Abstract
This review focuses on biodegradable synthetic polymers, discussing synthesis, properties and biodegradability, especially within the polyester family including polylactides.
Overview
CoChat Summary
TL;DR
This review surveys biodegradable synthetic polymers for tissue engineering, emphasizing polyesters (PGA, PLA, PLGA), polylactones, poly(propylene fumarate), polyanhydrides, tyrosine-derived polycarbonates, polyorthoesters, polyurethanes, and polyphosphazenes. It concludes that polyesters dominate clinically, while injectable in situ curable systems such as PPF and photocrosslinkable polyanhydrides are promising but face challenges in biocompatibility, degradation control, and heat generation.
Key findings
- Polyesters are the most studied biodegradable polymers. PGA has 46–50% crystallinity, Tg 36°C, Tm 225°C; in Dexon sutures in vitro, first-stage degradation predominates for 21 days, crystalline degradation takes a further 28 days, and after 49 days weight loss was about 42% with complete loss of mechanical properties.
- PLA/PGA copolymer behavior depends on composition: 25–75% (l)LA/GA and 0–70% (dl)LA/GA are amorphous; 70/30 GA/LA has the highest water uptake, while 50/50 is reported as most unstable to hydrolysis; Vicryl is 8% (l)LA and 92% GA.
- Poly(caprolactone) degrades slowly: homopolymer degradation is on the order of 2–3 years, and PCL with initial average molecular weight 50,000 takes about 3 years for complete in vitro degradation.
- Poly(propylene fumarate) degrades to fumaric acid and propylene glycol; time to 20% original weight loss ranged from 84 days (PPF/β-TCP composite) to over 200 days (PPF/CaSO4 composite). PPF formulations showed maximum curing temperatures of 38–48°C versus 94°C for PMMA cements, curing times of 1–121 min, and compressive strengths of 1–12 MPa.
- Polyanhydrides degrade by surface erosion; poly(sebacic acid) degrades in about 54 days in saline, while poly(1,6-bis(p-carboxyphenoxy)hexane) is estimated at 1 year. Poly[1,6-bis(carboxyphenoxy)hexane] has a Young’s modulus of 1.3 MPa versus human bone at 40–60 MPa; poly(anhydride-co-imides) reached compressive strengths of 50–60 MPa, and photocrosslinked systems showed compressive strengths of 30–40 MPa and tensile strengths of 15–27 MPa.
- Degradable polyurethanes based on lysine diisocyanate showed varied properties: dl-lactide networks were rigid (Tg = 60°C) with ultimate tensile strengths of ~40–70 MPa, caprolactone triol networks were low-modulus elastomers with tensile strengths of 1–4 MPa, and copolymer networks had elongation up to 600% with compressive strengths of 3–25 MPa. In vivo, porous polyurethane artificial skin degraded almost completely 4–8 weeks after implantation in guinea pigs with no adverse tissue reaction.
Methods
- Design: narrative literature review; no primary experimental study or systematic review protocol is reported.
- Data/sample: published literature on biodegradable synthetic polymers, including synthesis, properties, degradation, biocompatibility, and injectable polymer systems; Tables 1–3 summarize polymer properties and precursors.
- Analysis: qualitative synthesis of major polymer classes, their degradation modes/products, mechanical properties, biocompatibility, and potential for injectable tissue-engineering compositions.
Limitations
- Stated: the paper notes that Table 2 data “should be used as a guide only” and that sufficient data are not available to provide a comprehensive list of properties for polyanhydrides, polycarbonates, polyurethanes, and polyphosphazenes.
- Stated: for polyanhydrides, no data are reported about polymer sterilizability and heat generation during polymerization; for degradable polyurethanes, the effect of degradation products and how they are removed from the body are not clearly understood.
- Evident: as a narrative review, it lacks systematic search criteria, study quality appraisal, and meta-analysis, so conclusions depend on the cited literature and may not comprehensively cover all biodegradable polymers or tissue-engineering applications.
Model-written summary. Check it against the paper before relying on it.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
1 Valid · 20 Not valid · 105 Not checked · 89 Own results and interpretations
Every source the paper cites for this claim was checked and supports it.
In the paper
“A meniscal replica implanted contained only fibro-cartilage after 18 weeks and decreased the degradation of the articular cartilage.”
What the sources say
- Supportedcites De Groot et al.., 1996 source
The Aliphatic PU network passage (page not provided) reports that articular-cartilage degeneration was less severe with the prosthesis than in meniscectomized control knees. It also says the prostheses contained only fibrocartilage after 18 weeks. Degeneration was reduced, not eliminated. (LLM, conf=0.91)
plainstates a causeSingle case- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Supported
In the paper
“The compressive strengths varied between 1 and 12 MPa”
What the sources say
- Not matchedcites Peter et al., 1998a
Couldn’t be matched to a paper in Crossref, so it can’t be checked.
plain- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Not matched
In the paper
“Cross-linking characteristics reported for PPF, N-vinyl pyrrolidone (N-VP), benzoyl peroxide, sodium chloride, and TCP indicate that for a range of formulations, the maximum temperature varied within 38 to about 48ºC, compared to 94ºC observed for polymethylmethacrylate (PMMA) cements.”
What the sources say
- Not matchedcites Peter et al., 1998a
Couldn’t be matched to a paper in Crossref, so it can’t be checked.
hedged- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Not matched
None of the sources cited for this claim could be matched to a paper in Crossref, so there is nothing to check it against.
