Biodegradable synthetic polymers for tissue engineering
Open accessThe DOI matches its Crossref record; 96 of the 97 references it cites were found in a registry or an index; 1 of the 146 sources its claims cite were checked for support.
Abstract
This review focuses on biodegradable synthetic polymers, discussing synthesis, properties and biodegradability, especially within the polyester family including polylactides.
Overview
CoChat Summary
TL;DR
This review surveys biodegradable synthetic polymers for tissue engineering, emphasizing polyesters (PGA, PLA, PLGA), polylactones, poly(propylene fumarate), polyanhydrides, tyrosine-derived polycarbonates, polyorthoesters, polyurethanes, and polyphosphazenes. It concludes that polyesters dominate clinically, while injectable in situ curable systems such as PPF and photocrosslinkable polyanhydrides are promising but face challenges in biocompatibility, degradation control, and heat generation.
Key findings
- Polyesters are the most studied biodegradable polymers. PGA has 46–50% crystallinity, Tg 36°C, Tm 225°C; in Dexon sutures in vitro, first-stage degradation predominates for 21 days, crystalline degradation takes a further 28 days, and after 49 days weight loss was about 42% with complete loss of mechanical properties.
- PLA/PGA copolymer behavior depends on composition: 25–75% (l)LA/GA and 0–70% (dl)LA/GA are amorphous; 70/30 GA/LA has the highest water uptake, while 50/50 is reported as most unstable to hydrolysis; Vicryl is 8% (l)LA and 92% GA.
- Poly(caprolactone) degrades slowly: homopolymer degradation is on the order of 2–3 years, and PCL with initial average molecular weight 50,000 takes about 3 years for complete in vitro degradation.
- Poly(propylene fumarate) degrades to fumaric acid and propylene glycol; time to 20% original weight loss ranged from 84 days (PPF/β-TCP composite) to over 200 days (PPF/CaSO4 composite). PPF formulations showed maximum curing temperatures of 38–48°C versus 94°C for PMMA cements, curing times of 1–121 min, and compressive strengths of 1–12 MPa.
- Polyanhydrides degrade by surface erosion; poly(sebacic acid) degrades in about 54 days in saline, while poly(1,6-bis(p-carboxyphenoxy)hexane) is estimated at 1 year. Poly[1,6-bis(carboxyphenoxy)hexane] has a Young’s modulus of 1.3 MPa versus human bone at 40–60 MPa; poly(anhydride-co-imides) reached compressive strengths of 50–60 MPa, and photocrosslinked systems showed compressive strengths of 30–40 MPa and tensile strengths of 15–27 MPa.
- Degradable polyurethanes based on lysine diisocyanate showed varied properties: dl-lactide networks were rigid (Tg = 60°C) with ultimate tensile strengths of ~40–70 MPa, caprolactone triol networks were low-modulus elastomers with tensile strengths of 1–4 MPa, and copolymer networks had elongation up to 600% with compressive strengths of 3–25 MPa. In vivo, porous polyurethane artificial skin degraded almost completely 4–8 weeks after implantation in guinea pigs with no adverse tissue reaction.
Methods
- Design: narrative literature review; no primary experimental study or systematic review protocol is reported.
- Data/sample: published literature on biodegradable synthetic polymers, including synthesis, properties, degradation, biocompatibility, and injectable polymer systems; Tables 1–3 summarize polymer properties and precursors.
- Analysis: qualitative synthesis of major polymer classes, their degradation modes/products, mechanical properties, biocompatibility, and potential for injectable tissue-engineering compositions.
Limitations
- Stated: the paper notes that Table 2 data “should be used as a guide only” and that sufficient data are not available to provide a comprehensive list of properties for polyanhydrides, polycarbonates, polyurethanes, and polyphosphazenes.
- Stated: for polyanhydrides, no data are reported about polymer sterilizability and heat generation during polymerization; for degradable polyurethanes, the effect of degradation products and how they are removed from the body are not clearly understood.
- Evident: as a narrative review, it lacks systematic search criteria, study quality appraisal, and meta-analysis, so conclusions depend on the cited literature and may not comprehensively cover all biodegradable polymers or tissue-engineering applications.
Model-written summary. Check it against the paper before relying on it.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
1 Valid · 20 Not valid · 105 Not checked · 89 Own results and interpretations
Every source the paper cites for this claim was checked and supports it.
In the paper
“A meniscal replica implanted contained only fibro-cartilage after 18 weeks and decreased the degradation of the articular cartilage.”
What the sources say
- Supportedcites De Groot et al.., 1996 source
The Aliphatic PU network passage (page not provided) reports that articular-cartilage degeneration was less severe with the prosthesis than in meniscectomized control knees. It also says the prostheses contained only fibrocartilage after 18 weeks. Degeneration was reduced, not eliminated. (LLM, conf=0.91)
plainstates a causeSingle case- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Supported
In the paper
“The compressive strengths varied between 1 and 12 MPa”
What the sources say
- Not matchedcites Peter et al., 1998a
Couldn’t be matched to a paper in Crossref, so it can’t be checked.
plain- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Not matched
In the paper
“Cross-linking characteristics reported for PPF, N-vinyl pyrrolidone (N-VP), benzoyl peroxide, sodium chloride, and TCP indicate that for a range of formulations, the maximum temperature varied within 38 to about 48ºC, compared to 94ºC observed for polymethylmethacrylate (PMMA) cements.”
