Hydrolytic degradation of devices based on poly(dl-lactic acid) size-dependence
The DOI matches its Crossref record; 14 of the 15 references it cites were found in a registry or an index.
Abstract
The hydrolytic degradation of aliphatic polyesters derived from lactic and glycolic acids (PLA/GA polymers) has been previously shown to proceed heterogeneously in the case of large size devices, the rate of degradation being greater inside than at the surface. A qualitative model based on diffusion-reaction phenomena was proposed which accounts for the formation of the more stable outer layer. However, this model also suggested that devices with dimensions smaller than the thickness of the outer layer should degrade less rapidly than larger ones. In an attempt to check this hypothesis, 15 x 10 x 2 mm compression moulded plates, millimetric beads and submillimetric microspheres and cast films, derived from the same batch of poly (DL-lactic acid) polymer were allowed to age comparatively in isoosmolar 0.13 M phosphate buffer, pH 7.4, at 37 degrees C. Ageing of the various devices was monitored by measuring water absorption, weight loss, L-lactic acid formation, pH and molar mass changes. As expected, large size plates and millimetric beads degraded heterogeneously and much faster than homogeneously degraded submillimetric films and particles.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The ratio of surface area to volume has shown to be a significant factor for degradation of large devices. Higher surface area ratio leads to higher degradation of the matrix.”
From Poly Lactic-co-Glycolic Acid (PLGA) as Biodegradable Controlled Drug Delivery Carrier (2011) · cites this paper as [87]
Citations
Cites
Pitt, G. G., Gratzl, M. M., Kimmel, G. L., Surles, J., & Sohindler, A. (1981) · Biomaterials · doi:10.1016/0142-9612(81)90060-0 · Cited by 857
Li, S. M., Garreau, H., & Vert, M. (1990) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00700871 · Cited by 733
Self-citationLi, S., Garreau, H., & Vert, M. (1990) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00701077 · Cited by 488
Self-citationHolland, S. J., Tighe, B. J., & Gould, P. L. (1986) · Journal of Controlled Release · doi:10.1016/0168-3659(86)90001-5 · Cited by 478
Li, S. M., Garreau, H., & Vert, M. (1990) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00700872 · Cited by 383
Self-citationMore about the degradation of LA/GA-derived matrices in aqueous media
Vert, M., Li, S., & Garreau, H. (1991) · Journal of Controlled Release · doi:10.1016/0168-3659(91)90027-b · Cited by 295
Self-citationBiodegradable Polymers and Plastics
(2004) · Chemistry International -- Newsmagazine for IUPAC · doi:10.1515/ci.2004.26.2.30b · Cited by 293
In vivo degradation of massive poly(α-hydroxy acids): Validation of In vitro findings
Therin, M., Christel, P., Li, S., Garreau, H., & Vert, M. (1992) · Biomaterials · doi:10.1016/0142-9612(92)90027-l · Cited by 230
Self-citationA New Long-Acting Injectable Microcapsule System for the Administration of Progesterone
Beck, L. R., Cowsar, D. R., Lewis, D. H., Cosgrove, R. J., Riddle, C. T., Lowry, S. L., & Epperly, T. (1979) · Fertility and Sterility · doi:10.1016/s0015-0282(16)44002-1 · Cited by 221
Bioresorbable polymers for temporary therapeutic applications
Vert, M. (1989) · Die Angewandte Makromolekulare Chemie · doi:10.1002/apmc.1989.051660111 · Cited by 132
Self-citation
Cited by
Poly Lactic-co-Glycolic Acid (PLGA) as Biodegradable Controlled Drug Delivery Carrier
Makadia, H. K., & Siegel, S. J. (2011) · Polymers · doi:10.3390/polym3031377 · Cited by 4,816
“It has also been reported that bulk degradation is faster than pure surface degradation for PLGA, which makes the release of the drug faster from the devices with higher surface area to volume [82,86,87].”