In the paper
“Based on in-vitro studies, the time required to reach 20% loss in original weight ranged from 84 (PPF/ß-TCP composite) to over 200 days (PPF/CaSO 4 composite)”
What the sources say
- Not matchedcites Peter et al., 1997b
Couldn’t be matched to a paper in Crossref, so it can’t be checked.
- Not matchedcites Kharas et al., 1997
Couldn’t be matched to a paper in Crossref, so it can’t be checked.
plainstates an association- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Not matched
A result the paper states — it cites no source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“These composite materials exhibit compressive strengths in the range 2 to 30 MPa.”
plain- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
94 more claims
Create a free account to see all 215 claims and to verify the 2 references still open.
- It may state two separate claims as one. 62
- Probably not a substantial claim. 76
- The quote only partly states this claim. 1
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“Advantages include a tightly controlled manufacturing process, accurate reproducibility, adjustable biodegradability, and a wide variety of both chemical and physical properties.[ 171 ]”
From Unraveling and Harnessing the Immune Response at the Cell–Biomaterial Interface for Tissue Engineering Purposes (2024) · cites this paper as [171]
Experimental — accuracy not yet measured
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
Each contradiction between two passages listed here was confirmed by an independent check.
Rated major: it would touch a result — a value a result rests on, reported and recomputed p-values on opposite sides of the significance level, two passages that conflict with no sign which is right, or a cited work retracted before this paper was published.
In the paper
§ Polyanhydrides
“Polyanhydrides degrades by surface erosion (Kohn and Langer, 1997) and their main applications are in controlled drug delivery.”
§ Conclusions
“Polyanhydride degrade by bulk erosion and their main applications are in controlled drug delivery.”
Citations
Cites
Synthetic biodegradable polymers as orthopedic devices
Middleton, J. C., & Tipton, A. J. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00101-0 · Cited by 2,741 · cited 4×
“…developments in siloxane-based polyurethanes, which have greater in-vivo stability than conventional polyetherurethanes (e.g., poly(tetramethylene oxide) (PTMO)-based) have provided opportunities for development of a range of medical implants for chronic applications (Gunatillake et al., 2001).”
BackgroundInfluentialBiomaterial developments for bone tissue engineering
Burg, K. J. L., Porter, S., & Kellam, J. F. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00102-2 · Cited by 1,643 · cited 1×
“Polyesters have also been considered for development of tissue engineering applications (Hubbell, 1995; Thomson et al 1995a, Yazemski et al. 1996; Wong and Mooney, 1997), particularly for bone tissue engineering (Kohn and Langer, 1997; Burg et al., 2000).”
BackgroundChandra, R. (1998) · Progress in Polymer Science · doi:10.1016/s0079-6700(97)00039-7 · Cited by 1,462
Biodegradable polymers for use in surgery—polyglycolic/poly(actic acid) homo- and copolymers: 1
Gilding, D. K., & Reed, A. M. (1979) · Polymer · doi:10.1016/0032-3861(79)90009-0 · Cited by 1,345
Biomaterials in Tissue Engineering
Hubbell, J. A. (1995) · Nature Biotechnology · doi:10.1038/nbt0695-565 · Cited by 1,060 · cited 1×
“Polyesters have also been considered for development of tissue engineering applications (Hubbell, 1995; Thomson et al 1995a, Yazemski et al. 1996; Wong and Mooney, 1997), particularly for bone tissue engineering (Kohn and Langer, 1997; Burg et al., 2000).”
BackgroundPolylactic Acid for Surgical Implants
KULKARNI, R. K. (1966) · Archives of Surgery · doi:10.1001/archsurg.1966.01330050143023 · Cited by 841
Evolution of bone transplantation: molecular, cellular and tissue strategies to engineer human bone
Yaszemski, M. J., Payne, R. G., Hayes, W. C., Langer, R., & Mikos, A. G. (1996) · Biomaterials · doi:10.1016/0142-9612(96)85762-0 · Cited by 729
Miller, R. A., Brady, J. M., & Cutright, D. E. (1977) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820110507 · Cited by 722 · cited 2×
“For the (l)LA/GA copolymers, resistance to hydrolysis is more pronounced at either end of the copolymers compositions range (Miller et al., 1977; Gilding and Reed, 1979; Reed and Gilding, 1981; Vert et al., 1984).”
BackgroundInjectable biodegradable materials for orthopedic tissue engineering
Temenoff, J. S., & Mikos, A. G. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00108-3 · Cited by 554 · cited 8×
“A number of methods have been reported to prepare PPF, and each results in different polymer properties (Peter et al., 1997a,b, 1999; Temenoff and Mikos 2000).”
BackgroundMethodInfluentialLeong, K. W., Brott, B. C., & Langer, R. (1985) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820190806 · Cited by 541 · cited 12×
“The polyurethanes ranged from elastomers with elongations at break as high as 780 %, but with low tensile strengths (5.8 to 8.1 MPa).”
BackgroundInfluential
Research works printed but not linked: 5
- Scranton A, Bowman C, Peiffer R, eds. ACS Symposium Series 673; American Chemical Society, Washington DC. pp 189-202.
- Ratner BD, Hoffman AS, Schoen FJ, Lemon JE, eds. Aca- demic Press, San Diego. pp 65-73.
- Lamba NMK, Woodhouse KA, Cooper SL (1998) Poly- urethanes in Biomedical Applications. CRC Press: New York p 205-241.