What the sources say
- Not matchedcites Peter et al., 1998a
Couldn’t be matched to a paper in Crossref, so it can’t be checked.
hedged- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Not matched
None of the sources cited for this claim could be matched to a paper in Crossref, so there is nothing to check it against.
In the paper
“Based on in-vitro studies, the time required to reach 20% loss in original weight ranged from 84 (PPF/ß-TCP composite) to over 200 days (PPF/CaSO 4 composite)”
What the sources say
- Not matchedcites Peter et al., 1997b
Couldn’t be matched to a paper in Crossref, so it can’t be checked.
- Not matchedcites Kharas et al., 1997
Couldn’t be matched to a paper in Crossref, so it can’t be checked.
plainstates an association- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Not matched
A result the paper states — it cites no source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“These composite materials exhibit compressive strengths in the range 2 to 30 MPa.”
plain- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: unclear — It is unclear whether the paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
94 more claims
Create a free account to see all 215 claims and to verify the 2 references still open.
- It may state two separate claims as one. 62
- Probably not a substantial claim. 76
- The quote only partly states this claim. 1
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“Advantages include a tightly controlled manufacturing process, accurate reproducibility, adjustable biodegradability, and a wide variety of both chemical and physical properties.[ 171 ]”
From Unraveling and Harnessing the Immune Response at the Cell–Biomaterial Interface for Tissue Engineering Purposes (2024) · cites this paper as [171]
Experimental — accuracy not yet measured
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
Each contradiction between two passages listed here was confirmed by an independent check.
Rated major: it would touch a result — a value a result rests on, reported and recomputed p-values on opposite sides of the significance level, two passages that conflict with no sign which is right, or a cited work retracted before this paper was published.
In the paper
§ Polyanhydrides
“Polyanhydrides degrades by surface erosion (Kohn and Langer, 1997) and their main applications are in controlled drug delivery.”
§ Conclusions
“Polyanhydride degrade by bulk erosion and their main applications are in controlled drug delivery.”
Citations
Cites
Synthetic biodegradable polymers as orthopedic devices
Middleton, J. C., & Tipton, A. J. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00101-0 · Cited by 2,741 · cited 4×
“…developments in siloxane-based polyurethanes, which have greater in-vivo stability than conventional polyetherurethanes (e.g., poly(tetramethylene oxide) (PTMO)-based) have provided opportunities for development of a range of medical implants for chronic applications (Gunatillake et al., 2001).”
BackgroundInfluentialBiomaterial developments for bone tissue engineering
Burg, K. J. L., Porter, S., & Kellam, J. F. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00102-2 · Cited by 1,643 · cited 1×
“Polyesters have also been considered for development of tissue engineering applications (Hubbell, 1995; Thomson et al 1995a, Yazemski et al. 1996; Wong and Mooney, 1997), particularly for bone tissue engineering (Kohn and Langer, 1997; Burg et al., 2000).”
BackgroundChandra, R. (1998) · Progress in Polymer Science · doi:10.1016/s0079-6700(97)00039-7 · Cited by 1,462
Biodegradable polymers for use in surgery—polyglycolic/poly(actic acid) homo- and copolymers: 1
Gilding, D. K., & Reed, A. M. (1979) · Polymer · doi:10.1016/0032-3861(79)90009-0 · Cited by 1,345
Biomaterials in Tissue Engineering
Hubbell, J. A. (1995) · Nature Biotechnology · doi:10.1038/nbt0695-565 · Cited by 1,060 · cited 1×
“Polyesters have also been considered for development of tissue engineering applications (Hubbell, 1995; Thomson et al 1995a, Yazemski et al. 1996; Wong and Mooney, 1997), particularly for bone tissue engineering (Kohn and Langer, 1997; Burg et al., 2000).”
BackgroundPolylactic Acid for Surgical Implants
KULKARNI, R. K. (1966) · Archives of Surgery · doi:10.1001/archsurg.1966.01330050143023 · Cited by 841
Evolution of bone transplantation: molecular, cellular and tissue strategies to engineer human bone
Yaszemski, M. J., Payne, R. G., Hayes, W. C., Langer, R., & Mikos, A. G. (1996) · Biomaterials · doi:10.1016/0142-9612(96)85762-0 · Cited by 729
Miller, R. A., Brady, J. M., & Cutright, D. E. (1977) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820110507 · Cited by 722 · cited 2×
“For the (l)LA/GA copolymers, resistance to hydrolysis is more pronounced at either end of the copolymers compositions range (Miller et al., 1977; Gilding and Reed, 1979; Reed and Gilding, 1981; Vert et al., 1984).”
BackgroundInjectable biodegradable materials for orthopedic tissue engineering
Temenoff, J. S., & Mikos, A. G. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00108-3 · Cited by 554 · cited 8×
“A number of methods have been reported to prepare PPF, and each results in different polymer properties (Peter et al., 1997a,b, 1999; Temenoff and Mikos 2000).”
