Abstract
Metal and semiconductor oxides are ubiquitous electronic materials. Normally insulating, oxides can change behavior under high electric fields--through 'electroforming' or 'breakdown'--critically affecting CMOS (complementary metal-oxide-semiconductor) logic, DRAM (dynamic random access memory) and flash memory, and tunnel barrier oxides. An initial irreversible electroforming process has been invariably required for obtaining metal oxide resistance switches, which may open urgently needed new avenues for advanced computer memory and logic circuits including ultra-dense non-volatile random access memory (NVRAM) and adaptive neuromorphic logic circuits. This electrical switching arises from the coupled motion of electrons and ions within the oxide material, as one of the first recognized examples of a memristor (memory-resistor) device, the fourth fundamental passive circuit element originally predicted in 1971 by Chua. A lack of device repeatability has limited technological implementation of oxide switches, however. Here we explain the nature of the oxide electroforming as an electro-reduction and vacancy creation process caused by high electric fields and enhanced by electrical Joule heating with direct experimental evidence. Oxygen vacancies are created and drift towards the cathode, forming localized conducting channels in the oxide. Simultaneously, O(2-) ions drift towards the anode where they evolve O(2) gas, causing physical deformation of the junction. The problematic gas eruption and physical deformation are mitigated by shrinking to the nanoscale and controlling the electroforming voltage polarity. Better yet, electroforming problems can be largely eliminated by engineering the device structure to remove 'bulk' oxide effects in favor of interface-controlled electronic switching.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Strukov, D. B., Snider, G. S., Stewart, D. R., & Williams, R. S. (2008) · Nature · doi:10.1038/nature06932 · Cited by 11,828
Self-citationMemristor—The Missing Circuit Element
Chua, L. (1971) · IEEE Transactions on Circuit Theory · doi:10.1109/tct.1971.1083337 · Cited by 10,268
WSXM: A software for scanning probe microscopy and a tool for nanotechnology
Horcas, I., Fernández, R., Gómez-Rodríguez, J. M., Colchero, J., Gómez-Herrero, J., & Baro, A. M. (2007) · Review of Scientific Instruments · doi:10.1063/1.2432410 · Cited by 7,738
Nanoionics-based resistive switching memories
Waser, R., & Aono, M. (2007) · Nature Materials · doi:10.1038/nmat2023 · Cited by 4,923
Memristive switching mechanism for metal/oxide/metal nanodevices
Yang, J. J., Pickett, M. D., Li, X., Ohlberg, D. A. A., Stewart, D. R., & Williams, R. S. (2008) · Nature Nanotechnology · doi:10.1038/nnano.2008.160 · Cited by 2,987
Self-citationAnalog VLSI and Neural Systems
Mead, C. (1989) · CaltechAUTHORS (California Institute of Technology) · Cited by 2,776
Analog VLSI Implementation of Neural Systems
(1989) · The Kluwer International Series in Engineering and Computer Science · doi:10.1007/978-1-4613-1639-8 · Cited by 1,680
Switching the electrical resistance of individual dislocations in single-crystalline SrTiO3
Szot, K., Speier, W., Bihlmayer, G., & Waser, R. (2006) · Nature Materials · doi:10.1038/nmat1614 · Cited by 1,651
Direct electrochemical reduction of titanium dioxide to titanium in molten calcium chloride
Chen, G. Z., Fray, D. J., & Farthing, T. W. (2000) · Nature · doi:10.1038/35030069 · Cited by 1,537
Quantized conductance atomic switch
Terabe, K., Hasegawa, T., Nakayama, T., & Aono, M. (2005) · Nature · doi:10.1038/nature03190 · Cited by 1,208
Cited by
Memristive devices for computing
Yang, J. J., Strukov, D. B., & Stewart, D. R. (2013) · Nature Nanotechnology · doi:10.1038/nnano.2012.240 · Cited by 3,885
Self-citation‘Memristive’ switches enable ‘stateful’ logic operations via material implication
