Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly
Open accessThe DOI matches its Crossref record; 281 of the 281 references it cites were found in a registry or an index; 44 of the 222 sources its claims cite were checked for support.
Abstract
This review critically covers recent progress of key materials for MEAs, focusing on how to integrate materials into electrodes and MEAs, along with advanced designs and manufacturing techniques.
Overview
CoChat Summary
TL;DR
This critical review surveys recent progress in key PEM fuel cell materials—catalysts, membranes/ionomers, and gas diffusion layers—and state-of-the-art membrane electrode assembly (MEA) manufacturing. It argues that despite advances, cost and lifetime barriers remain, especially low-Pt-loading performance loss, PGM-free catalyst instability, and gaps between rotating-disk-electrode (RDE) activity and MEA performance.
Key findings
- Pt-based catalysts remain the benchmark: the first-generation Toyota Mirai had total Pt loading of 0.365 mg Pt cm⁻² versus 35 mg Pt cm⁻² for a 1962 practical fuel cell, and the second-generation Mirai stack reached 5.4 kW L⁻¹ versus 3.1 kW L⁻¹ for the first generation; Mirai anode/cathode loadings were 0.05 and 0.315 mg Pt cm⁻², respectively.
- Advanced Pt catalysts show high RDE activity: jagged Pt nanowires reached ECSA up to 118 m² g⁻¹ and mass activity of 13.6 A mg Pt⁻¹ at 0.9 V; sulfur-anchored intermetallics were controlled to <5 nm after up to 1 000 °C sintering and reached 1.3–1.8 A mg Pt⁻¹ at 0.9 V; Fe-N-C catalysts achieved a half-wave potential of (0.88 ± 0.01) V vs. RHE, but PGM-free catalysts remain less active and stable than Pt in acidic PEM fuel cells.
- MEA manufacturing advances include CCM over CCS, slot-die and roll-to-roll coating, and freeze-drying to increase catalyst-layer porosity; a moderate ionomer content of ~26 wt.% gave the highest electrokinetic performance, and decal transfer cost was estimated at ~1.67 times the electrode coating process at 500 000 units/year.
- Material and operational constraints persist: PFSA membranes may be <10 µm thick but suffer higher gas crossover; PA-doped PBI membranes can operate from −20 to 200 °C; a protonated phosphonic acid PEM fuel cell delivered 780 mW cm⁻² at 160 °C with minimal degradation over 2 500 h and 700 thermal cycles; GDL thickness is typically 200–400 µm, and DOE heavy-duty targets are 25 000 and 30 000 h for 2025 and 2030.
Methods
- Design: critical review, not a primary experimental study; it focuses on “mature materials” used in industrial production and on integrating materials into electrodes and MEAs.
- Data/sample: literature and prior studies on ORR catalysts, membranes/ionomers, GDLs, and MEA fabrication steps; no new experimental sample or dataset is reported.
- Analysis: narrative synthesis organized by material class and manufacturing step, with tables of physical/electrochemical characterization methods for screening catalysts, membranes, ionomers, and GDLs, plus discussion of constraints and advanced integration strategies.
Limitations
- Stated: decreasing Pt loading causes performance loss and the low-Pt barrier is not completely addressed; PGM-free catalysts such as Fe-N-C degrade severely and remain far behind Pt; PFSA membranes have a restricted operating window and hydrocarbon ionomers are not mature for scale-up; optimal GDL porosity and pore-size distribution are not widely agreed; catalyst ink stability and high-efficiency, low-cost dispersion remain challenging; ordered catalyst layers may be difficult to scale up; and roll-to-roll coating faces multiple precision, lamination, and defect-control challenges.
- Evident from the text: as a review, it provides no primary experimental validation and relies on cited literature; it also repeatedly notes that RDE activity often cannot be reproduced in MEA testing, so reported catalyst performance may not translate directly to practical MEAs.
Model-written summary. Check it against the paper before relying on it.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
40 Valid · 13 Not valid · 138 Not checked · 98 Own results and interpretations
The cited sources support only part of this claim — read each source’s verdict below.
In the paper
“In addition to the significant progress in Pt-based catalysts for ORR, a large number of efforts have been devoted to Pt-group-metal-free (PGM-free) catalysts, which are promising alternatives to replace costly and scarce Pt catalysts [44,45].”
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > 2.1 Catalysts
What the sources say
- Partly supportedcites [44] 44. Du, L., Zhang, G.X., Sun, S.H.: Proton exchange membrane (PEM) fuel cells with platinum group metal (PGM)-free cath- ode. Automot. Innov. 4, 131-143 (2021). https:// doi. org/ 10. 1007/ s42154-021-00146-0 sourceExperimental — accuracy not yet measured
The Introduction says Pt-based PGM catalysts raise fuel-cell costs and calls replacing cathode PGMs with PGM-free alternatives a promising strategy. The section on high-performance PGM-free catalysts also describes them as a promising replacement. Our copy does not establish the claim that Pt is scarce. (LLM, conf=0.84)
- Not checked — no full text of the sourcecites [45] 45. Du, L., Xing, L.X., Zhang, G.X., et al.: Strategies for engineer- ing high-performance PGM-free catalysts toward oxygen reduc- tion and evolution reactions. Small Methods 4, 2000016 (2020). https:// doi. org/ 10. 1002/ smtd. 20200 0016 source
plain- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Partly supported
Every source the paper cites for this claim was checked and supports it.