BackgroundMethodInfluentialLeong, K. W., Brott, B. C., & Langer, R. (1985) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820190806 · Cited by 541 · cited 12×
“The polyurethanes ranged from elastomers with elongations at break as high as 780 %, but with low tensile strengths (5.8 to 8.1 MPa).”
BackgroundInfluential
Research works printed but not linked: 5
- Scranton A, Bowman C, Peiffer R, eds. ACS Symposium Series 673; American Chemical Society, Washington DC. pp 189-202.
- Ratner BD, Hoffman AS, Schoen FJ, Lemon JE, eds. Aca- demic Press, San Diego. pp 65-73.
- Lamba NMK, Woodhouse KA, Cooper SL (1998) Poly- urethanes in Biomedical Applications. CRC Press: New York p 205-241.
- Mark JE, Alcock HR, West R (1992) Inorganic Poly- mers. Prentice Hall, Upper Saddle River, NJ. Chapter
- Ng SY, Vandamme T, Tayler MS, Heller J (1997) Syn- thesis and erosion studies of self-catalysed poly(orthoester)s. Macromolecules 30: 770-772.
Cited by
Items 201–300 of 1,762
Garkhal, K., Verma, S., Jonnalagadda, S., & Kumar, N. (2007) · Journal of Polymer Science Part A: Polymer Chemistry · doi:10.1002/pola.22031 · Cited by 110
Mathematical modeling of polymer erosion: Consequences for drug delivery
Sackett, C. K., & Narasimhan, B. (2010) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2010.11.048 · Cited by 131
PLA/PCL electrospun membranes of tailored fibres diameter as drug delivery systems
Herrero-Herrero, M., Gómez-Tejedor, J. A., & Vallés‐Lluch, A. (2018) · European Polymer Journal · doi:10.1016/j.eurpolymj.2017.12.045 · Cited by 120
Sutthiwanjampa, C., Hong, S., Kim, W. J., Kang, S. H., & Park, H. (2023) · Advanced Materials Interfaces · doi:10.1002/admi.202202333 · Cited by 121
Salerno, A., Guarnieri, D., Iannone, M., Zeppetelli, S., & Netti, P. A. (2010) · Tissue Engineering Part A · doi:10.1089/ten.tea.2009.0494 · Cited by 111
Metathesis of unsaturated fatty acids: Synthesis of long‐chain unsaturated‐α,ω‐dicarboxylic acids
Ngo, H. L., Jones, K., & Foglia, T. A. (2006) · Journal of the American Oil Chemists' Society · doi:10.1007/s11746-006-1249-0 · Cited by 109
“Aliphatic dicarboxylic acids are important intermediates in the synthesis of biodegradable polymers ( 1 ).”
BackgroundProtein adsorption on polymers
Rahmati, M., & Mozafari, M. (2018) · Materials Today Communications · doi:10.1016/j.mtcomm.2018.10.024 · Cited by 117
3D Printing Polymers with Supramolecular Functionality for Biological Applications
Pekkanen, A. M., Mondschein, R. J., Williams, C. B., & Long, T. E. (2017) · Biomacromolecules · doi:10.1021/acs.biomac.7b00671 · Cited by 118
Tissue Engineering in Liver Regenerative Medicine: Insights into Novel Translational Technologies
Heydari, Z., Najimi, M., Mirzaei, H., Shpichka, A. I., Ruoß, M., Farzaneh, Z., Montazeri, L., Piryaei, A., Timashev, P. S., Gramignoli, R., et al. (2020) · Cells · doi:10.3390/cells9020304 · Cited by 117
Biodegradation of Hemicellulose-Cellulose-Starch-Based Bioplastics and Microbial Polyesters
Abe, M. M., Branciforti, M. C., & Brienzo, M. (2021) · Recycling · doi:10.3390/recycling6010022 · Cited by 130
Biodegradable Polymers: Properties, Applications, and Environmental Impact
Dallaev, R., Papěž, N., Allaham, M. M., & Holcman, V. (2025) · Polymers · doi:10.3390/polym17141981 · Cited by 154
Dailey, L. A., Wittmar, M., & Kissel, T. (2004) · Journal of Controlled Release · doi:10.1016/j.jconrel.2004.09.003 · Cited by 108
Biodegradable polymer foams prepared with supercritical CO2–ethanol mixtures as blowing agents
Tsivintzelis, I., Pavlidou, E., & Panayiotou, C. G. (2007) · The Journal of Supercritical Fluids · doi:10.1016/j.supflu.2007.02.009 · Cited by 110
Koroleva, A., Gill, A. A., Asencio, Í. O., Haycock, J. W., Schlie, S., Gittard, S. D., Chichkov, B. N., & Claeyssens, F. (2012) · Biofabrication · doi:10.1088/1758-5082/4/2/025005 · Cited by 111
Surface modification of electrospun PLGA scaffold with collagen for bioengineered skin substitutes
Sadeghi, A. R., Nokhasteh, S., Molavi, A. M., Khorsand-Ghayeni, M., Naderi‐Meshkin, H., & Mahdizadeh, A. (2016) · Materials Science and Engineering C · doi:10.1016/j.msec.2016.04.073 · Cited by 116
Synthesis, characterization and biodegradation of functionalized amino acid-based poly(ester amide)s
Pang, X., & Chu, C. (2010) · Biomaterials · doi:10.1016/j.biomaterials.2010.01.027 · Cited by 110
Andreaus, U., Giorgio, I., & Lekszycki, T. (2013) · ZAMM ‐ Journal of Applied Mathematics and Mechanics / Zeitschrift für Angewandte Mathematik und Mechanik · doi:10.1002/zamm.201200182 · Cited by 107
“Calcium oxide, calcium carbonate and gypsum are other common materials that have been utilised during the last three decades [19, 25, 30, 43].”
