with four heating elements enabled. (D) Corresponding infrared (IR) thermography image of the freestanding device. Dashed lines in (C) and (D) outline the heater and sensor metal traces. (E) Autonomous hydrogel electronic skin controlled and read out continuously via mobile phone, worn on a human wrist with all heaters activated. (F) Corresponding IR image after ~450 s with all heater elements activated. (G) Measured temperature evolution of the heater elements measured via IR thermography and (H) the sensor elements. Switching of the heating elements is indicated by vertical lines. Recorded temperature traces of the sensor elements (solid lines) are in excellent agreement with data taken from IR images (open squares). (I) Concept of thermally triggered drug delivery where the substance is enclosed in a lipid shell. Temperature increase melts the shell, releasing the drug into the hydrogel. (J) Thermally triggered diffusion of a green food colorant throughout the hydrogel matrix.CC BY-NC · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 56 references

Research works printed but not linked: 2

  1. 10.1155/2008/520417 · doi:10.1155/2008/520417 · Paper page
  2. J. Crank The Mathematics of Diffusion (Oxford Univ. Press 1975).

Cited by

Metadata

Authors
Wirthl, D., Pichler, R., Drack, M., Kettlguber, G., Moser, R., Gerstmayr, R., Hartmann, F., Bradt, E., Kaltseis, R., Siket, C. M., Schausberger, S. E., Hild, S., Bauer, S., & Kaltenbrunner, M.
Affiliations
Johannes Kepler University of Linz (AT)
Corresponding author
  • Wirthl, Daniela
  • Pichler, Robert
  • Kaltenbrunner, Martin
Venue
Science Advances
Published
2017-06-02
Volume
3
Issue
6
Pages
e1700053-e1700053
ISSN
2375-2548 (ISSN-L)
OpenAlex
W2709454349
Cited by
471
References
57
Citations by year
2026: 24 · 2025: 45 · 2024: 52 · 2023: 58 · 2022: 58 · 2021: 49 · 2020: 73 · 2019: 60 · 2018: 44 · 2017: 8
FWCI
22.78
Type
journal article
Language
en
Open access
Licence
cc-by-nc
Locations
  • Science Advances (publishedVersion, cc-by-nc)
  • PubMed Central (publishedVersion, cc-by-nc)
  • PubMed (publishedVersion)
Funders
  • European Research Council (ID0EXBEK19758, SOFT-MAP)
  • Horizon 2020 Framework Programme (ID0EZHEK19759, WETFEET 641334)
Topics
  • Physical Sciences › Engineering › Biomedical Engineering › Advanced Sensor and Energy Harvesting Materials
  • Physical Sciences › Materials Science › Biomaterials › Hydrogels: synthesis, properties, applications
  • Physical Sciences › Engineering › Mechanical Engineering › Advanced Materials and Mechanics
Keywords
ionic hydrogels, soft electronics, soft machines, biaxial strain, stretchable batteries, self-powered circuits, electronic skin, drug delivery, rapid prototyping

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.