BackgroundLong-Circulating and Target-Specific Nanoparticles: Theory to Practice
Moghimi, S. M., Hunter, A. C., & Murray, J. C. (2001) · Pharmacological Reviews · doi:10.1016/s0031-6997(24)01494-7 · Cited by 3,515
An Overview of Polylactides as Packaging Materials
Auras, R., Harte, B., & Selke, S. (2004) · Macromolecular Bioscience · doi:10.1002/mabi.200400043 · Cited by 3,454
Polymeric systems for controlled drug release
Uhrich, K. E., Cannizzaro, S. M., Langer, R. S., & Shakesheff, K. M. (1999) · Chemical Reviews · doi:10.1021/cr940351u · Cited by 2,633
Biodegradation and biocompatibility of PLA and PLGA microspheres
Anderson, J. M., & Shive, M. S. (1997) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(97)00048-3 · Cited by 2,617
“Vert and coworkers have carried out extensive studies on the size dependence of the hydrolytic degradation of devices based on lactic and glycolic acid polymers [10].”
BackgroundBiomaterial developments for bone tissue engineering
Burg, K. J. L., Porter, S., & Kellam, J. F. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00102-2 · Cited by 1,643
Recent Developments in Ring Opening Polymerization of Lactones for Biomedical Applications
Albertsson, A.-C., & Varma, I. K. (2003) · Biomacromolecules · doi:10.1021/bm034247a · Cited by 1,582
Navarro, M., Michiardi, A., Castaño, O., & Planell, J. A. (2008) · Journal of The Royal Society Interface · doi:10.1098/rsif.2008.0151 · Cited by 1,513
Fu, Y., & Kao, W. J. (2010) · Expert Opinion on Drug Delivery · doi:10.1517/17425241003602259 · Cited by 1,305
Hydrolytic degradation of polylactic acid (PLA) and its composites
Elsawy, M. A., Kim, K.-H., Park, J.-W., & Deep, A. (2017) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2017.05.143 · Cited by 988
New emerging trends in synthetic biodegradable polymers—Polylactide: A critique
Gupta, A. P., & Kumar, V. (2007) · European Polymer Journal · doi:10.1016/j.eurpolymj.2007.06.045 · Cited by 941
“In vitro studies Different research groups have studied the degradation of PLA under various environments like in controlled environment in soil and in microbial culture of Fusarium moniliforme and Pseudomanas putida [150] in alkaline medium [151] in sea water [152], compost microorganisms [153], hydrolytic degradatio…”
Backgroundda Silva, D., Kaduri, M., Poley, M., Adir, O., Krinsky, N., Shainsky-Roitman, J., & Schroeder, A. (2018) · Chemical Engineering Journal · doi:10.1016/j.cej.2018.01.010 · Cited by 863
Biodegradation and biocompatibility of PLA and PLGA microspheres
Anderson, J. M., & Shive, M. S. (2012) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2012.09.004 · Cited by 814
Degradation mechanisms of polycaprolactone in the context of chemistry, geometry and environment
Bartnikowski, M., Dargaville, T. R., Ivanovski, S., & Hutmacher, D. W. (2019) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2019.05.004 · Cited by 769
Biodegradable Polymers-A Review on Recent Trends and Emerging Perspectives
Luckachan, G. E., & Pillai, C. K. S. (2011) · Journal of Polymers and the Environment · doi:10.1007/s10924-011-0317-1 · Cited by 767
Fu, K., Pack, D. W., Klibanov, A. M., & Langer, R. (2000) · Pharmaceutical Research · doi:10.1023/a:1007582911958 · Cited by 764
Nanoparticles as vehicles for delivery of photodynamic therapy agents