BackgroundPolydioxanone implants: A systematic review on safety and performance in patients
Martins, J. A., Lach, A. A., Morris, H. L., Carr, A. J., & Mouthuy, P. (2019) · Journal of Biomaterials Applications · doi:10.1177/0885328219888841 · Cited by 122
“These types of materials are attractive for medical applications due to their ability to tailor mechanical properties and degradation profiles, and the possibility to have designed functional groups for different medical purposes.(3,5) The small variability between batches and typically reduced chronic FBRs are also a…”
BackgroundInfluentialDesign, characterization and preliminary biological evaluation of new lignin-PLA biocomposites
Spiridon, I., & Tanase, C. E. (2018) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2018.03.140 · Cited by 113
Polymer Synthesis and Processing
Kariduraganavar, M. Y., Kittur, A. A., & Kamble, R. R. (2014) · Elsevier eBooks · doi:10.1016/b978-0-12-396983-5.00001-6 · Cited by 183
Goonoo, N., Bhaw‐Luximon, A., Bowlin, G. L., & Jhurry, D. (2013) · Polymer International · doi:10.1002/pi.4474 · Cited by 117
Poly(caprolactone) based magnetic scaffolds for bone tissue engineering
Bañobre‐López, M., Piñeiro, Y., Santis, R. D., Gloria, A., Ambrosio, L., Tampieri, A., Dediu, V., & Rivas, J. M. (2011) · Journal of Applied Physics · doi:10.1063/1.3561149 · Cited by 100
Willie, B. M., Petersen, A., Schmidt‐Bleek, K., Cipitria, A., Mehta, M., Strube, P., Lienau, J., Wildemann, B., Fratzl, P., & Duda, G. N. (2010) · Soft Matter · doi:10.1039/c0sm00262c · Cited by 126
In vitro and in vivo degradation of poly(l-lactide-co-glycolide) films and scaffolds
Pamuła, E., & Menaszek, E. (2007) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-007-3292-2 · Cited by 104
Heinemann, C., Heinemann, S., Bernhardt, A., et al. (2008) · Biomacromolecules · doi:10.1021/bm800693d · Cited by 102
Zhang, Q., Jiang, Y., Zhang, Y., Ye, Z., Tan, W., & Lang, M. (2013) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.10.008 · Cited by 102
Hsiao, S.-H., & Hsu, S. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b08362 · Cited by 104
Two-Dimensional (2D) and Three-Dimensional (3D) Cell Culturing in Drug Discovery
Joseph, J. S., Malindisa, S. T., & Ntwasa, M. M. (2019) · IntechOpen eBooks · doi:10.5772/intechopen.81552 · Cited by 130
Complicity of degradable polymers in health-care applications
Anju, S., Prajitha, N., Sukanya, V. S., & Mohanan, P. V. (2020) · Materials Today Chemistry · doi:10.1016/j.mtchem.2019.100236 · Cited by 101
A Novel Biomimetic Hybrid Material Made of Silicified Collagen: Perspectives for Bone Replacement
Heinemann, S., Heinemann, C., Ehrlich, H., Meyer, M., Baltzer, H., Worch, H., & Hanke, T. (2007) · Advanced Engineering Materials · doi:10.1002/adem.200700219 · Cited by 98
Localized delivery of growth factors for angiogenesis and bone formation in tissue engineering
Bai, Y., Yin, G., Huang, Z., Liao, X., Chen, X., Yao, Y., & Pu, X. (2013) · International Immunopharmacology · doi:10.1016/j.intimp.2013.04.001 · Cited by 100
Porous Inorganic Drug Delivery Systems—a Review
Sayed, E., Haj‐Ahmad, R., Ruparelia, K. C., Arshad, M. S., Chang, M., & Ahmad, Z. (2017) · AAPS PharmSciTech · doi:10.1208/s12249-017-0740-2 · Cited by 104
Yan, Y., Yao, R., Zhao, J., Chen, K., Duan, L., Wang, T., Zhang, S., Guan, J., Zheng, Z., Wang, X., et al. (2021) · Bioactive Materials · doi:10.1016/j.bioactmat.2021.09.030 · Cited by 124
“Comparing natural polymers with synthetic polymers, the former ones are less toxic and more biocompatible, in which some compositions can animate cellular proliferation and migration [65].”
BackgroundYang, H. S., Ieronimakis, N. M., Tsui, J. H., Kim, H. N., Suh, K. Y., Reyes, M., & Kim, D. (2013) · Biomaterials · doi:10.1016/j.biomaterials.2013.10.067 · Cited by 103
“Several experiments have demonstrated that the shortest degradation time of 1e2 months was achieved with a 50:50 lactide:glycolide ratio, while the longest degradation time of 5e6 months was observed for 85:15 lactide:glycolide PLGA in vivo [23].”