In the paper
“Over the past decades, several kinds of PGM-free catalysts have been developed, among which the most representative is Fe-N-C due to its superior activity as a site for ORR [47].”
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > 2.1 Catalysts
What the sources say
- Supportedcites [47] 47. Du, L., Zhang, G.X., Liu, X.H., et al.: Biomass-derived nonpre- cious metal catalysts for oxygen reduction reaction: the demand- oriented engineering of active sites and structures. Carbon Energy 2, 561-581 (2020). https:// doi. org/ 10. 1002/ cey2. 73 source
Section 3 identifies single-atom Fe-N-C as a representative, promising PGM-free ORR catalyst. Section 3.2 describes its FeNₓ moieties as among the most promising PGM-free active sites for ORR. The source does not claim Fe-N-C outperforms PGM-based catalysts, but the citing sentence does not make that comparison. (LLM, conf=0.88)
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Supported
Every source the paper cites for this claim was checked and supports it.
In the paper
“As shown in Fig. 3a, b, a reliable ensemble learner, XGBoost, was established and trained to rank the degrees of importance among 26 complicated features in PEM fuel cells.”
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > 2.1 Catalysts
What the sources say
- Supportedcites [57] 57. Ding, R., Wang, R., Ding, Y.Q., et al.: Designing AI-aided analy- sis and prediction models for nonprecious metal electrocatalyst- based proton-exchange membrane fuel cells. Angew. Chem. Int. Ed. 59, 19175-19183 (2020). https:// doi. org/ 10. 1002/ anie. 20200 6928 source
The Conclusion (p. of our copy) states almost verbatim that 'a reliable ensemble learner, XGBoost, ranked the degrees of importance among 26 complicated features', and the Methods section (Machine Learning Algorithms Applied as Computational Tools) confirms XGBoost was chosen 'to provide a fair assessment of the importance among the 26 features'. The Feature Importance Ranking section reports the F-score-based ranking shown in Figure 3 and describes XGBoost as 'a reliable learner' (91.4% weighted precision), matching the citing sentence's Fig. 3a,b reference. The PEMFC/NPME context is the paper's own subject throughout. (LLM, conf=0.94)
boostedstates an association- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Supported
The cited sources support only part of this claim — read each source’s verdict below.
In the paper
“to therefore present better performance in MEA, particularly at low humidity (Fig. 5c).”
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > 2.2 Membranes and Ionomers
What the sources say
- Partly supportedcites [78] 78. Li, T., Shen, J.B., Chen, G.Y., et al.: Performance comparison of proton exchange membrane fuel cells with Nafion and aquiv- ion perfluorosulfonic acids with different equivalent weights as the electrode binders. ACS Omega 5, 17628-17636 (2020). https:// doi. org/ 10. 1021/ acsom ega. 0c021 10 sourceExperimental — accuracy not yet measured
The Results and Discussion section (Static Performance Response to Operation Conditions; page not provided) reports better performance for Aquivion-based SSC-CCMs than Nafion-based LSC-CCMs, with the difference greatest at low humidity. But the Experimental Section (Preparation of CCM; page not provided) says both were made by spraying different electrode-binder ionomers onto the same Gore membrane. The study therefore does not establish that an Aquivion membrane outperforms a Nafion membrane in an MEA. (LLM, conf=0.90)
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Partly supported
The cited sources support only part of this claim — read each source’s verdict below.
In the paper
“Recently, dual single-atom catalysts were proposed to achieve better ORR intrinsic activity, e.g., Fe/ Co-N-C [53,54].”
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > 2.1 Catalysts
What the sources say
- Partly supportedcites [53] 53. Gollasch, M., Müller-Hülstede, J., Schmies, H., et al.: Elucidat- ing synergistic effects of different metal ratios in bimetallic Fe/ Co-N-C catalysts for oxygen reduction reaction. Catalysts 11, 841 (2021). https:// doi. org/ 10. 3390/ catal 11070 841 sourceExperimental — accuracy not yet measured
Our copy does support the concept the citing sentence attaches to this source: the Introduction (Sec. 1) frames bimetallic Fe/Co-N-C with atomically dispersed Me-N sites as a route to 'tackle the downsides of each individual metal' (Fe's high ORR activity plus Co's stability), and the Conclusions (Sec. 4) confirm 'Proposed atomically dispersed Me-N sites have been achieved'. However, the source does not use the term 'dual single-atom catalysts', and its own data do not show an intrinsic-activity gain: Sec. 2.2.1/Table 1 reports that all bimetallic catalysts have higher Tafel slopes (72-83 mV dec-1) than the monometallic ones (57-63), 'hence the higher kinetic activity' being lower, and the Conclusions state monometallic Fe-N-C shows the highest ORR activity. So the 'proposed to achieve better ORR intrinsic activity' part is only supported as a stated hypothesis/motivation, not as a finding of this work. (LLM, conf=0.72)
- Not checked — no full text of the sourcecites [54] 54. Han, Y., Yin, S.H., Chen, Y.H., et al.: Experimental and DFT studies of oxygen reduction reaction promoted by binary site Fe/Co-N-C catalyst in acid. J. Electroanal. Chem. 914, 116322 (2022). https:// doi. org/ 10. 1016/j. jelec hem. 2022. 116322 source
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Partly supported
144 more claims · 27 with their cited sources checked
Create a free account to see all 289 claims and to verify the 15 references still open.
