Interface issues of lithium metal anode for high‐energy batteries: Challenges, strategies, and perspectives
Open accessAbstract
Lithium (Li) metal is considered as one of the most promising anode materials for next‐generation high‐energy‐density storage systems. However, the practical application of Li metal anode is hindered by interfacial instability and air instability due to the highly reactivity of Li metal. Unstable interface in Li metal batteries (LMBs) directly dictates Li dendrite growth, “dead Li” and low Coulombic efficiency, resulting in inferior electrochemical performance of LMBs and even safety issues. In addition, its sensitivity to ambient air leads to the severe corrosion of Li metal anode, high requirements of production and storage, and increased manufacturing cost. Plenty of efforts in recent years have overcome many bottlenecks in these fields and hastened the practical applications of high‐energy‐density LMBs. In this review, we focus on emerging methods of these two aspects to fulfill a stable and low cost electrode. In this perspective, design artificial solid electrolyte interphase (SEI) layers, construct three‐dimensional conductive current collectors, optimize electrolytes, employ solid‐state electrolytes, and modify separators are summarized to be propitious to ameliorate interfacial stability. Meanwhile, ex situ/in situ formed protective layers are highlighted in favor of heightening air stability. Finally, several possible directions for the future research on advanced Li metal anode are addressed.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
Lithium battery chemistries enabled by solid-state electrolytes
Manthiram, A., Yu, X., & Wang, S. (2017) · Nature Reviews Materials · doi:10.1038/natrevmats.2016.103 · Cited by 4,689
A Review of Solid Electrolyte Interphases on Lithium Metal Anode
Cheng, X., Zhang, R., Zhao, C., Wei, F., Zhang, J., & Zhang, Q. (2016) · Advanced Science · doi:10.1002/advs.201500213 · Cited by 1,786
Design principles for electrolytes and interfaces for stable lithium-metal batteries
Tikekar, M. D., Choudhury, S., Tu, Z., & Archer, L. A. (2016) · Nature Energy · doi:10.1038/nenergy.2016.114 · Cited by 1,765
Chen, L., Li, Y., Li, S.-P., Fan, L.-Z., Nan, C.-W., & Goodenough, J. B. (2018) · Nano Energy · doi:10.1016/j.nanoen.2017.12.037 · Cited by 1,423
Quantifying inactive lithium in lithium metal batteries
Fang, C., Li, J., Zhang, M., Zhang, Y., Yang, F., Lee, J. Z., Lee, M.-H., Alvarado, J., Schroeder, M. A., Yang, Y., et al. (2019) · Nature · doi:10.1038/s41586-019-1481-z · Cited by 1,413
Self-citationHigh‐Voltage Lithium‐Metal Batteries Enabled by Localized High‐Concentration Electrolytes
Chen, S., Zheng, J., Mei, D., Han, K. S., Engelhard, M. H., Zhao, W., Xu, W., Liu, J., & Zhang, J. (2018) · Advanced Materials · doi:10.1002/adma.201706102 · Cited by 1,328
Recent Progress of the Solid‐State Electrolytes for High‐Energy Metal‐Based Batteries
Fan, L., Wei, S., Li, S., Li, Q., & Lu, Y. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201702657 · Cited by 1,179
A facile surface chemistry route to a stabilized lithium metal anode
Liang, X., Pang, Q., Kochetkov, I. R., Sempere, M. S., Huang, H., Sun, X., & Nazar, L. F. (2017) · Nature Energy · doi:10.1038/nenergy.2017.119 · Cited by 1,083
Cheng, X., Hou, T., Zhang, R., Peng, H., Zhao, C., Huang, J., & Zhang, Q. (2016) · Advanced Materials · doi:10.1002/adma.201506124 · Cited by 994