BackgroundYildirimer, L., & Seifalian, A. M. (2014) · Biotechnology Advances · doi:10.1016/j.biotechadv.2014.04.014 · Cited by 98
“5) (Gunatillake and Adhikari, 2003).”
BackgroundPolyurethane foam/nano hydroxyapatite composite as a suitable scaffold for bone tissue regeneration
Meskinfam, M., Bertoldi, S., Albanese, N., Cerri, A., Tanzi, M. C., Imani, R., Baheiraei, N., Farokhi, M., & Farè, S. (2017) · Materials Science and Engineering C · doi:10.1016/j.msec.2017.08.064 · Cited by 107
Bioprinted osteon-like scaffolds enhance in vivo neovascularization
Piard, C., Baker, H. B., Kamalitdinov, T. B., & Fisher, J. P. (2019) · Biofabrication · doi:10.1088/1758-5090/ab078a · Cited by 97
Poly(α-hydroxy acid) based polymers: A review on material and degradation aspects
Ginjupalli, K., Shavi, G. V., Averineni, R. K., Bhat, M., Udupa, N., & Upadhya, N. P. (2017) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2017.08.024 · Cited by 105
Hoornaert, A., d’Arros, C., Heymann, M., & Layrolle, P. (2016) · Biomedical Materials · doi:10.1088/1748-6041/11/4/045012 · Cited by 102
Engineering pharmaceutical nanocarriers for photodynamic therapy on wound healing: Review
Shanmugapriya, K., & Kang, H. W. (2019) · Materials Science and Engineering: C · doi:10.1016/j.msec.2019.110110 · Cited by 96
Biomaterials to Prevent Post-Operative Adhesion
Park, H., Baek, S., Kang, H., & Lee, D. (2020) · Materials · doi:10.3390/ma13143056 · Cited by 96
A perspective on molybdenum biocompatibility and antimicrobial activity for applications in implants
Ribeiro, A. M., Flores‐Sahagun, T. H. S., & Paredes, R. C. (2015) · Journal of Materials Science · doi:10.1007/s10853-015-9664-y · Cited by 99
“Biopolymers have many applications in various specialties and can be classified as synthetic or natural polymers that are degradable or stable [21, 22].”
BackgroundZhang, Z., Qian, H., Huang, J., Sha, H., Zhang, H., Yu, L., Liu, B., Hua, D., & Qian, X. (2018) · International Journal of Nanomedicine · doi:10.2147/ijn.s170148 · Cited by 96
Sajkiewicz, P., & Kołbuk, D. (2014) · Journal of Biomaterials Science Polymer Edition · doi:10.1080/09205063.2014.975392 · Cited by 101
“[52,53]), poly-L-lactide (PLLA),[54,55] resulting in electrospun bicomponent fibers.”
BackgroundIn-vitro evaluation of Polylactic acid (PLA) manufactured by fused deposition modeling
Wurm, M. C., Möst, T., Bergauer, B., Rietzel, D., Neukam, F. W., Cifuentes, S. C., & Wilmowsky, C. V. (2017) · Journal of Biological Engineering · doi:10.1186/s13036-017-0073-4 · Cited by 93
Carrow, J. K., Kerativitayanan, P., Jaiswal, M. K., Lokhande, G. K., & Gaharwar, A. K. (2015) · Elsevier eBooks · doi:10.1016/b978-0-12-800972-7.00013-x · Cited by 122
Preparation of Chitin-PLA laminated composite for implantable application
Nasrin, R., Biswas, S., Rashid, T. U., Afrin, S., Jahan, R. A., Haque, P., & Rahman, M. M. (2017) · Bioactive Materials · doi:10.1016/j.bioactmat.2017.09.003 · Cited by 93
Feng, B., Wang, S., Hu, D., Fu, W., Wu, J., Hong, H., Domian, I. J., Li, F., & Liu, J. (2019) · Acta Biomaterialia · doi:10.1016/j.actbio.2018.10.022 · Cited by 93
Printomics: the high-throughput analysis of printing parameters applied to melt electrowriting
Wunner, F. M., Mieszczanek, P., Bas, O., Eggert, S., Maartens, J. H., Dalton, P. D., De‐Juan‐Pardo, E. M., & Hutmacher, D. W. (2019) · Biofabrication · doi:10.1088/1758-5090/aafc41 · Cited by 99
Optimization of the structure of polyurethanes for bone tissue engineering applications
Bil, M., Ryszkowska, J., Woźniak, P. A., Kurzydłowski, K. J., & Lewandowska-Szumieł, M. (2009) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.08.037 · Cited by 96
“The quality of this attachment will influence cell capability to proliferate and differentiate [8,50].”