- It may state two separate claims as one. 103
- Probably not a substantial claim. 49
- Borderline: one of the tests for a substantial claim is unclear. 1
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
Each contradiction between two passages listed here was confirmed by an independent check.
Rated minor: it would not touch a result — a value no result rests on, a p-value that stays on the same side of the significance level, or a conflict that is clerical, resolved elsewhere in the paper, or outside its own findings.
In the paper
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > 3 State-of-the-Art Membrane Electrode Assembly Manufacturing Processes
“The MEA fabrication process generally includes ink dispersing, electrode coating, electrode drying, slitting and cutting, component assembly, and pressing (Fig. 12a-f).”
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > Materials integration into the MEAs.
“Figure: 12 Fig. 12 a Fig.12a-e General MEA fabrication process, including ink dispersing, coating, drying, cutting, assembly, and pressing”
Rated minor: it would not touch a result — a value no result rests on, a p-value that stays on the same side of the significance level, or a conflict that is clerical, resolved elsewhere in the paper, or outside its own findings.
In the paper
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > 3.2.2 Assembly Step
“The role of the GDL is discussed in Sect.2.4.”
§ Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly > 2.3 Gas Diffusion Layer (GDL)
“## 2.3 Gas Diffusion Layer (GDL)”
Citations
Cites
Items 201–281 of 281
Selamet, O. F., Pasaogullari, U., Spernjak, D., Hussey, D. S., Jacobson, D. L., & Mat, M. (2011) · ECS Transactions · doi:10.1149/1.3635568 · Cited by 41
Effect of rheological properties of catalyst slurry on the structure of catalyst layer in PEMFC
Yang, D., Guo, Y., Tang, H., Yang, D., Ming, P., Zhang, C., Li, B., & Zhu, S. (2022) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2021.12.227 · Cited by 41
Park, T., Chang, I., Jung, J. H., Lee, H. B., Ko, S. H., O'Hayre, R., Yoo, S. J., & Cha, S. W. (2017) · Energy · doi:10.1016/j.energy.2017.05.197 · Cited by 40 · cited 1×
“Excessive pressure can also cause a breakup of GDL fibers and deteriorate the hydrophobicity, resulting in failures in water management [223, 224].”
Chowdhury, A., Bird, A., Liu, J., Zenyuk, I. V., Kusoglu, A., Radke, C. J., & Weber, A. Z. (2021) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c07611 · Cited by 40 · cited 3×
“Meanwhile, it is necessary to provide high IEC without inducing negative effects on the catalyst and to further provide high oxygen permeability [100, 103, 104, 106, 107].”
Flow properties of an intact MPL from nano-tomography and pore network modelling
Ma, J., Zhang, X., Jiang, Z., Ostadi, H., Jiang, K. S., & Chen, R. (2014) · Fuel · doi:10.1016/j.fuel.2014.07.040 · Cited by 39 · cited 1×
“10b) (e.g., cracks and perforations as the liquid water pathway to the substrate layer, etc.) [144–149].”
New insights into the surface properties of hard-templated ordered mesoporous carbons
Li, X., Forouzandeh, F., Fürstenhaupt, T., Banham, D., Feng, F., Ye, S., Kwok, D. Y., & Birss, V. (2018) · Carbon · doi:10.1016/j.carbon.2017.11.049 · Cited by 39 · cited 1×
“The aligned catalyst framework concept has been intensively studied [260].”
Self-citationOn the state and stability of fuel cell catalyst inks
Bapat, S., Giehl, C., Kohsakowski, S., Peinecke, V., Schäffler, M., & Segets, D. (2021) · Advanced Powder Technology · doi:10.1016/j.apt.2021.08.030 · Cited by 38
Komoda, Y., Okabayashi, K., Nishimura, H., Hiromitsu, M., Oboshi, T., & Usui, H. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.04.015 · Cited by 38 · cited 1×
“Meanwhile, when a thick liquid film catalyst layer is coated, its high evaporation rate leads to an enrichment of ionomer at the top surface of the dried layer [213].”
Real time monitoring of water distribution in an operando fuel cell during transient states
Martínez, N., Peng, Z., Morin, A., Porcar, L., Gebel, G., & Lyonnard, S. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.08.067 · Cited by 38 · cited 1×
“Currently, optimization and improvement of MPLs revolve around (1) the thickness of MPLs [127–129], (2) the porosity and pore size distribution of MPLs [130–133], (3) hydrophobic or hydrophilic modifications of MPLs (Fig.”
Investigation of Water Transport in Perforated Gas Diffusion Layer by Neutron Radiography
Lu, Z., Waldecker, J. R., Xie, X., Lai, M., Hussey, D. S., & Jacobson, D. L. (2013) · ECS Transactions · doi:10.1149/05801.0315ecst · Cited by 38
Baker, A. M., Stewart, S. M., Ramaiyan, K. P., Banham, D., Ye, S., Garzón, F. H., Mukundan, R., & Borup, R. L. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/abdee6 · Cited by 37 · cited 1×
“It has been reported (7) Anode: that when using cerium oxide as a radical scavenging agent within membranes, the working lifespan is much longer than that of the reference membrane under accelerated durability test conditions [96–98].”