- Mark JE, Alcock HR, West R (1992) Inorganic Poly- mers. Prentice Hall, Upper Saddle River, NJ. Chapter
- Ng SY, Vandamme T, Tayler MS, Heller J (1997) Syn- thesis and erosion studies of self-catalysed poly(orthoester)s. Macromolecules 30: 770-772.
Cited by
Items 301–400 of 1,762
Biodegradable and radically polymerized elastomers with enhanced processing capabilities
Ifkovits, J. L., Padera, R. F., & Burdick, J. A. (2008) · Biomedical Materials · doi:10.1088/1748-6041/3/3/034104 · Cited by 75
Li, Y., Dånmark, S., Edlund, U., Finne‐Wistrand, A., He, X., Norgård, M., Blomén, E., Hultenby, K. R., Andersson, G., & Lindgren, U. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2010.09.008 · Cited by 78
A degradable, porous, emulsion‐templated polyacrylate
Lumelsky, Y., Michael, I., Levenberg, S., & Silverstein, M. S. (2009) · Journal of Polymer Science Part A Polymer Chemistry · doi:10.1002/pola.23744 · Cited by 82
Kidney diseases and tissue engineering
Moon, K. H., Ko, I. K., Yoo, J. J., & Atala, A. (2015) · Methods · doi:10.1016/j.ymeth.2015.06.020 · Cited by 79
Nano-enabled delivery of diverse payloads across complex biological barriers
Ross, K. A., Brenza, T. M., Binnebose, A. M., Phanse, Y., Kanthasamy, A. G., Gendelman, H. E., Salem, A. K., Bartholomay, L. C., Bellaire, B. H., & Narasimhan, B. (2015) · Journal of Controlled Release · doi:10.1016/j.jconrel.2015.08.039 · Cited by 74
“One of their most important properties is their low cytotoxicity attributable to their rapid degradation into metabolites that are quickly processed by cells [95].”
BackgroundMigration of “bioabsorbable” screws in ACL repair. How much do we know? A systematic review
Pereira, H., Correlo, V. M., Silva‐Correia, J., Oliveira, J. M., Reis, R. L., & Espregueira‐Mendes, J. (2013) · Knee Surgery Sports Traumatology Arthroscopy · doi:10.1007/s00167-013-2414-2 · Cited by 77
“When exposed to physiological conditions, polyglycolide is degraded by random hydrolysis, and apparently it is also broken down by some enzymes, particularly those with esterase activity [17].”
BackgroundA study on the rate of degradation of the bioabsorbable polymer polyglycolic acid (PGA)
Shawe, S., Buchanan, F., Harkin‐Jones, E., & Farrar, D. F. (2006) · Journal of Materials Science · doi:10.1007/s10853-006-0064-1 · Cited by 72
Gravel, M., Gross, T., Vago, R., & Tabrizian, M. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2005.10.020 · Cited by 73
Biomatrices for bladder reconstruction
Lin, H., Madihally, S. V., Palmer, B. W., Frimberger, D. C., Fung, K.-M. A., & Kropp, B. P. (2014) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2014.11.020 · Cited by 75
Chen, S., Wang, X., Xie, X., Zheng, L.-Z., Yao, D., Wang, D.-P., Leng, Y., Zhang, G., & Qin, L. (2012) · Acta Biomaterialia · doi:10.1016/j.actbio.2012.04.030 · Cited by 73
Ahn, J.-H., Kim, J. Y., Han, G., Kim, D., Cheon, K., Lee, H., Kim, H., Kim, Y., Jang, T., & Jung, H. (2021) · Additive manufacturing · doi:10.1016/j.addma.2021.101988 · Cited by 76
Hacker, M. C., Krieghoff, J., & Mikos, A. G. (2018) · Elsevier eBooks · doi:10.1016/b978-0-12-809880-6.00033-3 · Cited by 142
Recent Developments in Cyclic Acetal Biomaterials for Tissue Engineering Applications
Falco, E. E., Patel, M., & Fisher, J. P. (2008) · Pharmaceutical Research · doi:10.1007/s11095-008-9620-5 · Cited by 79
“Since the mechanical properties of polyanhydrides are generally modest, co-polymers and crosslinked polyanhydrides have been developed for bone tissue engineering applications ( 26 ,50).”
BackgroundMethodInfluentialMohammadrezaei, D., Golzar, H., Rad, M. R., Omidi, M., Rashedi, H., Yazdian, F. A., Khojasteh, A., & Tayebi, L. (2018) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.36422 · Cited by 72
Advancing Tissue Engineering by Using Electrospun Nanofibers
Ashammakhi, N. A., Halili, A. N., Nikkola, L., Wimpenny, I., & Yang, Y. (2008) · Regenerative Medicine · doi:10.2217/17460751.3.4.547 · Cited by 78
“Common methods for producing scaffolds include creation of polymer foams and engineering porous structures by using porogens, for example, salt leaching [4,5].”
MethodCurrent State of the Art in Myocardial Tissue Engineering
Giraud, M., Armbruster, C., Carrel, T. P., & Tevaearai, H. T. (2007) · Tissue Engineering · doi:10.1089/ten.2006.0110 · Cited by 69
“44 Major classes of polymers, such as polyester (PGA, PLA), and their copolymers and PCL have a long history as synthetic biodegradable materials in clinical application.”
Khan, M. U. A., Al-Arjan, W. S., Binkadem, M. S., et al. (2021) · Nanomaterials · doi:10.3390/nano11051319 · Cited by 68
“, polysaccharides, poly(-hydroxy ester), hydrogels, or thermoplastic elastomers) have been used as biomaterials for TE in the previous era [12,13].”