BackgroundResultLuo, Y., Dolder, C. K., Walker, J. M., Mishra, R., Dean, D., & Becker, M. L. (2016) · Biomacromolecules · doi:10.1021/acs.biomac.6b00014 · Cited by 92
Geesala, R., Bar, N., Dhoke, N. R., Basak, P., & Das, A. (2015) · Biomaterials · doi:10.1016/j.biomaterials.2015.11.003 · Cited by 94
Deng, M., Nair, L. S., Nukavarapu, S. P., Kumbar, S. G., Jiang, T., Krogman, N. R., Singh, A., Allcock, H. R., & Laurencin, C. T. (2007) · Biomaterials · doi:10.1016/j.biomaterials.2007.09.029 · Cited by 91
“Biodegradable polymers as scaffold materials need to possess a number of properties including non-toxic degradation products, mechanical properties that match the surrounding tissue and appropriate degradation rate to match new tissue formation under physiological conditions [6].”
BackgroundLi, Y., Shi, X., Tian, L., Sun, H.-Y., Wu, Y., Li, X., Li, J., Wei, Y., Han, X., Zhang, J., et al. (2016) · Advanced Materials · doi:10.1002/adma.201603027 · Cited by 96
A novel polyurethane/cellulose fibrous scaffold for cardiac tissue engineering
Chen, P.-H., Liao, H., Hsu, S., Chen, R., Wu, M., Yang, Y., Wu, C., Chen, M., & Su, W. (2014) · RSC Advances · doi:10.1039/c4ra12486c · Cited by 94
Tissue Engineering Using Ceramics and Polymers
Gough, J. E. (2007) · CRC Press eBooks · doi:10.1201/9781439823989 · Cited by 96
Haque, S. T., Saha, S. K., Haque, M. E., & Biswas, N. (2021) · Biomaterials Science · doi:10.1039/d1bm01211h · Cited by 92
Influence of the Mechanical Environment on the Regeneration of Osteochondral Defects
Davis, S., Roldo, M., Blunn, G. W., Tozzi, G., & Roncada, T. (2021) · Frontiers in Bioengineering and Biotechnology · doi:10.3389/fbioe.2021.603408 · Cited by 99
Recent Developments in Polyurethane-Based Materials for Bone Tissue Engineering
Szczepańczyk, P., Szlachta, M., Złocista-Szewczyk, N., Chłopek, J., & Pielichowska, K. (2021) · Polymers · doi:10.3390/polym13060946 · Cited by 94
Manufacture of degradable polymeric scaffolds for bone regeneration
Ge, Z., Jin, Z., & Cao, T. (2008) · Biomedical Materials · doi:10.1088/1748-6041/3/2/022001 · Cited by 94
Moers-Carpi, M., & Sherwood, S. (2013) · Dermatologic Surgery · doi:10.1111/dsu.12054 · Cited by 94
Ostrowski, N. J., Lee, B., Enick, N., Carlson, B., Kunjukunju, S., Roy, A., & Kumta, P. N. (2013) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.05.010 · Cited by 91
“The three anionic polymers used in this study were chosen based on the variety of anticipated degradation rates, from PLGA 50:50 degrading the most rapidly to PCL degrading the most slowly [36,37].”
BackgroundClassification of biodegradable polymers
Clarinval, A.-M., & Halleux, J. (2005) · Elsevier eBooks · doi:10.1533/9781845690762.1.3 · Cited by 104
Biodegradable polymer scaffolds
Hsu, S.-H., Hung, K.-C., & Chen, C.-W. (2016) · Journal of Materials Chemistry B · doi:10.1039/c6tb02176j · Cited by 87
Biomimetic immunomodulation strategies for effective tissue repair and restoration
Villarreal-Leal, R. A., Healey, G. D., & Corradetti, B. (2021) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2021.113913 · Cited by 86
Güiza-Argüello, V. R., Solarte-David, V. A., Pinzón-Mora, A. V., Ávila-Quiroga, J. E., & Becerra‐Bayona, S. M. (2022) · Polymers · doi:10.3390/polym14142764 · Cited by 96
“As opposed to their natural counterparts, synthetic polymers can be more easily produced at an industrial scale, and their tunability allows for their use in different configurations that favor desired tissue growth [64].”
BackgroundSynthetic Biomaterials for Regenerative Medicine Applications
Samavedi, S., Poindexter, L. K., Dyke, M. E. V., & Goldstein, A. S. (2013) · Elsevier eBooks · doi:10.1016/b978-0-12-398523-1.00007-0 · Cited by 129
A Review on Biodegradable Polymeric Materials Striving Towards the Attainment of Green Environment
Jayanth, D., Kumar, P. S., Nayak, G. C., Kumar, J. S., Pal, S. K., & Rathanasamy, R. (2017) · Journal of Polymers and the Environment · doi:10.1007/s10924-017-0985-6 · Cited by 88
Khan, I., Nagarjuna, R., Dutta, J. R., & Ganesan, R. (2019) · ACS Omega · doi:10.1021/acsomega.8b02642 · Cited by 88
Xylan hemicellulose improves chitosan hydrogel for bone tissue regeneration
Bush, J. R., Liang, H., Dickinson, M., & Botchwey, E. A. (2016) · Polymers for Advanced Technologies · doi:10.1002/pat.3767 · Cited by 90
Wang, X., Han, C., Hu, X., Sun, H., You, C., Gao, C., & Haiyang, Y. (2011) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2011.04.009 · Cited by 90
“The materials used for the fabrication of the knitted mesh are commonly synthetic materials, such as poly(lactic-coglycolic acid) (PLGA), which are hydrophobic and lack the cellrecognition sites necessary for cell adhesion and function (Gunatillake and Adhikari, 2003).”