Self-citationNumerical simulation of the ordered catalyst layer in cathode of proton exchange membrane fuel cells
Du, C. Y., Cheng, X. Q., Yang, T., Yin, G. P., & Shi, P. F. (2005) · Electrochemistry Communications · doi:10.1016/j.elecom.2005.09.022 · Cited by 37 · cited 1×
“The simulation results revealed that the ordered catalyst layers show better performance than conventional catalyst layers due to the improvements in mass transport and the uniformity of the electrochemical reaction rate across the whole width of the catalyst layer [252].”
Jiang, S., Yi, B., Cao, L., Song, W., Zhao, Q., Yu, H., & Shao, Z. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.08.098 · Cited by 37 · cited 1×
“In addition, the electronic conductive polymer polypyrrole (PPy) nanowire can also be employed as the ordered catalyst support [266].”
Zheng, Z., Luo, L., Zhu, F., Cheng, X., Yang, F., Shen, S., Wei, G., & Zhang, J. (2019) · Electrochimica Acta · doi:10.1016/j.electacta.2019.134751 · Cited by 36 · cited 1×
“To date, various strategies to improve the performance have been developed, such as alloying Pt with transition metals [23, 24], building the core–shell structure [25, 26], nanowires [27–29], nanoplates [30], and nanoframes [31, 32].”
The effect of membrane electrode assembly methods on the performance in fuel cells
Yurko, Y., & Elbaz, L. (2021) · Electrochimica Acta · doi:10.1016/j.electacta.2021.138676 · Cited by 36 · cited 1×
“It has been found that to achieve the maximum performance of MEAs, hot-pressing conditions are crucial and should be optimized [221, 222].”
Modeling an ordered nanostructured cathode catalyst layer for proton exchange membrane fuel cells
Hussain, M. M., Song, D., Liu, Z.-S., & Xie, Z. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.10.111 · Cited by 35 · cited 1×
“In the absence of liquid water, oxygen diffusion in the pore phase was not the limiting factor, due to its parallel gas pores [254].”
Effect of Perforation Structure of Cathode GDL on Liquid Water Removal in PEFC
Okuhata, G., Tonoike, T., Nishida, K., Tsushima, S., & Hirai, S. (2013) · ECS Transactions · doi:10.1149/05801.1047ecst · Cited by 34 · cited 1×
“This strategy improves the wettability of the GDL while enhancing liquid water removal, effectively improving water management performance [150, 152, 158].”
1D PtCo nanowires as catalysts for PEMFCs with low Pt loading
Huang, J. S., Peng, B., Stracensky, T. S., Liu, Z., Zhang, A., Xu, M., Liu, Y., Zhao, Z., Duan, X., Jia, Q., et al. (2021) · Science China Materials · doi:10.1007/s40843-021-1777-x · Cited by 34 · cited 1×
“To date, various strategies to improve the performance have been developed, such as alloying Pt with transition metals [23, 24], building the core–shell structure [25, 26], nanowires [27–29], nanoplates [30], and nanoframes [31, 32].”
Tsushima, S., & Hirai, S. (2015) · Journal of Thermal Science and Technology · doi:10.1299/jtst.2015jtst0002 · Cited by 33 · cited 1×
“Therefore, it is important to balance crack and void formation to ensure high performance and durability under the operating conditions of PEM fuel cells [208].”
Ye, D. H., Zhan, Z. G., Lee, Y. J., Tu, Z. K., Zhang, Y., & Pan, M. (2013) · Fuel Cells · doi:10.1002/fuce.201300073 · Cited by 32 · cited 1×
“Another reason for membrane failure is mechanical degradation [7].”
Du, C. Y., Yang, T., Shi, P. F., Yin, G. P., & Cheng, X. Q. (2006) · Electrochimica Acta · doi:10.1016/j.electacta.2006.01.047 · Cited by 32 · cited 1×
“The detailed analysis indicated that the improved performance of the ordered catalyst layer can be primarily attributed to the uniform distributions of oxygen concentration and overpotential [253].”
Electrochemistry of Multilayer Electrodes: From the Basics to Energy Applications
Gu, M., & Kim, B.-S. (2021) · Accounts of Chemical Research · doi:10.1021/acs.accounts.0c00524 · Cited by 32 · cited 1×
“In practice, applying a multilayer design in the catalyst layer can also precisely control the internal architecture in the catalyst layer in three dimensions [268].”
Degradation of Platinum-Cobalt Alloy PEMFC Cathode Catalysts in Catalyst-Ionomer Inks
Myers, D. J., Kropf, A. J., Wegener, E. C., Mistry, H., Kariuki, N., & Park, J. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/abf4ab · Cited by 32 · cited 1×
“For example, in the representative Pt–Co alloying catalyst ink, applying a low EW ionomer causes more loss of Co and of lattice contraction compared to Nafion ionomer [184].”