MethodA Review of Biopolymers’ Utility as Emulsion Stabilizers
Tamang, N., Shrestha, P., Khadka, B., Mondal, M. H., Saha, B., & Bhattarai, A. (2021) · Polymers · doi:10.3390/polym14010127 · Cited by 81
Fabrication and Application of Nanofibrous Scaffolds in Tissue Engineering
Li, W., & Tuan, R. S. (2009) · Current Protocols in Cell Biology · doi:10.1002/0471143030.cb2502s42 · Cited by 68
“Constructs cultured in a RWV bioreactor encounter low shear stress when the rotation speed of the culture chamber is set to balance the weight of the construct and the hydrodynamic force (Lappa, 2003).”
BackgroundBiomaterials Advances in Patches for Congenital Heart Defect Repair
Pok, S., & Jacot, J. G. (2011) · Journal of Cardiovascular Translational Research · doi:10.1007/s12265-011-9289-8 · Cited by 71
“Since PGA is a rigid thermoplastic material with high crystallinity, it has a high melting point of 225°C and low solubility in most organic solvents except highly fluorinated organic solvents such as hexafluoroisopropanol [74].”
McDonald, P. F., Lyons, J. G., Geever, L. M., & Higginbotham, C. L. (2009) · Journal of Materials Science · doi:10.1007/s10853-009-4080-9 · Cited by 73
ten Brink, T., Damanik, F., Rotmans, J. I., & Moroni, L. (2024) · Advanced Healthcare Materials · doi:10.1002/adhm.202301939 · Cited by 71
Biomaterials for Adhesion in Orthopedic Applications: A Review
Zaokari, Y., Persaud, A., & Ibrahim, A. (2020) · Engineered Regeneration · doi:10.1016/j.engreg.2020.07.002 · Cited by 97
Electrospinning of cellulose using ionic liquids: An overview on processing and applications
da Silva, B. A., Cunha, R. S., Valério, A., Noni, A. D., Hotza, D., & González, S. Y. G. (2021) · European Polymer Journal · doi:10.1016/j.eurpolymj.2021.110283 · Cited by 67
Morelli, S., Salerno, S., Holopainen, J., Ritala, M., & Bartolo, L. D. (2015) · Journal of Biotechnology · doi:10.1016/j.jbiotec.2015.03.023 · Cited by 68
Porous three-dimensional carbon nanotube scaffolds for tissue engineering
Lalwani, G., Gopalan, A., D’Agati, M. J., Sankaran, J. S., Judex, S., Qin, Y., & Sitharaman, B. (2015) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.35449 · Cited by 68
Thermogravimetric study for polyurethane materials for biomedical applications
Filip, D., Macocinschi, D., & Vlad, S. (2011) · Composites Part B Engineering · doi:10.1016/j.compositesb.2011.04.050 · Cited by 59
Nano‐Enabled Approaches for Stem Cell‐Based Cardiac Tissue Engineering
Kharaziha, M., Memic, A., Akbari, M., Brafman, D. A., & Nikkhah, M. (2016) · Advanced Healthcare Materials · doi:10.1002/adhm.201600088 · Cited by 66
Novel forsterite/polycaprolactone nanocomposite scaffold for tissue engineering applications
Diba, M., Fathi, M., & Kharaziha, M. (2011) · Materials Letters · doi:10.1016/j.matlet.2011.03.047 · Cited by 66
Porous Poly(ε-Caprolactone) Scaffolds for Retinal Pigment Epithelium Transplantation
McHugh, K. J., Tao, S. L., & Saint‐Geniez, M. (2014) · Investigative Ophthalmology & Visual Science · doi:10.1167/iovs.13-12833 · Cited by 73
Abukawa, H., Papadaki, M. E., Abulikemu, M., Leaf, J., Vacanti, J. P., Kaban, L. B., & Troulis, M. J. (2006) · Dental Clinics of North America · doi:10.1016/j.cden.2005.11.006 · Cited by 85
Johari, N., Khodaei, A., Samadikuchaksaraei, A., Reis, R. L., Kundu, S. C., & Moroni, L. (2022) · Acta Biomaterialia · doi:10.1016/j.actbio.2022.09.030 · Cited by 70
Biomimetic Collagen Nanofibrous Materials for Bone Tissue Engineering
Zheng, W., Zhang, W., & Jiang, X. (2010) · Advanced Engineering Materials · doi:10.1002/adem.200980087 · Cited by 69
Rapid prototyping fabrication of soft and oriented polyester scaffolds for axonal guidance
Kaplan, B., Merdler, U., Szklanny, A. A., Redenski, I., Guo, S., Bar-Mucha, Z., Michael, N., & Levenberg, S. (2020) · Biomaterials · doi:10.1016/j.biomaterials.2020.120062 · Cited by 70
Kasoju, N., & Bora, U. (2012) · Biomedical Materials · doi:10.1088/1748-6041/7/4/045004 · Cited by 64
Diban, N., Haimi, S. P., Bolhuis‐Versteeg, L. A. M., Teixeira, S., Miettinen, S., Poot, A. A., Grijpma, D. W., & Stamatialis, D. F. (2013) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.01.005 · Cited by 65
“PCL is a flexible material with a slow degradation rate, which helps to maintain the mechanical properties over the time necessary for tissue reconstruction [11].”