Bechet, D., Couleaud, P., Frochot, C., Viriot, M.-L., Guillemin, F., & Barberi-Heyob, M. (2008) · Trends in Biotechnology · doi:10.1016/j.tibtech.2008.07.007 · Cited by 760
Griffith, L. G. (2000) · Acta Materialia · doi:10.1016/s1359-6454(99)00299-2 · Cited by 730
From Lactic Acid to Poly(lactic acid) (PLA): Characterization and Analysis of PLA and Its Precursors
Inkinen, S., Hakkarainen, M., Albertsson, A.-C., & Södergård, A. (2011) · Biomacromolecules · doi:10.1021/bm101302t · Cited by 710
Li, S. (1999) · Journal of Biomedical Materials Research · doi:10.1002/(sici)1097-4636(1999)48:3<342::aid-jbm20>3.0.co;2-7 · Cited by 664
Self-citationLifetime prediction of biodegradable polymers
Laycock, B., Nikolić, M., Colwell, J. M., Gauthier, E., Halley, P., Bottle, S., & George, G. (2017) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2017.02.004 · Cited by 662
PLGA: a Unique Polymer for Drug Delivery
Kapoor, D. N., Bhatia, A., Kaur, R., Sharma, R., Kaur, G., & Dhawan, S. (2015) · Therapeutic Delivery · doi:10.4155/tde.14.91 · Cited by 609
Evaluation of polycaprolactone scaffold degradation for 6 months in vitro and in vivo
Lam, C. X. F., Hutmacher, D. W., Schantz, J., Woodruff, M. A., & Teoh, S. H. (2009) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.32052 · Cited by 599
Aliphatic Polyesters: Great Degradable Polymers That Cannot Do Everything
Vert, M. (2005) · Biomacromolecules · doi:10.1021/bm0494702 · Cited by 565
Self-citationKim, K., Yu, M., Zong, X., Chiu, J., Fang, D., Seo, Y.-S., Hsiao, B. S., Chu, B., & Hadjiargyrou, M. (2003) · Biomaterials · doi:10.1016/s0142-9612(03)00407-1 · Cited by 562
Effect of acidic pH on PLGA microsphere degradation and release
Zolnik, B. S., & Burgess, D. J. (2007) · Journal of Controlled Release · doi:10.1016/j.jconrel.2007.05.034 · Cited by 560
“In particular, the size and porosity of the PLGA microspheres appeared to be critical to acid build up [11,12].”
Degradability of Polymers for Implantable Biomedical Devices
Lyu, S., & Untereker, D. (2009) · International Journal of Molecular Sciences · doi:10.3390/ijms10094033 · Cited by 538
Panyam, J., Dali, M. M., Sahoo, S. K., Ma, W., Chakravarthi, S. S., Amidon, G. L., Levy, R. J., & Labhasetwar, V. (2003) · Journal of Controlled Release · doi:10.1016/s0168-3659(03)00328-6 · Cited by 529
Wu, L., & Ding, J. (2004) · Biomaterials · doi:10.1016/j.biomaterials.2004.01.038 · Cited by 515
Biomedical Applications of Biodegradable Polyesters
Manavitehrani, I., Fathi, A., Badr, H., Daly, S., Negahi Shirazi, A., & Dehghani, F. (2016) · Polymers · doi:10.3390/polym8010020 · Cited by 514
Multi-pulse drug delivery from a resorbable polymeric microchip device
Grayson, A. C. R., Choi, I. S., Tyler, B. M., Wang, P. P., Brem, H., Cima, M. J., & Langer, R. (2003) · Nature Materials · doi:10.1038/nmat998 · Cited by 444
Lam, C. X. F., Savalani, M. M., Teoh, S.-H., & Hutmacher, D. W. (2008) · Biomedical Materials · doi:10.1088/1748-6041/3/3/034108 · Cited by 444
Dunne, M., Corrigan, O. I., & Ramtoola, Z. (2000) · Biomaterials · doi:10.1016/s0142-9612(00)00040-5 · Cited by 444
Alexis, F. (2005) · Polymer International · doi:10.1002/pi.1697 · Cited by 443
MicroRNA delivery through nanoparticles
Lee, S. W. L., Paoletti, C., Campisi, M., Osaki, T., Adriani, G., Kamm, R. D., Mattu, C., & Chiono, V. (2019) · Journal of Controlled Release · doi:10.1016/j.jconrel.2019.10.007 · Cited by 437