Wu, R. F., Zhu, X., Liao, Q., Chen, R., & Cui, G. (2013) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2013.01.045 · Cited by 32 · cited 1×
“10b) (e.g., cracks and perforations as the liquid water pathway to the substrate layer, etc.) [144–149].”
Su, H.-N., Zeng, Q., Liao, S.-J., & Wu, Y.-N. (2010) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2010.06.070 · Cited by 31
Kumar, A., Hong, J., Yun, Y., Bhardwaj, A., & Song, S. (2020) · Journal of Materials Chemistry A · doi:10.1039/d0ta09397a · Cited by 31
Wang, M., Rome, G., Medina, S., Pfeilsticker, J. R., Kang, Z., Pylypenko, S., Ulsh, M., & Bender, G. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.228344 · Cited by 31 · cited 1×
“These defects include cracks, spots, and coating irregularities [218, 219].”
Ferrara, A., Polverino, P., & Pianese, C. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.04.005 · Cited by 31 · cited 1×
“The PFSA molecule is composed of a polytetrafluoroethylene (PTFE) main chain, perfluoroethylene side chain, and sulfonic acid group [72].”
Influence of Equivalent Weight of Ionomer on Proton Conduction Behavior in Fuel Cell Catalyst Layers
Shen, S., Han, A., Yan, X., Chen, J., Cheng, X., & Zhang, J. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0451912jes · Cited by 31 · cited 1×
“Usually, ionomers with lower equivalent weights (EWs) possess higher proton conductivity [183] but are sensitive to water.”
Self-citationTardy, E., Courtois, F., Chandesris, M., Poirot-Crouvezier, J.-P., Morin, A., & Bultel, Y. (2019) · International Journal of Heat and Mass Transfer · doi:10.1016/j.ijheatmasstransfer.2019.118720 · Cited by 30
Chen, Y., Singh, Y., Ramani, D., Orfino, F. P., Dutta, M., & Kjeang, E. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.230674 · Cited by 30 · cited 1×
“In this regard, the outer frames are employed to provide a firm and reliable MEA structure [4, 5] and are also used as seals.”
Main Cell Components, Material Properties, and Processes
Barbir, F. (2013) · PEM Fuel Cells · doi:10.1016/b978-0-12-387710-9.00004-7 · Cited by 30 · cited 1×
“Therefore, the GDL mainly serves the important functions of conducting electricity and heat and transporting reaction gases [115, 116].”
Manahan, M. P., Sr., Clement, J. T., Srouji, A.-K., Brown, S. W., Reutzel, E. W., & Mench, M. M. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0591410jes · Cited by 28
Zhao, N., Shi, Z., & Girard, F. (2021) · Materials · doi:10.3390/ma15010078 · Cited by 28 · cited 1×
“PFSA, especially under high-temperature and low-humidity working conditions [246].”
Water Management by Material Design and Engineering for PEM Fuel Cells
Nguyen, T. V. (2006) · ECS Transactions · doi:10.1149/1.2356236 · Cited by 28 · cited 1×
“In the pursuit of optimum PEM fuel cell performance, it is essential to optimize the GDL [108, 109, 124, 125].”
Liu, Y., Zhang, W., Han, G., Zhou, Y.-W., Li, L., Kong, F., Gao, Y., Du, C., Wang, J., Du, L., et al. (2021) · ACS Catalysis · doi:10.1021/acscatal.1c01680 · Cited by 27
Self-citationArcot, M. P., Zheng, K., McGrory, J., Fowler, M. W., & Pritzker, M. D. (2018) · International Journal of Energy Research · doi:10.1002/er.4107 · Cited by 27 · cited 1×
“20a), which also works for the characterization of membrane pinholes [196, 218].”
Yu, S., Li, X., Hao, J., Liu, S., Shao, Z., & Yi, B. (2014) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2014.07.062 · Cited by 25
Talukdar, K., Helmly, S., Schulze, M., Sánchez, D. G., Handl, M., Hiesgen, R., Kraut, J., & Friedrich, K. A. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.03.093 · Cited by 23
Moçotéguy, P., Ludwig, B., & Yousfi Steiner, N. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.10.078 · Cited by 23 · cited 1×
“2, the cathode reaction produces a large amount of water (especially under heavy working conditions), some of which is transferred through the PEM to the anode, while the rest of which needs to be efficiently exhausted through the GDL to the flow fields [120].”
Temperature-induced shear-thinning in catalyst inks
Yoshimune, W., & Harada, M. (2021) · Electrochemistry Communications · doi:10.1016/j.elecom.2021.107099 · Cited by 22 · cited 1×
“It is preferred to prepare the catalyst ink in an ice bath due to the shear-thinning behavior at elevated temperatures [188].”
Du, L., Kong, F., Chen, G., Du, C., Gao, Y., & Yin, G. (2016) · CHINESE JOURNAL OF CATALYSIS (CHINESE VERSION) · doi:10.1016/s1872-2067(16)62480-4 · Cited by 21
Self-citationSo, S., Kang, H., Choi, D., & Oh, K.-H. (2020) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2020.05.128 · Cited by 20 · cited 1×
“Reasonably, the decreased ionomer aggregation leads to a more homogeneous ionomer distribution in the catalyst layer, which can facilitate proton transfer at low relative humidity (RH) conditions [171].”