Progress of enhancing the safety of lithium ion battery from the electrolyte aspect
Wang, Q., Jiang, L., Yu, Y., & Sun, J. (2019) · Nano Energy · doi:10.1016/j.nanoen.2018.10.035 · Cited by 915
Recent Advances in Energy Chemistry between Solid-State Electrolyte and Safe Lithium-Metal Anodes
Cheng, X.-B., Zhao, C.-Z., Yao, Y.-X., Liu, H., & Zhang, Q. (2019) · Chem · doi:10.1016/j.chempr.2018.12.002 · Cited by 874
Thick Electrode Batteries: Principles, Opportunities, and Challenges
Kuang, Y., Chen, C., Kirsch, D., & Hu, L. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201901457 · Cited by 842
Zhang, H., Eshetu, G. G., Judez, X., Li, C., Rodriguez‐Martínez, L. M., & Armand, M. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201712702 · Cited by 774
High-energy lithium metal pouch cells with limited anode swelling and long stable cycles
Niu, C., Lee, H., Chen, S., Li, Q., Du, J., Xu, W., Zhang, J.-G., Whittingham, M. S., Xiao, J., & Liu, J. (2019) · Nature Energy · doi:10.1038/s41560-019-0390-6 · Cited by 732
Artificial Interphases for Highly Stable Lithium Metal Anode
Xu, R., Cheng, X.-B., Yan, C., Zhang, X.-Q., Xiao, Y., Zhao, C.-Z., Huang, J.-Q., & Zhang, Q. (2019) · Matter · doi:10.1016/j.matt.2019.05.016 · Cited by 721
The role of nanotechnology in the development of battery materials for electric vehicles
Lu, J., Chen, Z., Ma, Z., Pan, F., Curtiss, L. A., & Amine, K. (2016) · Nature Nanotechnology · doi:10.1038/nnano.2016.207 · Cited by 700
Self-smoothing anode for achieving high-energy lithium metal batteries under realistic conditions
Niu, C., Pan, H., Xu, W., Xiao, J., Zhang, J.-G., Luo, L., Wang, C., Mei, D., Meng, J., Wang, X., et al. (2019) · Nature Nanotechnology · doi:10.1038/s41565-019-0427-9 · Cited by 589
Self-citationGraphitized Carbon Fibers as Multifunctional 3D Current Collectors for High Areal Capacity Li Anodes
Zuo, T., Wu, X., Yang, C., Yin, Y., Ye, H., Li, N., & Guo, Y. (2017) · Advanced Materials · doi:10.1002/adma.201700389 · Cited by 579
Huo, H., Chen, Y., Luo, J., Yang, X., Guo, X., & Sun, X. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201804004 · Cited by 579
Zhang, X., Wang, S., Xue, C., Xin, C., Lin, Y., Shen, Y., Li, L., & Nan, C. (2019) · Advanced Materials · doi:10.1002/adma.201806082 · Cited by 551
Liu, L., Yin, Y., Li, J., Wang, S., Guo, Y., & Wan, L. (2018) · Advanced Materials · doi:10.1002/adma.201706216 · Cited by 538
Fast ion transport at solid–solid interfaces in hybrid battery anodes
Tu, Z., Choudhury, S., Zachman, M. J., Wei, S., Zhang, K., Kourkoutis, L. F., & Archer, L. A. (2018) · Nature Energy · doi:10.1038/s41560-018-0096-1 · Cited by 536
Uniform High Ionic Conducting Lithium Sulfide Protection Layer for Stable Lithium Metal Anode
Chen, H., Pei, A., Lin, D., Xie, J., Yang, A., Xu, J., Lin, K., Wang, J., Wang, H., Shi, F., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201900858 · Cited by 472
Air-stable and freestanding lithium alloy/graphene foil as an alternative to lithium metal anodes
Zhao, J., Zhou, G., Yan, K., Xie, J., Li, Y., Liao, L., Jin, Y., Liu, K., Hsu, P.-C., Wang, J., et al. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.129 · Cited by 468
An Armored Mixed Conductor Interphase on a Dendrite‐Free Lithium‐Metal Anode
Yan, C., Cheng, X., Yao, Y., Shen, X., Li, B., Li, W., Zhang, R., Huang, J., Li, H., & Zhang, Q. (2018) · Advanced Materials · doi:10.1002/adma.201804461 · Cited by 427