Design and Control of Compostability in Synthetic Biopolyesters
Samantaray, P. K., Little, A., Wemyss, A. M., Iacovidou, E., & Wan, C. (2021) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.1c01424 · Cited by 88
Zhang, H., & Chen, Z. (2010) · Journal of Bioactive and Compatible Polymers · doi:10.1177/0883911509359486 · Cited by 86
Gambogic acid-loaded biomimetic nanoparticles in colorectal cancer treatment
Zhang, Z., Qian, H., Yang, M., Li, R., Hu, J. Y., Li, L., Yu, L., Liu, B., & Qian, X. (2017) · International Journal of Nanomedicine · doi:10.2147/ijn.s127256 · Cited by 83
“12,13 Despite the utilization of biocompatible and biodegradable materials, such as poly(lactic-co -glycolic acid) (PLGA), polylactic acid, and polycaprolactone, 14,15 nano-carriers are unavoidably met with quick excretion from the mononuclear phagocyte system.”
Vandghanooni, S., & Eskandani, M. (2019) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2019.09.020 · Cited by 84
Wu, S., Zhou, Y., Yu, Y., Zhou, X., Du, W. T., Wan, M., Fan, Y., Zhou, X., Xu, X., & Zheng, L. (2019) · Stem Cells International · doi:10.1155/2019/1515040 · Cited by 81
“Generally, agent release from biocompatible materials is related to initial agent loading, agent solubility, carrier material degradation, and so on [49].”
BackgroundBrugmans, M. C. P., Söntjens, S. H. M., Cox, M. A. J., Nandakumar, A., Bosman, A. W., Mes, T., Janssen, H. M., Bouten, C. V. C., Baaijens, F. F., & Driessen‐Mol, A. (2015) · Acta Biomaterialia · doi:10.1016/j.actbio.2015.08.034 · Cited by 90
Growth factor-eluting technologies for bone tissue engineering
Nyberg, E. L., Holmes, C. A., Witham, T. F., & Grayson, W. L. (2015) · Drug Delivery and Translational Research · doi:10.1007/s13346-015-0233-3 · Cited by 90
“Decades of research into drug delivery materials have yielded a broad array of naturally and synthetically-derived biodegradable materials which can be employed to produce 3D scaffolds of varying architectures (reviewed in detail in [34–36]).”
BackgroundKim, B. S., Jang, J., Chae, S., Gao, G., Kong, J., Ahn, M., & Cho, D. (2016) · Biofabrication · doi:10.1088/1758-5090/8/3/035013 · Cited by 84
Bone Tissue Engineering and Nanotechnology: A Promising Combination for Bone Regeneration
Bauso, L. V., Fauci, V. L., Longo, C., & Calabrese, G. (2024) · Biology · doi:10.3390/biology13040237 · Cited by 104
“Despite these advantages, some important limitations, such as poor biocompatibility, high toxicity, and reduced bioactivity and osteoconduc-tivity have restricted their application in BTE [69].”
BackgroundSynthesis, characterization, degradation of biodegradable castor oil based polyesters
Sathiskumar, P. S., & Madras, G. (2011) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2011.07.002 · Cited by 79
Jaiswal, A. K., Kadam, S. S., Soni, V., & Bellare, J. R. (2013) · Applied Surface Science · doi:10.1016/j.apsusc.2012.12.152 · Cited by 82
Blends and Nanocomposite Biomaterials for Articular Cartilage Tissue Engineering
Doulabi, A. H., Mequanint, K., & Mohammadi, H. (2014) · Materials · doi:10.3390/ma7075327 · Cited by 82
“Among these polymers, natural polymers could provide some properties such as biocompatibility, biodegradability, low toxicity, and cell signaling [8,9] whereas synthetic polymers provide some other properties such as mechanical and physical properties and thermal stability [10].”
BackgroundLin, H.-H., Hsieh, F.-Y., Tseng, C.-S., & Hsu, S.-H. (2016) · Journal of Materials Chemistry B · doi:10.1039/c6tb01501h · Cited by 79
Arjmand, M., Ardeshirylajimi, A., Maghsoudi, H., & Azadian, E. (2017) · Journal of Cellular Physiology · doi:10.1002/jcp.25962 · Cited by 79
“These seeded cells, under proper biochemical and biomechanical conditions, will grow up to the expected tissue with full potentials of a normal one (Gunatillake & Adhikari, 2003).”
BackgroundSharmin, N., & Rudd, C. D. (2017) · Journal of Materials Science · doi:10.1007/s10853-017-0784-4 · Cited by 93
“In physiological environment, these bioresorbable polymers gradually break down into biocompatible solution degradation products over time [198].”