Influence of Ionomer Content in the Catalytic Layer of MEAs Based on Aquivion® Ionomer
Gatto, I., Saccà, A., Sebastián, D., Baglio, V., Aricò, A. S., Oldani, C., Merlo, L., & Carbone, A. (2021) · Polymers · doi:10.3390/polym13213832 · Cited by 19 · cited 1×
“The MEA with a moderate ionomer content of ~ 26 wt.% (wt.% means the weight percentage) shows the highest performance in terms of electrokinetic parameters, such as ECSA, suggesting balanced electronic and ionic percolation within the catalyst layer [181].”
Xing, Z., Xiao, M., Guo, Z., & Yang, W. (2018) · Chemical Communications · doi:10.1039/c8cc00846a · Cited by 19 · cited 1×
“In addition, metal-free catalysts, i.e., doped carbon matrices by heteroatoms such as N, S, O, and F, have also been studied [62–64].”
Predicting Membrane Lifetime with Cerium Oxide in Heavy Duty Fuel Cell Systems
Macauley, N., Lauritzen, M. V., Knights, S., & Kjeang, E. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0271810jes · Cited by 19 · cited 1×
“It has been reported (7) Anode: that when using cerium oxide as a radical scavenging agent within membranes, the working lifespan is much longer than that of the reference membrane under accelerated durability test conditions [96–98].”
Gollasch, M., Müller-Hülstede, J., Schmies, H., Schonvogel, D., Wagner, P., Dyck, A., & Wark, M. (2021) · Catalysts · doi:10.3390/catal11070841 · Cited by 19 · cited 1×
“C [53, 54].”
Tailoring Carbon Nanotube Microsphere Architectures with Controlled Porosity
Zhang, Z., Sadeghi, M. A., Jervis, R., Ye, S., Gostick, J. T., Barralet, J. E., & Merle, G. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201903983 · Cited by 19 · cited 1×
“Meanwhile, the drying step is helpful in removing solvents in catalyst layers and enhancing cell performance [209].”
Self-citationNovel catalysts, catalysts support and catalysts coated membrane methods
Debe, M. K. (2010) · Handbook of Fuel Cells · doi:10.1002/9780470974001.f303050 · Cited by 19 · cited 1×
“The NSTF electrode is an ultrathin electrode covered with a continuous thin Pt or Pt alloy catalyst [264], where the support is a crystalline organic pigment material (namely, nanowhiskers) [265].”
Optimum condition of membrane electrode assembly fabrication for PEM fuel cells
Nakrumpai, B., Pruksathorn, K., & Piumsomboon, P. (2006) · Korean Journal of Chemical Engineering · doi:10.1007/bf02706796 · Cited by 18
Composite Carbon Nanotube Microsphere Coatings for Use as Electrode Supports
Fraser, A., Zhang, Z., Merle, G., Gbureck, U., Ye, S., Gostick, J., & Barralet, J. (2018) · Advanced Functional Materials · doi:10.1002/adfm.201803713 · Cited by 17 · cited 1×
“We highlight the current status that the excellent performance of key materials, particularly the catalyst, cannot be completely reproduced when they are integrated into an MEA, especially when the Pt loading is low [248].”
Self-citationLiu, Y., Zhang, W., Han, G., Zhou, Y.-W., Li, L., Kang, C., Kong, F., Gao, Y., Du, C., Wang, J., et al. (2022) · Catalysis Science & Technology · doi:10.1039/d2cy00141a · Cited by 17
Self-citationIncreased Performance of PEFCs with Engineered Mass-Transport Pathways
Manahan, M., & Mench, M. (2011) · ECS Transactions · doi:10.1149/1.3635590 · Cited by 16
High performance proton exchange membrane fuel cell electrode assemblies
Yang, T.-F., Hourng, L.-W., Yu, T. L., Chi, P.-H., & Su, A. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.04.063 · Cited by 16 · cited 2×
“Therefore, this issue is potentially addressed by not only preparing well-defined catalyst ink (discussed above) but also constructing well-defined three-phase boundaries (discussed below) to increase the catalyst utilization rate in the catalyst layer [249].”
Chen, J., Jiang, X., Tang, W., Ma, L., Li, Y., Huang, Y., & Yin, Z. (2019) · Proceedings of the Institution of Mechanical Engineers Part B Journal of Engineering Manufacture · doi:10.1177/0954405419862090 · Cited by 15 · cited 1×
“22c [232] illustrate the R2R design for “seal lamination” and “GDL overlay”, respectively.”
Self-citationIto, H., Ishikawa, T., Ishida, M., Someya, S., & Munakata, T. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0051915jes · Cited by 14
Han, Y., Yin, S., Chen, Y., Chen, C., Yan, W., Cheng, X., Li, Y., Zhang, T., Yang, J., Jiang, Y., et al. (2022) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2022.116322 · Cited by 14 · cited 1×
“C [53, 54].”
Wan, Y. F., Qiu, D., Yi, P., Peng, L., & Lai, X. (2021) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2021.08.204 · Cited by 12 · cited 1×
“In this configuration, binders cohering to the frame are applied [6–9].”