Langmuir–Blodgett artificial solid-electrolyte interphases for practical lithium metal batteries
Kim, M. S., Ryu, J.-H., Deepika, Lim, Y. R., Nah, I. W., Lee, K.-R., Archer, L. A., & Il Cho, W. (2018) · Nature Energy · doi:10.1038/s41560-018-0237-6 · Cited by 417
Lithium anode stable in air for low-cost fabrication of a dendrite-free lithium battery
Shen, X., Li, Y., Qian, T., Liu, J., Zhou, J., Yan, C., & Goodenough, J. B. (2019) · Nature Communications · doi:10.1038/s41467-019-08767-0 · Cited by 386
Li, C., Liu, S., Shi, C., Liang, G., Lu, Z., Fu, R., & Wu, D. (2019) · Nature Communications · doi:10.1038/s41467-019-09211-z · Cited by 384
Wang, X., Zhai, H., Qie, B., Cheng, Q., Li, A., Borovilas, J., Xu, B., Shi, C., Jin, T., Liao, X., et al. (2019) · Nano Energy · doi:10.1016/j.nanoen.2019.03.051 · Cited by 364
Self-citationYu, L., Chen, S., Lee, H., Zhang, L., Engelhard, M. H., Li, Q., Jiao, S., Liu, J., Xu, W., & Zhang, J.-G. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b00935 · Cited by 363
Ye, H., Zheng, Z., Yao, H., Liu, S., Zuo, T., Wu, X., Yin, Y., Li, N., Gu, J., Cao, F., et al. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201811955 · Cited by 360
Crumpled Graphene Balls Stabilized Dendrite-free Lithium Metal Anodes
Liu, S., Wang, A., Li, Q., Wu, J., Chiou, K., Huang, J., & Luo, J. (2018) · Joule · doi:10.1016/j.joule.2017.11.004 · Cited by 347
Challenges and issues facing lithium metal for solid-state rechargeable batteries
Mauger, A., Armand, M. B., Julien, C. M., & Zaghib, K. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.04.018 · Cited by 333
High‐Fluorinated Electrolytes for Li–S Batteries
Zheng, J., Ji, G., Fan, X., Chen, J., Li, Q., Wang, H., Yang, Y., DeMella, K. C., Raghavan, S. R., & Wang, C. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803774 · Cited by 331
High-rate lithium cycling in a scalable trilayer Li-garnet-electrolyte architecture
Hitz, G. T., McOwen, D. W., Zhang, L., Ma, Z., Fu, Z., Wen, Y., Gong, Y., Dai, J., Hamann, T. R., Hu, L., et al. (2019) · Materials Today · doi:10.1016/j.mattod.2018.04.004 · Cited by 318
Synergistic Dual‐Additive Electrolyte Enables Practical Lithium‐Metal Batteries
Li, S., Zhang, W., Wu, Q., Fan, L., Wang, X., Wang, X., Shen, Z., He, Y., & Lu, Y. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.202004853 · Cited by 318
Self-citationHuang, G., Han, J., Zhang, F., Wang, Z., Kashani, H., Watanabe, K., & Chen, M. (2019) · Advanced Materials · doi:10.1002/adma.201805334 · Cited by 313
Countersolvent Electrolytes for Lithium‐Metal Batteries
Piao, N., Ji, X., Xu, H., Fan, X., Chen, L., Liu, S., Garaga, M. N., Greenbaum, S. G., Wang, L., Wang, C., et al. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201903568 · Cited by 297
Transient Behavior of the Metal Interface in Lithium Metal–Garnet Batteries
Fu, K. (., Gong, Y., Fu, Z., Xie, H., Yao, Y., Liu, B., Carter, M., Wachsman, E., & Hu, L. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201708637 · Cited by 290
Self-citationAdvances in Interfaces between Li Metal Anode and Electrolyte
Zhang, X., Cheng, X., & Zhang, Q. (2018) · Advanced Materials Interfaces · doi:10.1002/admi.201701097 · Cited by 287
Protecting the Li‐Metal Anode in a Li–O2 Battery by using Boric Acid as an SEI‐Forming Additive
Huang, Z., Ren, J., Zhang, W., Xie, M., Li, Y., Sun, D., Shen, Y., & Huang, Y. (2018) · Advanced Materials · doi:10.1002/adma.201803270 · Cited by 275