BackgroundPolysaccharide Nanosystems for Future Progress in Cardiovascular Pathologies
Silva, A., Letourneur, D., & Chauvierre, C. (2014) · Theranostics · doi:10.7150/thno.7688 · Cited by 70
“Even though, they still present poor biocompatibility, loss of mechanical properties during degradation and release of acidic degradation products.[9] Knowledge at the cellular and molecular levels has increased greatly.”
BackgroundStem cell differentiation on electrospun nanofibrous substrates for vascular tissue engineering
Jia, L., Prabhakaran, M. P., Qin, X., & Ramakrishna, S. (2013) · Materials Science and Engineering C · doi:10.1016/j.msec.2013.07.021 · Cited by 65
Sawadkar, P., Mohanakrishnan, J., Rajasekar, P., Rahmani, B., Kohli, N., Bozec, L., & García-Gareta, E. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b19715 · Cited by 62
Osteochondral Injury, Management and Tissue Engineering Approaches
Jacob, G., Shimomura, K., & Nakamura, N. (2020) · Frontiers in Cell and Developmental Biology · doi:10.3389/fcell.2020.580868 · Cited by 67
Zanetta, M., Quirici, N., Demarosi, F., Tanzi, M. C., Rimondini, L., & Farè, S. (2008) · Acta Biomaterialia · doi:10.1016/j.actbio.2008.12.003 · Cited by 70
Zhang, C. Y., Lu, H., Zhuang, Z., et al. (2010) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-010-4161-y · Cited by 62
“In this context there is an ongoing search in the field of bone repair for new biomaterials that are biocompatible, biodegradable to nontoxic products, osteoinductive, osteoconductive, and have composition and mechanical properties similar to natural bones [2–30].”
BackgroundAyyoob, M., & Kim, Y. J. (2018) · Polymers · doi:10.3390/polym10101132 · Cited by 62
Engineering of Functional Skeletal Tissues
Bronner, F., Mikos, A. G., & Farach‐Carson, M. C. (2007) · Springer eBooks · doi:10.1007/978-1-84628-366-6 · Cited by 71
“Although these properties are advantageous, the potential for the transmission of infectious diseases remains a great concern [1, 2, 4, 10, 12, 24, 26, 27, 32, 38, 49, 53].”
BackgroundMethodInfluentialNew application of three‐dimensional printing biomaterial in nasal reconstruction
Park, S. H., Yun, B. G., Won, J. Y., Yun, W. S., Shim, J. H., Lim, M. H., Kim, D. H., Baek, S. A., Alahmari, Y. D., Jeun, J. H., et al. (2017) · The Laryngoscope · doi:10.1002/lary.26400 · Cited by 64
“Longterm follow-up of these animals would be necessary to determine the outcome after complete resorption of the implant has occurred, which could be more than 2 years as previously reported.(26) Long-term results of PCL implants should be pursued in future clinical trials.”
BackgroundYe, K. Y., & Black, L. D. (2011) · Journal of Cardiovascular Translational Research · doi:10.1007/s12265-011-9303-1 · Cited by 67
“The polymer composition can be tailored to create mechanical strength and controllable degradation patterns [72].”
BackgroundPhenylalanine-Based Poly(ester urea): Synthesis, Characterization, and in vitro Degradation
Yu, J., Lin, F., Lin, P., Gao, Y., & Becker, M. L. (2014) · Macromolecules · doi:10.1021/ma401752b · Cited by 60
Horáková, J., Mikeš, P., Saman, A., Jenčová, V., Klapstova, A., Svarcova, T., Ackermann, M., Novotný, V., Suchý, T., & Lukáš, D. (2018) · Materials Science and Engineering C · doi:10.1016/j.msec.2018.06.041 · Cited by 66
Biomaterials for Regenerative Medicine: Historical Perspectives and Current Trends
Rahmati, M., Pennisi, C. P., Budd, E., Mobasheri, A., & Mozafari, M. (2018) · Advances in experimental medicine and biology · doi:10.1007/5584_2018_278 · Cited by 72
The emergence of transient electronic devices
Kang, S., Yin, L., & Bettinger, C. J. (2020) · MRS Bulletin · doi:10.1557/mrs.2020.19 · Cited by 65
Biomechanical study on implantable and interventional medical devices
Wang, L., Ding, X., Feng, W., Gao, Y., Zhao, S., & Fan, Y. (2021) · Acta Mechanica Sinica · doi:10.1007/s10409-021-01116-9 · Cited by 59
Production Technologies and Application of Polymer Composites in Engineering: A Review
Bukvić, M., Milojević, S., Gajević, S., Đorđević, M., & Stojаnović, B. (2025) · Polymers · doi:10.3390/polym17162187 · Cited by 82
“A wide variety of fiber-reinforced polymer composites are currently utilized in prosthetics, bone defect correction, and the manufacture of prostheses and sutures [150].”
Guarino, V., Lewandowska, M., Bil, M., Polak, B., & Ambrosio, L. (2010) · Composites Science and Technology · doi:10.1016/j.compscitech.2010.06.015 · Cited by 60
“PCL shows a remarkably slow degradation rate – from 6 months up to 3 years for its complete removal from the host body - as a function of the starting molecular weight [14][15].”
BackgroundIn vitro degradation of porous PLLA/pearl powder composite scaffolds
Liu, Y. S., Huang, Q., Kienzle, A., Müller, W. E. G., & Feng, Q. (2014) · Materials Science and Engineering C · doi:10.1016/j.msec.2014.02.007 · Cited by 61
Biocompatibility of Different Nerve Tubes
Stang, F. H., Keilhoff, G., & Fansa, H. (2009) · Materials · doi:10.3390/ma2041480 · Cited by 58
“Currently PGA and its copolymers (poly(lactic-co-glycolic acid) with lactic acid, poly(glycolide-co-caprolactone) with ε-caprolactone, and poly(glycolide-co-trimethylene carbonate) with trimethylene carbonate) are widely used as a material for tissue engineering or controlled drug delivery [11].”