Borghetti, J., Snider, G. S., Kuekes, P. J., Yang, J. J., Stewart, D. R., & Williams, R. S. (2010) · Nature · doi:10.1038/nature08940 · Cited by 1,929
Self-citationResistive switching materials for information processing
Wang, Z., Wu, H., Burr, G. W., Hwang, C. S., Wang, K. L., Xia, Q., & Yang, J. J. (2020) · Nature Reviews Materials · doi:10.1038/s41578-019-0159-3 · Cited by 1,214
Resistive Random Access Memory (ReRAM) Based on Metal Oxides
Akinaga, H., & Shima, H. (2010) · Proceedings of the IEEE · doi:10.1109/jproc.2010.2070830 · Cited by 1,037
Memory effects in complex materials and nanoscale systems
Pershin, Y. V., & Di Ventra, M. (2011) · Advances In Physics · doi:10.1080/00018732.2010.544961 · Cited by 823
Switching dynamics in titanium dioxide memristive devices
Pickett, M. D., Strukov, D. B., Borghetti, J. L., Yang, J. J., Snider, G. S., Stewart, D. R., & Williams, R. S. (2009) · Journal of Applied Physics · doi:10.1063/1.3236506 · Cited by 764
Self-citationHigh switching endurance in TaOx memristive devices
Yang, J. J., Zhang, M.-X., Strachan, J. P., Miao, F., Pickett, M. D., Kelley, R. D., Medeiros-Ribeiro, G., & Williams, R. S. (2010) · Applied Physics Letters · doi:10.1063/1.3524521 · Cited by 637
Self-citationKim, K. M., Jeong, D. S., & Hwang, C. S. (2011) · Nanotechnology · doi:10.1088/0957-4484/22/25/254002 · Cited by 631
Graphene Oxide Thin Films for Flexible Nonvolatile Memory Applications
Jeong, H. Y., Kim, J. Y., Kim, J. W., Hwang, J. O., Kim, J.-E., Lee, J. Y., Yoon, T. H., Cho, B. J., Kim, S. O., Ruoff, R. S., et al. (2010) · Nano Letters · doi:10.1021/nl101902k · Cited by 604
Niobium oxides and niobates physical properties: Review and prospects
Nico, C., Monteiro, T., & Graça, M. P. F. (2016) · Progress in Materials Science · doi:10.1016/j.pmatsci.2016.02.001 · Cited by 581
Memristor-based neural networks
Thomas, A. (2013) · Journal of Physics D: Applied Physics · doi:10.1088/0022-3727/46/9/093001 · Cited by 471
“The nano-switches can be deposited by, e.g., electron-beam evaporation or sputtering and more than 10 10 switching cycles were shown for some of the layer stacks [10, 11].”
BackgroundResistive switching phenomena: A review of statistical physics approaches
Lee, J. S., Lee, S., & Noh, T. W. (2015) · Applied Physics Reviews · doi:10.1063/1.4929512 · Cited by 463
Anatomy of a Nanoscale Conduction Channel Reveals the Mechanism of a High‐Performance Memristor
Miao, F., Strachan, J. P., Yang, J. J., Zhang, M., Goldfarb, I., Torrezan, A. C., Eschbach, P., Kelley, R. D., Medeiros‐Ribeiro, G., & Williams, R. S. (2011) · Advanced Materials · doi:10.1002/adma.201103379 · Cited by 444
Self-citationPickett, M. D., & Stanley Williams, R. (2012) · Nanotechnology · doi:10.1088/0957-4484/23/21/215202 · Cited by 385
Self-citationBrain-inspired computing with memristors: Challenges in devices, circuits, and systems
Zhang, Y., Wang, Z., Zhu, J., Yang, Y., Rao, M., Song, W., Zhuo, Y., Zhang, X., Cui, M., Shen, L., et al. (2020) · Applied Physics Reviews · doi:10.1063/1.5124027 · Cited by 384
Self-citationMuenstermann, R., Menke, T., Dittmann, R., & Waser, R. (2010) · Advanced Materials · doi:10.1002/adma.201001872 · Cited by 363
High‐Speed and Low‐Energy Nitride Memristors
Choi, B. J., Torrezan, A. C., Strachan, J. P., Kotula, P. G., Lohn, A. J., Marinella, M. J., Li, Z., Williams, R. S., & Yang, J. J. (2016) · Advanced Functional Materials · doi:10.1002/adfm.201600680 · Cited by 356
Self-citationResistive Switches and Memories from Silicon Oxide
Yao, J., Sun, Z., Zhong, L., Natelson, D., & Tour, J. M. (2010) · Nano Letters · doi:10.1021/nl102255r · Cited by 338
Yan, X., Pei, Y., Chen, H., Zhao, J., Zhou, Z., Wang, H., Zhang, L., Wang, J., Li, X., Qin, C., et al. (2019) · Advanced Materials · doi:10.1002/adma.201805284 · Cited by 335
Evidence for oxygen vacancies movement during wake-up in ferroelectric hafnium oxide