Xu, Y., Kim, C., Saylor, D. M., & Koo, D. (2017) · Journal of Biomedical Materials Research Part B: Applied Biomaterials · doi:10.1002/jbm.b.33648 · Cited by 424
de Jong, S. J., Arias, E. R., Rijkers, D. T. S., van Nostrum, C. F., Kettenes-van den Bosch, J. J., & Hennink, W. E. (2001) · Polymer · doi:10.1016/s0032-3861(00)00646-7 · Cited by 414
Controlled drug delivery in tissue engineering
Biondi, M., Ungaro, F., Quaglia, F., & Netti, P. A. (2008) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2007.08.038 · Cited by 412
Khouri, N. G., Bahú, J. O., Blanco-Llamero, C., Severino, P., Concha, V. O. C., & Souto, E. B. (2024) · Journal of Molecular Structure · doi:10.1016/j.molstruc.2024.138243 · Cited by 403
Stewart, S. A., Domínguez-Robles, J., Donnelly, R. F., & Larrañeta, E. (2018) · Polymers · doi:10.3390/polym10121379 · Cited by 390
Melt–solid polycondensation of lactic acid and its biodegradability
Maharana, T., Mohanty, B., & Negi, Y. S. (2009) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2008.10.001 · Cited by 368
How porosity and size affect the drug release mechanisms from PLGA-based microparticles
Klose, D., Siepmann, F., Elkharraz, K., Krenzlin, S., & Siepmann, J. (2006) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2005.07.031 · Cited by 358
Bourges, J.-L., Gautier, S. E., Delie, F., Bejjani, R. A., Jeanny, J.-C., Gurny, R., BenEzra, D., & Behar-Cohen, F. F. (2003) · Investigative Opthalmology & Visual Science · doi:10.1167/iovs.02-1068 · Cited by 357
Ford Versypt, A. N., Pack, D. W., & Braatz, R. D. (2013) · Journal of Controlled Release · doi:10.1016/j.jconrel.2012.10.015 · Cited by 345
Kissel, T., Li, Y., & Unger, F. (2002) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(01)00244-7 · Cited by 332
Tsuji, H., & Ikada, Y. (2000) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(99)00111-1 · Cited by 329
Polylactide/montmorillonite nanocomposites: study of the hydrolytic degradation
Paul, M.-A., Delcourt, C., Alexandre, M., Degée, P., Monteverde, F., & Dubois, P. (2005) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2004.10.011 · Cited by 326
“It happens mainly in the bulk of the material and not from its surface [3].”
BackgroundBölgen, N., Menceloğlu, Y. Z., Acatay, K., Vargel, İ., & Pişkin, E. (2005) · Journal of Biomaterials Science, Polymer Edition · doi:10.1163/156856205774576655 · Cited by 311
How Autocatalysis Accelerates Drug Release from PLGA-Based Microparticles: A Quantitative Treatment
Siepmann, J., Elkharraz, K., Siepmann, F., & Klose, D. (2005) · Biomacromolecules · doi:10.1021/bm050228k · Cited by 308
Rydz, J., Sikorska, W., Kyulavska, M., & Christova, D. (2014) · International Journal of Molecular Sciences · doi:10.3390/ijms16010564 · Cited by 303
Aliphatic Polyesters: Abiotic and Biotic Degradation and Degradation Products
Hakkarainen, M. (2002) · Advances in Polymer Science · doi:10.1007/3-540-45734-8_4 · Cited by 293
Copinet, A., Bertrand, C., Govindin, S., Coma, V., & Couturier, Y. (2004) · Chemosphere · doi:10.1016/j.chemosphere.2003.11.038 · Cited by 288
Deroiné, M., Le Duigou, A., Corre, Y.-M., Le Gac, P.-Y., Davies, P., César, G., & Bruzaud, S. (2014) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2014.01.020 · Cited by 279
“It appears here that during hydrolytic degradation the PLA undergoes bulk degradation, as previously noted [36,37].”