Pt/C-TiO2 as Oxygen Reduction Electrocatalysts against Sulfur Poisoning
Liu, Y., Ye, J., Kong, F., Du, C., Zuo, P., Du, L., & Yin, G. (2022) · Catalysts · doi:10.3390/catal12050571 · Cited by 10 · cited 1×
“Moreover, catalysts suffer from less CO-induced degradation at high temperatures [80–83].”
Self-citationYang, J., Hübner, R., Zhang, J., Wan, H., Zheng, Y., Wang, H., Qi, H., He, L., Li, Y., Dubale, A. A., et al. (2021) · Angewandte Chemie · doi:10.1002/ange.202015679 · Cited by 10
Advanced materials for improved PEMFC performance and life
Curtin, D. E., Lousenberg, R. D., Henry, T. J., Tangeman, P. C., & Tisack, M. E. (2005) · Elsevier eBooks · doi:10.1016/b978-008044696-7/50053-2 · Cited by 10
Koga, M., Matsumoto, H., Tokita, M., Masunaga, H., Hikima, T., Sugimori, H., Sasabe, T., Yoshida, T., Shinohara, K., & Hirai, S. (2018) · ECS Transactions · doi:10.1149/08613.0157ecst · Cited by 9 · cited 1×
“Pt/C catalysts generate aggregates during the drying process until the catalyst layer is completely dried [211].”
Communication—Investigation of catalyst ink degradation by X-ray CT
Uemura, S., Kameya, Y., Iriguchi, N., Yoshida, T., Shinohara, K., & Hirai, S. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0411803jes · Cited by 9 · cited 1×
“For example, analytical centrifugation (AC) is a nondestructive technique to study particle migration behavior [166]; X-ray computed tomography (CT) is also useful in observing the interior changes of catalyst ink over time [190].”
Slot-Die Coating: A New Preparation Method for Direct Methanol Fuel Cells Catalyst Layers
Glüsen, A., Müller, M., & Stolten, D. (2013) · Journal of Fuel Cell Science and Technology · doi:10.1115/1.4024607 · Cited by 8 · cited 1×
“[206].”
Engineering a Membrane Electrode Assembly
Weidner, J. W., Sethuraman, V. A., & Zee, J. W. V. (2003) · The Electrochemical Society Interface · doi:10.1149/2.f07034if · Cited by 7
Guan, S., Zhou, F., Du, S., & Pan, M. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac44bd · Cited by 6 · cited 1×
“It should be noted that rolling can increase the contact area between the catalyst layer and PEM, thus reducing the contact resistance [242].”
Impact of CeOx Additives on Cathode Catalyst Layer Poisoning
Banham, D., Ye, S., Cheng, T., Knights, S., Stewart, S. M., & Garzon, F. H. (2013) · ECS Transactions · doi:10.1149/05801.0369ecst · Cited by 5 · cited 1×
“The grafting of free radical scavengers and organic antioxidants can help polymer membranes obtain superior chemical stability and maintain proton conductivities [94, 95].”
Self-citationSabli, N., Abu Bakar, N. A., Izhar, S., & Hilal, H. S. (2019) · Sains Malaysiana · doi:10.17576/jsm-2019-4804-20 · Cited by 5 · cited 1×
“However, high boiling point solvents require higher temperatures for drying, presenting higher toxicity and leading to severe swelling of the PEM [178].”
Influence of Triple MPL Coated GDL on the PEFC Performance under Low and High Humidity
Kitahara, T., Nakajima, H., Inamoto, M., & Shinto, K. (2013) · ECS Transactions · doi:10.1149/05801.1401ecst · Cited by 4 · cited 1×
“10a) [134–138], (4) MPLs with multiple hydrophilic and hydrophobic layers [139–143], and (5) modifications of MPL structures (Fig.”
Devaraj, V., Lopez, L. F., Beaman, J. J., & Prudhomme, S. (2015) · International Journal of Chemical Engineering · doi:10.1155/2015/572983 · Cited by 1 · cited 2×
“If these two measures can be suitably combined, additional postproduction quality control steps may be eliminated [233].”