BackgroundInfluentialPlant-based biomaterials in tissue engineering
Indurkar, A. R., Pandit, A., Jain, R. D., & Dandekar, P. P. (2021) · Bioprinting · doi:10.1016/j.bprint.2020.e00127 · Cited by 85
Wang, S., Lu, L., Gruetzmacher, J. A., Currier, B. L., & Yaszemski, M. J. (2005) · Macromolecules · doi:10.1021/ma050884c · Cited by 78
Protected N-heterocyclic carbenes as latent pre-catalysts for the polymerization of ε-caprolactone
Naumann, S., Schmidt, F. G., Frey, W. U., & Buchmeiser, M. R. (2013) · Polymer Chemistry · doi:10.1039/c3py00548h · Cited by 83
Caracciolo, P. C., Buffa, F., & Abraham, G. A. (2008) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-008-3561-8 · Cited by 80
Debnath, T., Ghosh, S., Shalini, U., Kona, L. K., Kamaraju, S. R., Sarkar, S., Gaddam, S., & Chelluri, L. K. (2015) · PLoS ONE · doi:10.1371/journal.pone.0120803 · Cited by 82
“These are fibrous, non-toxic, and biodegradable molecules, and can be easily manipulated without encouraging cell adhesion [14].”
BackgroundSilk fibroin-based scaffolds for tissue engineering
Li, Z., Ji, S., Wang, Y., Shen, X., & Liang, H. (2013) · Frontiers of Materials Science · doi:10.1007/s11706-013-0214-8 · Cited by 81
“Gunatillake and Adhikari found that the change of mechanical property is out of step with cells growth [66].”
BackgroundMohammadi, Y., Soleimani, M., Fallahi‐Sichani, M., et al. (2007) · The International Journal of Artificial Organs · doi:10.1177/039139880703000305 · Cited by 78
“Over the last few decades, a vast majority of natural and synthetic scaffolding materials have been studied (11-14).”
BackgroundComparison of a resorbable magnesium implant in small and large growing-animal models
Grün, N. G., Holweg, P. L., Tangl, S., Eichler, J., Berger, L., van den Beucken, J. J. J. P., Löffler, J. F., Klestil, T., & Weinberg, A. (2018) · Acta Biomaterialia · doi:10.1016/j.actbio.2018.07.044 · Cited by 78
Generation and Characterization of Novel Magnetic Field-Responsive Biomaterials
López‐López, M. T., Scionti, G., Oliveira, A. C., Durán, J. D. G., Campos, A., Alaminos, M., & Rodríguez, I. Á. (2015) · PLoS ONE · doi:10.1371/journal.pone.0133878 · Cited by 80
“They should thus meet a number of requirements, including biocompatibility [1–4].”
BackgroundKumbar, S. G., Bhattacharyya, S., Nukavarapu, S. P., Khan, Y., Nair, L. S., & Laurencin, C. T. (2006) · Journal of Inorganic and Organometallic Polymers and Materials · doi:10.1007/s10904-006-9071-6 · Cited by 76
Boddupalli, A., Zhu, L., & Bratlie, K. M. (2016) · Advanced Healthcare Materials · doi:10.1002/adhm.201600532 · Cited by 76
Roy, T., Maity, P. P., Rameshbabu, A. P., Das, B., John, A., Dutta, A., Ghorai, S. K., Chattopadhyay, S., & Dhara, S. (2018) · Bioengineering · doi:10.3390/bioengineering5030068 · Cited by 78
Supercritical fluids in 3-D tissue engineering
Reverchon, E., & Cardea, S. (2012) · The Journal of Supercritical Fluids · doi:10.1016/j.supflu.2012.05.010 · Cited by 91
Jäger, M., Feser, T., Denck, H., & Krauspe, R. (2005) · Annals of Biomedical Engineering · doi:10.1007/s10439-005-5889-2 · Cited by 88
Metadata
- Authors
- CSIRO Molecular Science, B. 1., & Gunatillake, P.
- Corresponding author
- CSIRO Molecular Science, Bag 10, Clayton South MDC, Vic 3169, Australia
- Venue
- European Cells and Materials
- Publisher
- Forum Multimedia Publishing LLC
- Published
- 2003-10-01
- Volume
- 5
- Pages
- 1-16
- ISSN
- 1473-2262 (ISSN-L)
- OpenAlex
- W2106035984
- Cited by
- 1,765
- References
- 97
- Citations by year
- 2026: 43 · 2025: 61 · 2024: 59 · 2023: 80 · 2022: 90 · 2021: 112 · 2020: 102 · 2019: 115 · 2018: 105 · 2017: 128 · 2016: 110 · 2015: 106 · 2014: 110 · 2013: 91 · 2012: 86
- FWCI
- 1.32
- Type
- journal article
- Language
- en
- Open access
- gold
- doi.org
- Licence
- cc-by
- Locations
- European Cells and Materials (publishedVersion, cc-by)
- PubMed (publishedVersion)
- DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion)
- Topics
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
- Health Sciences › Medicine › Surgery › Surgical Sutures and Adhesives
- Keywords
- tissue engineering, polyesters, polyglycolic acid, polylactic acid, polyanhydrides, polyphosphazenes, polyurethane, poly(propylene fumarate), injectable polymers, orthopedic tissue engineering, biodegradation, biocompatibility, degradation products
- MeSH terms
- Biocompatible Materials, Models, Chemical, Polymers, Tissue Engineering
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
A language model drew the claims from the paper on 2026-10-10, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).
A second model labelled each claim on 2026-10-10 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).
Cited sources are checked with a language model’s help (gpt-6-sol).
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.