Starschich, S., Menzel, S., & Böttger, U. (2016) · Applied Physics Letters · doi:10.1063/1.4940370 · Cited by 308
Physics of the Switching Kinetics in Resistive Memories
Menzel, S., Böttger, U., Wimmer, M., & Salinga, M. (2015) · Advanced Functional Materials · doi:10.1002/adfm.201500825 · Cited by 301
Zhang, Y., Mao, G.-Q., Zhao, X., Li, Y., Zhang, M., Wu, Z., Wu, W., Sun, H., Guo, Y., Wang, L., et al. (2021) · Nature Communications · doi:10.1038/s41467-021-27575-z · Cited by 300
Recent Advances and Future Prospects for Memristive Materials, Devices, and Systems
Song, M.-K., Kang, J.-H., Zhang, X., Ji, W., Ascoli, A., Messaris, I., Demirkol, A. S., Dong, B., Aggarwal, S., Wan, W., et al. (2023) · ACS Nano · doi:10.1021/acsnano.3c03505 · Cited by 300
TiO2—a prototypical memristive material
Szot, K., Rogala, M., Speier, W., Klusek, Z., Besmehn, A., & Waser, R. (2011) · Nanotechnology · doi:10.1088/0957-4484/22/25/254001 · Cited by 297
Forming and switching mechanisms of a cation-migration-based oxide resistive memory
Tsuruoka, T., Terabe, K., Hasegawa, T., & Aono, M. (2010) · Nanotechnology · doi:10.1088/0957-4484/21/42/425205 · Cited by 296
Sub-10 nm Ta Channel Responsible for Superior Performance of a HfO2 Memristor
Jiang, H., Han, L., Lin, P., Wang, Z., Jang, M. H., Wu, Q., Barnell, M., Yang, J. J., Xin, H. L., & Xia, Q. (2016) · Scientific Reports · doi:10.1038/srep28525 · Cited by 277
Recent Advances in Memristive Materials for Artificial Synapses
Kim, S. G., Han, J. S., Kim, H., Kim, S. Y., & Jang, H. W. (2018) · Advanced Materials Technologies · doi:10.1002/admt.201800457 · Cited by 272
Nanoscale resistive switching devices: mechanisms and modeling
Yang, Y., & Lu, W. (2013) · Nanoscale · doi:10.1039/c3nr03472k · Cited by 270
Memristive Synapses and Neurons for Bioinspired Computing
Yang, R., Huang, H., & Guo, X. (2019) · Advanced Electronic Materials · doi:10.1002/aelm.201900287 · Cited by 263
Nonvolatile resistive switching memories-characteristics, mechanisms and challenges
PAN, F., CHEN, C., WANG, Z.-S., YANG, Y.-C., YANG, J., & ZENG, F. (2010) · Progress in Natural Science: Materials International · doi:10.1016/s1002-0071(12)60001-x · Cited by 244
Prospective of Semiconductor Memory Devices: from Memory System to Materials
Hwang, C. S. (2015) · Advanced Electronic Materials · doi:10.1002/aelm.201400056 · Cited by 243
State of the art of metal oxide memristor devices
Mohammad, B., Jaoude, M. A., Kumar, V., Al Homouz, D. M., Nahla, H. A., Al-Qutayri, M., & Christoforou, N. (2016) · Nanotechnology Reviews · doi:10.1515/ntrev-2015-0029 · Cited by 228
Formation and Instability of Silver Nanofilament in Ag-Based Programmable Metallization Cells
Hsiung, C.-P., Liao, H.-W., Gan, J.-Y., Wu, T.-B., Hwang, J.-C., Chen, F., & Tsai, M.-J. (2010) · ACS Nano · doi:10.1021/nn1010667 · Cited by 209
Electrical Performance and Scalability of Pt Dispersed SiO2Nanometallic Resistance Switch
Choi, B. J., Torrezan, A. C., Norris, K. J., Miao, F., Strachan, J. P., Zhang, M.-X., Ohlberg, D. A. A., Kobayashi, N. P., Yang, J. J., & Williams, R. S. (2013) · Nano Letters · doi:10.1021/nl401283q · Cited by 201
Self-citationAtomically Thin Femtojoule Memristive Device
Zhao, H., Dong, Z., Tian, H., DiMarzi, D., Han, M., Zhang, L., Yan, X., Liu, F., Shen, L., Han, S., et al. (2017) · Advanced Materials · doi:10.1002/adma.201703232 · Cited by 199
Emerging non-volatile memories: opportunities and challenges
Xue, C. J., Zhang, Y., Chen, Y., Sun, G., Yang, J. J., & Li, H. (2011) · Proceedings of the seventh IEEE/ACM/IFIP international conference on Hardware/software codesign and system synthesis · doi:10.1145/2039370.2039420 · Cited by 197
“The ‘electroforming’ process is a one-time application of high voltage or current that produces a significant reduction of the electronic conductivity [41].”