ResultSurface characteristics of PLA and PLGA films
Paragkumar N, T., Edith, D., & Six, J.-L. (2006) · Applied Surface Science · doi:10.1016/j.apsusc.2006.05.047 · Cited by 273
Biodegradation of polylactide in aerobic and anaerobic thermophilic conditions
Itävaara, M., Karjomaa, S., & Selin, J.-F. (2002) · Chemosphere · doi:10.1016/s0045-6535(01)00163-1 · Cited by 269
Mechanical study of PLA–PCL fibers during in vitro degradation
Vieira, A. C., Vieira, J. C., Ferra, J. M., Magalhães, F. D., Guedes, R. M., & Marques, A. T. (2011) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2010.12.006 · Cited by 266
Parent, M., Nouvel, C., Koerber, M., Sapin, A., Maincent, P., & Boudier, A. (2013) · Journal of Controlled Release · doi:10.1016/j.jconrel.2013.08.024 · Cited by 263
Henton, D., Gruber, P., Lunt, J., & Randall, J. (2005) · Natural Fibers, Biopolymers, and Biocomposites · doi:10.1201/9780203508206.ch16 · Cited by 253
Exploiting Sequence To Control the Hydrolysis Behavior of Biodegradable PLGA Copolymers
Li, J., Stayshich, R. M., & Meyer, T. Y. (2011) · Journal of the American Chemical Society · doi:10.1021/ja200895s · Cited by 249
Biomimetic scaffolds for regeneration of volumetric muscle loss in skeletal muscle injuries
Grasman, J. M., Zayas, M. J., Page, R. L., & Pins, G. D. (2015) · Acta Biomaterialia · doi:10.1016/j.actbio.2015.07.038 · Cited by 244
Silica‐Gelatin Hybrids with Tailorable Degradation and Mechanical Properties for Tissue Regeneration
Mahony, O., Tsigkou, O., Ionescu, C., Minelli, C., Ling, L., Hanly, R., Smith, M. E., Stevens, M. M., & Jones, J. R. (2010) · Advanced Functional Materials · doi:10.1002/adfm.201000838 · Cited by 244
Yoon, J. J., & Park, T. G. (2001) · Journal of Biomedical Materials Research · doi:10.1002/1097-4636(20010605)55:3<401::aid-jbm1029>3.0.co;2-h · Cited by 244
O'Hagan, D. (1998) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(98)00012-x · Cited by 243
In vitro degradation of a novel poly(lactide-co-glycolide) 75/25 foam
Holy, C. E., Dang, S. M., Davies, J. E., & Shoichet, M. S. (1999) · Biomaterials · doi:10.1016/s0142-9612(98)00256-7 · Cited by 241
“As has been shown previously using other polyester devices [9], the molecular weight of our polymer foams decreased prior to their mass.”
BackgroundKinetics and Time−Temperature Equivalence of Polymer Degradation
Lyu, Schley, J., Loy, B., Lind, D., Hobot, C., Sparer, R., & Untereker, D. (2007) · Biomacromolecules · doi:10.1021/bm070313n · Cited by 237
Naturally derived and synthetic scaffolds for skeletal muscle reconstruction
Wolf, M. T., Dearth, C. L., Sonnenberg, S. B., Loboa, E. G., & Badylak, S. F. (2015) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2014.08.011 · Cited by 230
“Like PLGA, PCL is biodegradable in vivo, although at a much slower rate on the order of months to years depending on the specific scaffold configuration [75,76,82,83].”