Carbon-based metal-free oxygen reduction reaction electrocatalysts: Past, present and future
An, F., Bao, X., Deng, X., Zi-zai, M. A., & Xiao-guang, W. A. N. G. (2022) · Carbon · doi:10.1016/j.carbon.2022.04.053 · Cited by 1
Effect of Sub-Freezing Temperature on a PEM Fuel Cell
Yan, Q., & Toghiani, H. (2006) · ASME International Conference on Fuel Cell Science, Engineering and Technology (FuelCell) · doi:10.1115/fuelcell2006-97162
(Invited) Catalyst Layer Interactions That Affect Coatability
Dixit, M. B., Harkey, B., Shen, F., & Hatzell, K. B. (2018) · ECS Meeting Abstracts · doi:10.1149/ma2018-02/41/1392
Han, Y., Yin, S., Chen, Y., et al. (2021) · doi:10.2139/ssrn.3946129
Catalyst Poisoning Property of Sulfonimide Acid Ionomer On Pt (111) Surface
Kodama, K., Shinohara, A., Hasegawa, N., Shinozaki, K., Jinnouchi, R., Suzuki, T., Hatanaka, T., & Morimoto, Y. (2013) · ECS Meeting Abstracts · doi:10.1149/ma2013-02/15/1300
Influence of Triple MPL Coated GDL on the PEFC Performance under Low and High Humidity
Kitahara, T., Nakajima, H., Inamoto, M., & Shinto, K. (2013) · ECS Meeting Abstracts · doi:10.1149/ma2013-02/15/1545
ChemInform Abstract: Advances in the High Performance Polymer Electrolyte Membranes for Fuel Cells
Zhang, H., & Shen, P. K. (2012) · ChemInform · doi:10.1002/chin.201224279
Protonated Phosphonic Acid Electrodes for High Power Heavy-Duty Vehicle Fuel Cells
Lim, K., Lee, A., Atanasov, V., Kerres, J., Adhikari, S., Maurya, S., Park, E. J., Delfin, L., Jung, J., Cy, F., et al. (2021) · doi:10.21203/rs.3.rs-542999/v1
Manahan, M. P., Clement, J. T., Srouji, A. K., Brown, S. W., Reutzel, T., & Mench, M. M. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0461412jes
Guccini, V., Carlson, A., Yu, S., Lindbergh, G., Lindström, R. W., & Salazar-Alvarez, G. (2019) · doi:10.26434/chemrxiv.7851461.v3
Research works printed but not linked: 1
- Jie, N.: Investigation of the colloidal behaviour of carbon black and perfluorosulfonated ionomer in various solvents. Dissertation, Queen’s University (2016). http://hdl.handle.net/1974/14081.
Cited by
Oxygen- and proton-transporting open framework ionomer for medium-temperature fuel cells
Yang, J., Xu, H., Li, J., Gong, K., Yue, F., Han, X., Wu, K., Shao, P., Fu, Q., Zhu, Y., et al. (2024) · Science · doi:10.1126/science.adq2259 · Cited by 237
Bin, S., Chen, Z., Zhu, Y., Zhang, Y., Xia, Y., Gong, S., Zhang, F., Shi, L., Duan, X., & Sun, Z. (2024) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2024.04.188 · Cited by 133
Zhao, C., Ding, Z., Zhang, K., Du, Z., Fang, H., Chen, L., Jiang, H., Wang, M., & Wu, M. (2025) · Nano-Micro Letters · doi:10.1007/s40820-025-01653-z · Cited by 136
“In contrast, the proton exchange membrane (PEM) elec-trolyzers [136, 137], which conduct protons, are more vulnerable to corrosion in chloride-rich environments due to potential Cl − infiltration that compromises membrane integrity [138].”
Celadon, A., Sun, H., Sun, S., & Zhang, G. (2024) · SusMat · doi:10.1002/sus2.234 · Cited by 122
“187 The penultimate challenge highlights the potential for recycling batteries to foster a new local economy, benefiting states through increased tax revenues, providing jobs for workers, and reducing transportation costs for materials.”
Lei, H., Yang, X., Chen, Z., Rawach, D., Du, L., Liang, Z., Li, D., Zhang, G., Tavares, A. C., & Sun, S. (2025) · Advanced Materials · doi:10.1002/adma.202410106 · Cited by 121
Self-citation
Metadata
- Authors
- Mo, S., Du, L., Huang, Z., Chen, J., Zhou, Y., Wu, P., Meng, L., Wang, N., Xing, L., Zhao, M., Yang, Y., Tang, J., Zou, Y., & Ye, S.
- Affiliations
- Guangzhou University (CN)
- Corresponding author
- Xing, Lixin
- Ye, Siyu
- Venue
- Electrochemical Energy Reviews
- Published
- 2023-08-17
- Volume
- 6
- Issue
- 1
- ISSN
- 2520-8136 (ISSN-L)
- 2520-8489
- OpenAlex
- W4385950481
- Semantic Scholar
- c0da1c409a6ea52ab5ae981dd027dfa5bbc1427c
- Cited by
- 277
- References
- 267
- Citations by year
- 2026: 82 · 2025: 119 · 2024: 75 · 2023: 1
- FWCI
- 20.53
- Type
- journal article
- Language
- en
- Open access
- hybrid
- doi.org
- Licence
- cc-by
- creativecommons.org/licenses/by/4.0 (tdm)
- creativecommons.org/licenses/by/4.0 (vor)
- Locations
- Electrochemical Energy Reviews (publishedVersion, cc-by)
- Funders
- National Key Research and Development Program of China (2020YFB1505800)
- National Natural Science Foundation of China (22250710133, 51803042)
- Outstanding Youth Project of Natural Science Foundation of Guangdong Province (2022B1515020020)
- Funding by Science and Technology Projects in Guangzhou (202206050003, 202201010603)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
- Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
- Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
- Keywords
- proton exchange membrane fuel cells, membrane electrode assembly, fuel cell materials, fuel cell manufacturing, fuel cell lifetime, fuel cell cost, electrode materials, fuel cell vehicles
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
The claim verdicts this report counts are experimental: their accuracy is not yet measured.
A language model drew the claims from the paper on 2026-10-10, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).
A second model labelled each claim on 2026-10-10 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).
Cited sources are checked with a language model’s help (gpt-6-sol and qwen3.8-omni-flash).
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.