Self-citationJiang, Z., Wang, S., Chen, X., Yang, W., Yao, X., Hu, X., Han, Q., & Wang, H. (2020) · Advanced Materials · doi:10.1002/adma.201906221 · Cited by 266
Jie, Y., Liu, X., Lei, Z., Wang, S., Chen, Y., Huang, F., Cao, R., Zhang, G., & Jiao, S. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.201914250 · Cited by 246
Chen, D., Huang, S., Zhong, L., Wang, S., Xiao, M., Han, D., & Meng, Y. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201907717 · Cited by 239
Liao, K., Wu, S., Mu, X., Lu, Q., Han, M., He, P., Shao, Z., & Zhou, H. (2018) · Advanced Materials · doi:10.1002/adma.201705711 · Cited by 226
Ju, Z., Nai, J., Wang, Y., Liu, T., Zheng, J., Yuan, H., Sheng, O., Jin, C., Zhang, W., Jin, Z., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-14358-1 · Cited by 224
Self-citationPeng, Z., Cao, X., Gao, P., Jia, H., Ren, X., Roy, S., Li, Z., Zhu, Y., Xie, W., Liu, D., et al. (2020) · Advanced Functional Materials · doi:10.1002/adfm.202001285 · Cited by 217
Lithium Silicide Surface Enrichment: A Solution to Lithium Metal Battery
Tang, W., Yin, X., Kang, S., Chen, Z., Tian, B., Teo, S. L., Wang, X., Chi, X., Loh, K. P., Lee, H., et al. (2018) · Advanced Materials · doi:10.1002/adma.201801745 · Cited by 213
Self-citationWu, J., Zeng, H., Li, X., Xiao, X. H., Liao, Y., Xue, Z., Ye, Y., & Xie, X. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201802430 · Cited by 213
Surface engineering of commercial Ni foams for stable Li metal anodes
Ke, X., Liang, Y., Ou, L., Liu, H., Chen, Y., Wu, W., Cheng, Y., Guo, Z., Lai, Y., Liu, P., et al. (2019) · Energy Storage Materials · doi:10.1016/j.ensm.2019.04.003 · Cited by 205
Rong, G., Zhang, X., Zhao, W. J., Qiu, Y., Liu, M., Ye, F., Xu, Y., Chen, J., Hou, Y., Li, W., et al. (2017) · Advanced Materials · doi:10.1002/adma.201606187 · Cited by 203
Tan, S., Yue, J., Hu, X., Shen, Z., Wang, W., Li, J., Zuo, T., Duan, H., Xiao, Y., Yin, Y., et al. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201903466 · Cited by 202
A 3D and Stable Lithium Anode for High‐Performance Lithium–Iodine Batteries
Li, K., Hu, Z., Ma, J., Chen, S., Mu, D., & Zhang, J. (2019) · Advanced Materials · doi:10.1002/adma.201902399 · Cited by 196
Xu, J., Liu, Q., Yu, Y., Wang, J., Yan, J., & Zhang, X. (2017) · Advanced Materials · doi:10.1002/adma.201606552 · Cited by 193
Zhang, C., Lyu, R., Lv, W., Li, H., Jiang, W., Li, J., Gu, S., Zhou, G., Huang, Z., Zhang, Y., et al. (2019) · Advanced Materials · doi:10.1002/adma.201904991 · Cited by 184
Electroless Formation of Hybrid Lithium Anodes for Fast Interfacial Ion Transport
Choudhury, S., Tu, Z., Stalin, S., Vu, D., Fawole, K., Gunceler, D., Sundararaman, R., & Archer, L. A. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201707754 · Cited by 183
Ultrathin Bilayer of Graphite/SiO2 as Solid Interface for Reviving Li Metal Anode
Pathak, R., Chen, K., Gurung, A., Reza, K. M., Bahrami, B., Wu, F., Chaudhary, A., Ghimire, N., Zhou, B., Zhang, W., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201901486 · Cited by 182
Self-citationLiu, S., Xia, X., Deng, S., Xie, D., Yao, Z., Zhang, L., Zhang, S., Wang, X., & Tu, J. (2019) · Advanced Materials · doi:10.1002/adma.201806470 · Cited by 177
Self-citationNacre‐Inspired Composite Electrolytes for Load‐Bearing Solid‐State Lithium‐Metal Batteries
Li, A., Liao, X., Zhang, H., Shi, L., Wang, P., Cheng, Q., Borovilas, J., Li, Z., Huang, W., Fu, Z., et al. (2020) · Advanced Materials · doi:10.1002/adma.201905517 · Cited by 162