BackgroundBorden, M. (2003) · Biomaterials · doi:10.1016/s0142-9612(02)00374-5 · Cited by 227
Tsuji, H. (2002) · Polymer · doi:10.1016/s0032-3861(01)00752-2 · Cited by 226
Huang, M.-H., Li, S., & Vert, M. (2004) · Polymer · doi:10.1016/j.polymer.2004.10.054 · Cited by 222
Self-citationCleland, J. L., Duenas, E. T., Park, A., Daugherty, A., Kahn, J., Kowalski, J., & Cuthbertson, A. (2001) · Journal of Controlled Release · doi:10.1016/s0168-3659(01)00258-9 · Cited by 222
Regeneration of Periodontal Tissues: Guided Tissue Regeneration
Villar, C. C., & Cochran, D. L. (2010) · Dental Clinics of North America · doi:10.1016/j.cden.2009.08.011 · Cited by 221
Nanoclay and crystallinity effects on the hydrolytic degradation of polylactides
Zhou, Q., & Xanthos, M. (2008) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2008.05.014 · Cited by 218
Blaker, J. J., Gough, J. E., Maquet, V., Notingher, I., & Boccaccini, A. R. (2003) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.20055 · Cited by 215
Biodegradable microspheres for vitreoretinal drug delivery
Herrero-Vanrell, R., & Refojo, M. F. (2001) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(01)00200-9 · Cited by 211
Peritoneal adhesions: Occurrence, prevention and experimental models
Tang, J., Xiang, Z., Bernards, M. T., & Chen, S. (2020) · Acta Biomaterialia · doi:10.1016/j.actbio.2020.08.036 · Cited by 211
Lam, C. X., Teoh, S. H., & Hutmacher, D. W. (2007) · Polymer International · doi:10.1002/pi.2195 · Cited by 209
Wu, L., & Ding, J. (2005) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.30487 · Cited by 208
Schliecker, G., Schmidt, C., Fuchs, S., & Kissel, T. (2003) · Biomaterials · doi:10.1016/s0142-9612(03)00243-6 · Cited by 208
Tsuji, H., & Miyauchi, S. (2001) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(00)00191-9 · Cited by 204
Tsuji, H. (2000) · Polymer · doi:10.1016/s0032-3861(99)00545-5 · Cited by 200
Degradation Behaviors of Electrospun Resorbable Polyester Nanofibers
Dong, Y., Liao, S., Ngiam, M., Chan, C. K., & Ramakrishna, S. (2009) · Tissue Engineering Part B: Reviews · doi:10.1089/ten.teb.2008.0619 · Cited by 200
“Grizzi et al. 91 compared the degradation rate of different shapes of PDLLA: compression-molded plate, millimetric beads, microspheres, and cast films.”
A phenomenological model for the degradation of biodegradable polymers
Wang, Y., Pan, J., Han, X., Sinka, C., & Ding, L. (2008) · Biomaterials · doi:10.1016/j.biomaterials.2008.04.042 · Cited by 191
Li, J., Rothstein, S. N., Little, S. R., Edenborn, H. M., & Meyer, T. Y. (2012) · Journal of the American Chemical Society · doi:10.1021/ja306866w · Cited by 186
Pan, H., & Qiu, Z. (2010) · Macromolecules · doi:10.1021/ma9023685 · Cited by 185
Uskokovic, D., & Stevanovic, M. (2009) · Current Nanoscience · doi:10.2174/157341309787314566 · Cited by 182
“This has been documented in several longterm studies [183, 184].”
BackgroundHydrolysis and Biodegradation of Poly(lactic acid)
Gorrasi, G., & Pantani, R. (2017) · Advances in Polymer Science · doi:10.1007/12_2016_12 · Cited by 181
“For small size samples, such as nano and microparticles, the characteristic size of the device is smaller than the outer diffusion layer and, since the diffusion of the oligomers is not limiting, degradation proceeds invariably through a bulk erosion path [17,121,122].”
BackgroundNew trends in bioactive scaffolds: The importance of nanostructure
Jones, J. R. (2009) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2008.08.003 · Cited by 179
Cao, X., & Shoichet, M. S. (1999) · Biomaterials · doi:10.1016/s0142-9612(98)00172-0 · Cited by 178
“5a) disproves Vert’s [18] prediction that devices smaller than 200 lm degrade homogeneously.”