BackgroundNanoionic memristive phenomena in metal oxides: the valence change mechanism
Dittmann, R., Menzel, S., & Waser, R. (2021) · Advances in Physics · doi:10.1080/00018732.2022.2084006 · Cited by 194
Voltage-controlled domain wall traps in ferromagnetic nanowires
Bauer, U., Emori, S., & Beach, G. S. D. (2013) · Nature Nanotechnology · doi:10.1038/nnano.2013.96 · Cited by 191
Strukov, D. B., Alibart, F., & Stanley Williams, R. (2012) · Applied Physics A · doi:10.1007/s00339-012-6902-x · Cited by 191
Probing nanoscale oxygen ion motion in memristive systems
Yang, Y., Zhang, X., Qin, L., Zeng, Q., Qiu, X., & Huang, R. (2017) · Nature Communications · doi:10.1038/ncomms15173 · Cited by 189
“The dielectric constant is expected to stay unchanged unless the phase or stoichiometry of HfO 2 varies, while the geometric parameters can also change, for example, upon structural deformations occurring to the stimulated region due to strong Joule heating effects or oxygen gas eruptions 14,39,40 .”
InfluentialInterface‐Engineered Amorphous TiO2‐Based Resistive Memory Devices
Jeong, H. Y., Lee, J. Y., & Choi, S. (2010) · Advanced Functional Materials · doi:10.1002/adfm.201001254 · Cited by 185
Nanoionic Resistive Switching Memories: On the Physical Nature of the Dynamic Reset Process
Marchewka, A., Roesgen, B., Skaja, K., Du, H., Jia, C., Mayer, J., Rana, V., Waser, R., & Menzel, S. (2016) · Advanced Electronic Materials · doi:10.1002/aelm.201500233 · Cited by 182
TiO2-based memristors and ReRAM: materials, mechanisms and models (a review)
Gale, E. (2014) · Semiconductor Science and Technology · doi:10.1088/0268-1242/29/10/104004 · Cited by 181
“The oxygen ions may combine at the anode and evolve O2 gas, this has been seen in ReRAM [86], the Strukov memristor when fabricated with macroscale electrodes [87] and the sol-gel memristor [81].”
BackgroundTransition of stable rectification to resistive-switching in Ti/TiO2/Pt oxide diode
Huang, J.-J., Kuo, C.-W., Chang, W.-C., & Hou, T.-H. (2010) · Applied Physics Letters · doi:10.1063/1.3457866 · Cited by 175
Probing memristive switching in nanoionic devices
Yang, Y., & Huang, R. (2018) · Nature Electronics · doi:10.1038/s41928-018-0069-1 · Cited by 169
In situ imaging of the conducting filament in a silicon oxide resistive switch
Yao, J., Zhong, L., Natelson, D., & Tour, J. M. (2012) · Scientific Reports · doi:10.1038/srep00242 · Cited by 169
“3b ), as is often associated with the electroforming proces”
Bulk mixed ion electron conduction in amorphous gallium oxide causes memristive behaviour
Aoki, Y., Wiemann, C., Feyer, V., Kim, H.-S., Schneider, C. M., Ill-Yoo, H., & Martin, M. (2014) · Nature Communications · doi:10.1038/ncomms4473 · Cited by 166
Bipolar resistive switching and conduction mechanism of an Al/ZnO/Al-based memristor
Gul, F., & Efeoglu, H. (2017) · Superlattices and Microstructures · doi:10.1016/j.spmi.2016.11.043 · Cited by 77
Gul, F., & Efeoglu, H. (2017) · Ceramics International · doi:10.1016/j.ceramint.2017.05.090 · Cited by 71
Self-Adaptive Write Circuit for Low-Power and Variation-Tolerant Memristors
Jo, K.-H., Jung, C.-M., Min, K.-S., & Kang, S.-M. (2010) · IEEE Transactions on Nanotechnology · doi:10.1109/tnano.2010.2052108 · Cited by 53
“1 mA for 100 nm × 100 nm, which is very comparable to the writing current for 50 nm × 50 nm in [9].”
BackgroundInfluentialElectronic Conduction in Ti/Poly-TiO2/Ti Structures
Hossein-Babaei, F., & Alaei-Sheini, N. (2016) · Scientific Reports · doi:10.1038/srep29624 · Cited by 47
Kwon, J. U., Song, Y. G., Kim, J. E., Chun, S. Y., Kim, G. H., Noh, G., Kwak, J. Y., Hur, S., Kang, C.-Y., Jeong, D. S., et al. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.2c12247 · Cited by 44
Shi, T., Yin, X.-B., Yang, R., & Guo, X. (2016) · Physical Chemistry Chemical Physics · doi:10.1039/c5cp07675g · Cited by 37
Metadata
- Authors
- Joshua Yang, J., Miao, F., Pickett, M. D., Ohlberg, D. A. A., Stewart, D. R., Lau, C. N., & Williams, R. S.
- Venue
- Nanotechnology
- Publisher
- IOP Publishing
- Published
- 2009-05-05
- Volume
- 20
- Issue
- 21
- Pages
- 215201
- ISSN
- 0957-4484 (ISSN-L)
- 1361-6528
- OpenAlex
- W2154890396
- Cited by
- 860
- References
- 51
- FWCI
- 45.94
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.