Liang, J., Li, X., Zhao, Y., Goncharova, L. V., Li, W., Adair, K. R., Banis, M. N., Hu, Y., Sham, T., Huang, H., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201902125 · Cited by 157
Liu, X., Liu, J., Qian, T., Chen, H., & Yan, C. (2019) · Advanced Materials · doi:10.1002/adma.201902724 · Cited by 139
Ceramic–Salt Composite Electrolytes from Cold Sintering
Lee, W., Lyon, C. K., Seo, J., Lopez-Hallman, R., Leng, Y., Wang, C., Hickner, M. A., Randall, C. A., & Gomez, E. D. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201807872 · Cited by 131
A Nacre‐Inspired Separator Coating for Impact‐Tolerant Lithium Batteries
Song, Y., Wu, K., Zhang, T., Lu, L., Guan, Y., Zhou, F., Wang, X., Yin, Y., Tan, Y., Li, F., et al. (2019) · Advanced Materials · doi:10.1002/adma.201905711 · Cited by 115
Self-citationMartínez‐Ibáñez, M., Sánchez‐Díez, E., Qiao, L., Zhang, Y., Júdez, X., Santiago, A., Aldalur, I., Carrasco, J., Zhu, H., Forsyth, M., et al. (2020) · Advanced Functional Materials · doi:10.1002/adfm.202000455 · Cited by 99
Suppressing Li Metal Dendrites Through a Solid Li‐Ion Backup Layer
Salvatierra, R. V., López‐Silva, G. A., Jalilov, A. S., Yoon, J., Wu, G., Tsai, A., & Tour, J. M. (2018) · Advanced Materials · doi:10.1002/adma.201803869 · Cited by 84
An air-stable and waterproof lithium metal anode enabled by wax composite packaging
Zhang, Y., Lv, W. Z., Huang, Z., Zhou, G., Deng, Y., Zhang, J., Zhang, C., Hao, B., Qi, Q., He, Y., et al. (2019) · 中国科学通报:英文版 · doi:10.1016/j.scib.2019.05.025 · Cited by 74
A Li-dual carbon composite as stable anode material for Li batteries
Guo, F., Wang, Y., Kang, T., Liu, C., Shen, Y., Lu, W. M., Wu, X., & Chen, L. (2018) · Energy storage materials · doi:10.1016/j.ensm.2018.03.018 · Cited by 68
Li, X., Liu, Y., Pan, Y., Wang, M., Chen, J., Xu, H., Huang, Y., Lau, W., Shan, A., Zheng, J., et al. (2019) · Journal of Materials Chemistry A · doi:10.1039/c9ta06908a · Cited by 59
A highly stable host for lithium metal anode enabled by Li9Al4-Li3N-AlN structure
Peng, Z., Ren, F., Yang, S., Wang, M., Sun, J., Wang, D., Xu, W., & Zhang, J. (2019) · Nano Energy · doi:10.1016/j.nanoen.2019.02.033 · Cited by 51
Yang, Y., Wang, W., & Zhang, J. (2020) · Materials Today Energy · doi:10.1016/j.mtener.2020.100420 · Cited by 47
Park, S.-J., Hwang, J., & Sun, Y. (2019) · Journal of Materials Chemistry A · doi:10.1039/c9ta03713f · Cited by 44
Efficiently suppressing lithium dendrites on atomic level by ultrafiltration membrane of graphdiyne
Shang, H., Zuo, Z., Dong, X., Wang, F., Lu, F., Zheng, H., Li, K., & Li, Y.-L. (2018) · Materials Today Energy · doi:10.1016/j.mtener.2018.09.008 · Cited by 29
Noelle, D. J., Shi, Y., Wang, M., Le, A. V., & Qiao, Y. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.02.068 · Cited by 18
Cited by
Xue, P., Guo, C., Li, L., Li, H., Luo, D., Tan, L., & Chen, Z. (2022) · Advanced Materials · doi:10.1002/adma.202110047 · Cited by 259
Xiang, Y., Lu, L., Kottapalli, A. G. P., & Pei, Y. (2022) · Carbon Energy · doi:10.1002/cey2.185 · Cited by 253
Metadata
- Authors
- Han, Y., Liu, B., Xiao, Z., Zhang, W., Wang, X., Pan, G., Xia, Y., Xia, X., & Tu, J.
- Venue
- InfoMat
- Publisher
- Wiley
- Published
- 2021-01-15
- Volume
- 3
- Issue
- 2
- Pages
- 155-174
- ISSN
- 2567-3165 (ISSN-L)
- OpenAlex
- W3124865101
- Cited by
- 267
- References
- 74
- FWCI
- 16.13
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.