BackgroundMaquet, V., Boccaccini, A. R., Pravata, L., Notingher, I., & Jérôme, R. (2003) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.10587 · Cited by 177
Nanotherapy for posterior eye diseases
Kaur, I. P., & Kakkar, S. (2014) · Journal of Controlled Release · doi:10.1016/j.jconrel.2014.05.031 · Cited by 175
Andersson, S. R., Hakkarainen, M., Inkinen, S., Södergård, A., & Albertsson, A.-C. (2010) · Biomacromolecules · doi:10.1021/bm100029t · Cited by 174
Something new in the field of PLA/GA bioresorbable polymers?
Vert, M., Schwach, G., Engel, R., & Coudane, J. (1998) · Journal of Controlled Release · doi:10.1016/s0168-3659(97)00240-x · Cited by 173
Self-citationHakkarainen, M., Karlsson, S., & Albertsson, A. (2000) · Polymer · doi:10.1016/s0032-3861(99)00393-6 · Cited by 173
Fukushima, K., Tabuani, D., Dottori, M., Armentano, I., Kenny, J. M., & Camino, G. (2011) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2011.09.018 · Cited by 172
Chen, Y., Zhou, S., & Li, Q. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2010.09.038 · Cited by 172
A New Strategy for Recycling and Preparation of Poly(l-lactic acid): Hydrolysis in the Melt
Tsuji, H., Daimon, H., & Fujie, K. (2003) · Biomacromolecules · doi:10.1021/bm034060j · Cited by 168
Effect of TiO2 nanoparticles on the long-term hydrolytic degradation behavior of PLA
Luo, Y., Wang, X., & Wang, Y. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.02.011 · Cited by 168
Effects of Temperature and pH on the Degradation of Poly(lactic acid) Brushes
Xu, L., Crawford, K., & Gorman, C. B. (2011) · Macromolecules · doi:10.1021/ma2000948 · Cited by 167
Gleadall, A., Pan, J., Kruft, M.-A., & Kellomäki, M. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.12.039 · Cited by 165
Degradable and bioresorbable polymers in surgery and in pharmacology: beliefs and facts
Vert, M. (2008) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-008-3581-4 · Cited by 164
Self-citation
Metadata
- Authors
- Grizzi, I., Garreau, H., Li, S., & Vert, M.
- Affiliations
- Centre National de la Recherche Scientifique (FR)
- Corresponding author
- Garreau, H.
- Venue
- Biomaterials
- Publisher
- Elsevier BV
- Published
- 1995-03
- Volume
- 16
- Issue
- 4
- Pages
- 305-311
- ISSN
- 0142-9612 (ISSN-L)
- OpenAlex
- W2097892579
- Semantic Scholar
- e2f6d6592b9169fc0f64e0d3d927b66dab49b7b9
- Cited by
- 895
- References
- 15
- Citations by year
- 2026: 21 · 2025: 25 · 2024: 20 · 2023: 19 · 2022: 26 · 2021: 30 · 2020: 44 · 2019: 32 · 2018: 25 · 2017: 36 · 2016: 36 · 2015: 40 · 2014: 51 · 2013: 30 · 2012: 36
- FWCI
- 11.81
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- www.elsevier.com/legal/tdmrep-license (tdm)
- Locations
- Biomaterials (publishedVersion)
- PubMed (publishedVersion)
- HAL (submittedVersion)
- Topics
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
- Physical Sciences › Materials Science › Biomaterials › Magnesium Alloys: Properties and Applications
- Keywords
- poly(D,L-lactide), hydrolytic degradation, heterogeneous degradation, size effect, reaction-diffusion systems, aliphatic polyesters, water absorption, weight loss, microspheres, beads, phosphate buffer
- MeSH terms
- Absorption, Delayed-Action Preparations, Hydrogen-Ion Concentration, Hydrolysis, Lactates, Microscopy, Electron, Scanning, Microspheres, Molecular Weight, Particle Size, Polyesters, Polymers, Temperature, Time Factors, Water, Lactic Acid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.