BackgroundInfluentialKouser, S., Sheik, S., Nagaraja, G. K., Prabhu, A., Prashantha, K., D’Souza, J. N., Navada, M. K., & Manasa, D. J. (2020) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2020.09.188 · Cited by 60
Matricellular proteins and biomaterials
Morris, A. H., & Kyriakides, T. R. (2014) · Matrix Biology · doi:10.1016/j.matbio.2014.03.002 · Cited by 67
Zhu, J., Cao, L., Li, C., Zhao, G., Zhu, T., Hu, W., Sun, W., & Lu, Y. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b11703 · Cited by 58
Mozaffari, A., Gashti, M. P., Mirjalili, M., & Parsania, M. (2021) · Membranes · doi:10.3390/membranes11010031 · Cited by 61
“It was reported that tannic acid crosslinked nanofibers were not only able to maintain the physical structure in water, but they can also act as antioxidants with antimicrobial functionality against different microorganisms including bacteria, viruses and fungi [20].”
BackgroundFabrication of Tissue Engineering Scaffolds
Kramschuster, A., & Turng, L. (2012) · Elsevier eBooks · doi:10.1016/b978-1-4557-2834-3.00017-3 · Cited by 83
Ayyoob, M., Lee, D. H., Kim, J., Nam, S. W., & Kim, Y. J. (2017) · Fibers and Polymers · doi:10.1007/s12221-017-6889-1 · Cited by 61
Bose, S., Vu, A. A., Emshadi, K., & Bandyopadhyay, A. K. (2018) · Materials Science and Engineering C · doi:10.1016/j.msec.2018.02.019 · Cited by 60
Advances in Protein-Based Materials: From Origin to Novel Biomaterials
Choi, S. M., Chaudhry, P., Zo, S. M., & Han, S. S. (2018) · Advances in experimental medicine and biology · doi:10.1007/978-981-13-0950-2_10 · Cited by 67
Alemzadeh, E., Oryan, A., & Mohammadi, A. A. (2019) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.34411 · Cited by 59
Abazari, M. F., Soleimanifar, F., Faskhoudi, M. A., Mansour, R. N., Mahabadi, J. A., Sadeghi, S., Hassannia, H., Saburi, E., Enderami, S. E., Khani, M., et al. (2019) · Journal of Cellular Physiology · doi:10.1002/jcp.29029 · Cited by 63
“The use of synthetic polymers has been much more considered for bone tissue engineering due to their mechanical properties (Gunatillake & Adhikari, 2003).”
BackgroundA Biomimetic Macroporous Hybrid Scaffold with Sustained Drug Delivery for Enhanced Bone Regeneration
Lee, S. S., Santschi, M., & Ferguson, S. J. (2021) · Biomacromolecules · doi:10.1021/acs.biomac.1c00241 · Cited by 61
Nanoparticle-polymer composite scaffolds for bone tissue engineering. A review
Chimal, R. Á., Arenas-Alatorre, J. A., & Álvarez-Pérez, M. A. (2024) · European Polymer Journal · doi:10.1016/j.eurpolymj.2024.113093 · Cited by 70
A Novel Bioresorbable Implant for Repair of Orbital Floor Fractures
Teo, L., Teoh, S. H., Liu, Y., Lim, L. S., Tan, B., Schantz, J., & Seah, L. L. (2015) · Orbit · doi:10.3109/01676830.2015.1015263 · Cited by 59
“PCL implants have a long degradation time of more than 2 years.(21) This makes them ideal as bone implants as they degrade in tandem with neobone regeneration.”
BackgroundNeffe, A. T., Tronci, G., Alteheld, A., & Lendlein, A. (2009) · Macromolecular Chemistry and Physics · doi:10.1002/macp.200900441 · Cited by 62
Neut, D., Kluin, O. S., Crielaard, B. J., van der Mei, H. C., Busscher, H. J., & Grijpma, D. W. (2009) · Acta Orthopaedica · doi:10.3109/17453670903350040 · Cited by 59
“It has been suggested that acidic degradation products and a subsequent decrease in local pH are the cause of decreased bone regeneration (Gunatillake and Adhikari 2003).”
BackgroundMethodYuan, S., Xiong, G. M., Roguin, A., & Choong, C. S. N. (2012) · Biointerphases · doi:10.1007/s13758-012-0030-1 · Cited by 59
Biomaterials for bone tissue engineering: achievements to date and future directions
Garimella, A., Ghosh, S. B., & Ghosh, S. N. (2024) · Biomedical Materials · doi:10.1088/1748-605x/ad967c · Cited by 79
“Some of the examples of artificial or synthetic biopolymers that are exhaustively employed in bone implant materials are, poly-(glycolic acid) (PGA), poly-(vinyl alcohol) (PVA), poly-( ε -caprolactone) (PCL), poly-(lactic acid) (PLA), etc [43, 125–129].”
Development of tissue engineered vascular grafts and application of nanomedicine
Rathore, A., Cleary, M. A., Naito, Y., Rocco, K. A., & Breuer, C. K. (2012) · Wiley Interdisciplinary Reviews Nanomedicine and Nanobiotechnology · doi:10.1002/wnan.1166 · Cited by 66
Tissue engineering of oral mucosa: a shared concept with skin
Kınıkoğlu, B., Damour, O., & Hasırcı, V. (2014) · Journal of Artificial Organs · doi:10.1007/s10047-014-0798-5 · Cited by 65
“Synthetic polymers such as poly(glycolic acid) (PGA), poly(lactic acid) (PLA) and their copolymers (PLGA), poly(p-dioxanone) (PDO), and copolymers of trimethylene carbonate (TMC) are popular in tissue engineering because they allow the researcher to tailor the mechanical properties and the degradation kinetics to suit…”
BackgroundRecent developments in plant oil based functional materials
Mosiewicki, M. A., & Aranguren, M. I. (2015) · Polymer International · doi:10.1002/pi.5033 · Cited by 60
Ching, K. Y., Andriotis, O. G., Li, S., Basnett, P., Su, B., Roy, I., Tare, R. S., Sengers, B. G., & Stolz, M. (2016) · Journal of Biomaterials Applications · doi:10.1177/0885328216639749 · Cited by 63
“23 26 A major hurdle in the engineering of cartilage is the de-differentiation of chondrocytes when exposed to a synthetic microenvironment, 27 which often results in the development of calcified or fibrous cartilage.”
Biomaterials and Tissue Engineering
Lee, S. J., Yoo, J. J., & Atala, A. (2017) · Springer eBooks · doi:10.1007/978-981-10-2723-9_2 · Cited by 72
Jahani, H., Kaviani, S., Hassanpour-Ezatti, M., Soleimani, M., Kaviani, Z., & Zonoubi, Z. (2012) · PubMed Central · Cited by 74
Dermal substitute-assisted healing: enhancing stem cell therapy with novel biomaterial design
Hodgkinson, T., & Bayat, A. (2011) · Archives of Dermatological Research · doi:10.1007/s00403-011-1131-2 · Cited by 47
“polytetra Xuoroethylene (PTFE), polycaprolactone (PCL)[119], polyethylene terephthalate (PET), Poly(l-lactide) (PLLA)[169] and poly(ethyleneglycolterephthalate)poly(butylenes terephthalate) (PEGT/PBT) [21, 39], [157] Despite their ease of manipulation and manufacture, the safety of these materials remains a concern [5…”
BackgroundThe Importance of Biophysical and Biochemical Stimuli in Dynamic Skeletal Muscle Models
Maleiner, B., Tomasch, J., Heher, P., Spadiut, O., Rünzler, D., & Fuchs, C. (2018) · Frontiers in Physiology · doi:10.3389/fphys.2018.01130 · Cited by 63
Albarova, J. G., Salinas, A. J., Bueno-Lozano, A. L., et al. (2004) · Biomaterials · doi:10.1016/j.biomaterials.2004.11.006 · Cited by 56
“Scaffolds made from synthetic and natural polymers and ceramics have been investigated extensively for bone repair, including advantages such as the ability to generate porous structures, matching size, shape and mechanical properties for a variety of indications [35].”
BackgroundKokai, L. E., Tan, H., Jhunjhunwala, S., Little, S. R., Frank, J. W., & Marra, K. G. (2009) · Journal of Controlled Release · doi:10.1016/j.jconrel.2009.09.003 · Cited by 64
Li, F., Sun, J., Zhu, H., Wen, X., Lin, C., & Shi, D. (2011) · Colloids and Surfaces B Biointerfaces · doi:10.1016/j.colsurfb.2011.06.003 · Cited by 59
Near-infrared-labeled tetracycline derivative is an effective marker of bone deposition in mice
Kovar, J. L., Xu, X., Draney, D., Cupp, A. S., Simpson, M. A., & Olive, D. M. (2011) · Analytical Biochemistry · doi:10.1016/j.ab.2011.05.011 · Cited by 57
Lan, S.-F., Kehinde, T., Zhang, X., KHAJOTIA, S. S., Schmidtke, D. W., & Starly, B. (2013) · Dental Materials · doi:10.1016/j.dental.2013.03.014 · Cited by 65
Micro and nanotechnologies in heart valve tissue engineering
Hasan, A., Saliba, J., Modarres, H. P., Bakhaty, A. A., Nasajpour, A., Mofrad, M. R. K., & Sanati‐Nezhad, A. (2016) · Biomaterials · doi:10.1016/j.biomaterials.2016.07.001 · Cited by 58
Biotechnological production of bio-based long-chain dicarboxylic acids with oleogenious yeasts
Werner, N., & Zibek, S. (2017) · World Journal of Microbiology and Biotechnology · doi:10.1007/s11274-017-2360-0 · Cited by 56
Developing a Clinically Relevant Tissue Engineered Heart Valve—A Review of Current Approaches
Nachlas, A. L. Y., Li, S., & Davis, M. E. (2017) · Advanced Healthcare Materials · doi:10.1002/adhm.201700918 · Cited by 62
Yan, S., Xia, P., Xu, S., Zhang, K., Li, G., Cui, L., & Yin, J. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b02448 · Cited by 55
Constantinides, C., Basnett, P., Lukasiewicz, B., Carnicer, R., Swider, E., Majid, Q. A., Srinivas, M., Carr, C. A., & Roy, I. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b06096 · Cited by 57
Long-term release of fluocinolone acetonide using biodegradable fumarate-based polymers
Haesslein, A., Ueda, H., Hacker, M. C., Jo, S., Ammon, D. M., Borazjani, R. N., Künzler, J., Salamone, J. C., & Mikos, A. G. (2006) · Journal of Controlled Release · doi:10.1016/j.jconrel.2006.05.024 · Cited by 55
Degradable particulate composite reinforced with nanofibres for biomedical applications
Pinho, E. D., Martins, A. M., Araújo, J. V., et al. (2008) · Acta Biomaterialia · doi:10.1016/j.actbio.2008.11.018 · Cited by 54
“The polyester bonds of synthetic polymers are hydrolysed in nontoxic natural metabolites and are eliminated from the body by the normal physiological processes [29].”
BackgroundCaracciolo, P. C., Thomas, V., Vohra, Y. K., Buffa, F., & Abraham, G. A. (2009) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-009-3768-3 · Cited by 54
Regenerative implants for cardiovascular tissue engineering
Lee, A. Y., Mahler, N., Best, C. A., Lee, Y., & Breuer, C. K. (2014) · Translational research · doi:10.1016/j.trsl.2014.01.014 · Cited by 60
“Food and Drug Administration (FDA); however, individual approval of each new tissue engineering application is ultimately required before clinical implementation.(88,89,97,98) Recently, an innovative, rationally designed polymer, poly-glycerol sebacate (PGS), has been reported by Wang et al(100,101) to show promise in…”
BackgroundInfluentialEnabling nanomaterial, nanofabrication and cellular technologies for nanoneuromedicines
Mallapragada, S. K., Brenza, T. M., McMillan, J., Narasimhan, B., Sakaguchi, D. S., Sharma, A. D., Zbarska, S., & Gendelman, H. E. (2015) · Nanomedicine Nanotechnology Biology and Medicine · doi:10.1016/j.nano.2014.12.013 · Cited by 57
“Additionally, the preparation of polymers into nanoparticles is such that the therapeutic agent can be incorporated into the polymer matrix, coupling their release to polymer degradation kinetics.(25,26) Surface modifications can be performed either by altering the polymer prior to particle formation or by conjugation…”
Biodegradable Polyesters Derived from Amino Acids
Kolitz, M., Cohen-Arazi, N., Hagag, I., Katzhendler, J., & Domb, A. J. (2009) · Macromolecules · doi:10.1021/ma900464g · Cited by 54
Noriega, S. E., & Subramanian, A. (2011) · International Journal of Carbohydrate Chemistry · doi:10.1155/2011/809743 · Cited by 61
Biodegradable intestinal stents: A review
Wang, Z., Li, N., Li, R., Li, Y., & Ruan, L. (2014) · Progress in Natural Science Materials International · doi:10.1016/j.pnsc.2014.08.008 · Cited by 55
Synthesis, characterization and antibacterial activity of juglone encapsulated PLGA nanoparticles
Arasoğlu, T., Derman, S., Mansuroğlu, B., Yelkenci, G., KOÇYİĞİT, B., Gumus, B., Acar, T., & Kocaçalışkan, İ. (2017) · Journal of Applied Microbiology · doi:10.1111/jam.13601 · Cited by 56
“Because of its inert properties in physiological environment, which are biodegradability, biocompatibility and nontoxic degradation components, PLGA is one of the FDA approved biopolymers used frequently for drug delivery systems, and appropriate carrier to prepare nanoparticle systems with substances soluble in water…”
BackgroundIntervertebral disc tissue engineering: A brief review
Stergar, J., Gradišnik, L., Velnar, T., & Maver, U. (2019) · Bosnian Journal of Basic Medical Sciences · doi:10.17305/bjbms.2019.3778 · Cited by 63
“In addition to natural polymers and natural-polymer derived materials, biodegradable synthetic polymers are also utilized as scaffolds in tissue engineering [57,58].”
Metadata
- Authors
- CSIRO Molecular Science, B. 1., & Gunatillake, P.
- Corresponding author
- CSIRO Molecular Science, Bag 10, Clayton South MDC, Vic 3169, Australia
- Venue
- European Cells and Materials
- Publisher
- Forum Multimedia Publishing LLC
- Published
- 2003-10-01
- Volume
- 5
- Pages
- 1-16
- ISSN
- 1473-2262 (ISSN-L)
- OpenAlex
- W2106035984
- Cited by
- 1,765
- References
- 97
- Citations by year
- 2026: 43 · 2025: 61 · 2024: 59 · 2023: 80 · 2022: 90 · 2021: 112 · 2020: 102 · 2019: 115 · 2018: 105 · 2017: 128 · 2016: 110 · 2015: 106 · 2014: 110 · 2013: 91 · 2012: 86
- FWCI
- 1.32
- Type
- journal article
- Language
- en
- Open access
- gold
- doi.org
- Licence
- cc-by
- Locations
- European Cells and Materials (publishedVersion, cc-by)
- PubMed (publishedVersion)
- DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion)
- Topics
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
- Health Sciences › Medicine › Surgery › Surgical Sutures and Adhesives
- Keywords
- tissue engineering, polyesters, polyglycolic acid, polylactic acid, polyanhydrides, polyphosphazenes, polyurethane, poly(propylene fumarate), injectable polymers, orthopedic tissue engineering, biodegradation, biocompatibility, degradation products
- MeSH terms
- Biocompatible Materials, Models, Chemical, Polymers, Tissue Engineering
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
A language model drew the claims from the paper on 2026-10-10, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).
A second model labelled each claim on 2026-10-10 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).
Cited sources are checked with a language model’s help (gpt-6-sol).
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.