Open accessAbstract
Polyurethane elastomers have a combination of excellent mechanical, physical and chemical properties along with exceptional biocompatibility. Therefore, these elastomeric systems are used in a diverse range of indoor, outdoor, underwater and biomedical applications. However, under certain conditions polyurethane elastomers undergo degradation, resulting in modified properties during usage or even complete failure. The degradation will not only severely affect the quality of the associated items, devices, or instruments, but may also cause catastrophic outcomes risking people’s safety and health. This review presents a comprehensive survey of the literature regarding various types of degradation of polyurethane elastomers, including photo-, thermal, ozonolytic, hydrolytic, chemical, enzymatic, in-vivo/in-vitro oxidative, biological, and mechanical degradation. The stability of polyurethane elastomers based on different building blocks of macrodiols (polyester, polyether, polycarbonate, polybutadiene, and polyisobutylene), isocyanates (aromatic and aliphatic), and chain extenders (diols, triols, and diamines) are summarised, and the mechanisms of different types of degradation are presented. The chemical components significantly influence not only the material structure and properties but also the degradative stability. Focussing on the components, we explore strategies for the enhancement of polyurethane stability through chemistry and engineering. A range of stabilizers, including both organic and inorganic additives for better stability against different types of degradation, are discussed, with a focus on their efficacy and mechanisms of action. A perspective on novel polyurethane materials with desired structures and properties combined with exceptional stability is also provided.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Fundamentals of zinc oxide as a semiconductor
Janotti, A., & Van de Walle, C. G. (2009) · Reports on Progress in Physics · doi:10.1088/0034-4885/72/12/126501 · Cited by 3,948
Solutions able to reproduce in vivo surface‐structure changes in bioactive glass‐ceramic A‐W3
Kokubo, T., Kushitani, H., Sakka, S., Kitsugi, T., & Yamamuro, T. (1990) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820240607 · Cited by 3,836
Some aspects of the surface chemistry of carbon blacks and other carbons
Boehm, H. P. (1994) · Carbon · doi:10.1016/0008-6223(94)90031-0 · Cited by 3,043
Behl, M., & Lendlein, A. (2007) · Materials Today · doi:10.1016/s1369-7021(07)70047-0 · Cited by 1,965
Polyurethane types, synthesis and applications – a review
Akindoyo, J. O., Beg, M. D. H., Ghazali, S., Islam, M. R., Jeyaratnam, N., & Yuvaraj, A. R. (2016) · RSC Advances · doi:10.1039/c6ra14525f · Cited by 1,831
Thermal stability and flame retardancy of polyurethanes
Chattopadhyay, D. K., & Webster, D. C. (2009) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2009.06.002 · Cited by 1,748
Mechanistic implications of plastic degradation
Singh, B., & Sharma, N. (2008) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.11.008 · Cited by 1,569
Photodegradation and photostabilization of polymers, especially polystyrene: review
Yousif, E., & Haddad, R. (2013) · SpringerPlus · doi:10.1186/2193-1801-2-398 · Cited by 1,503
Shape-memory polymers and their composites: stimulus methods and applications
Leng, J., Lan, X., Liu, Y., & Du, S. (2011) · Progress in Materials Science · doi:10.1016/j.pmatsci.2011.03.001 · Cited by 1,495
Polymer biodegradation: Mechanisms and estimation techniques – A review
Lucas, N., Bienaime, C., Belloy, C., Queneudec, M., Silvestre, F., & Nava-Saucedo, J.-E. (2008) · Chemosphere · doi:10.1016/j.chemosphere.2008.06.064 · Cited by 1,384
Polyurethanes: Versatile Materials and Sustainable Problem Solvers for Today’s Challenges
Engels, H., Pirkl, H., Albers, R., Albach, R. W., Krause, J., Hoffmann, A., Casselmann, H., & Dormish, J. (2013) · Angewandte Chemie International Edition · doi:10.1002/anie.201302766 · Cited by 1,234
The physical and chemical properties of eumelanin
Meredith, P., & Sarna, T. (2006) · Pigment Cell Research · doi:10.1111/j.1600-0749.2006.00345.x · Cited by 1,033
Polyurethanes from Vegetable Oils
Petrović, Z. S. (2008) · Polymer Reviews · doi:10.1080/15583720701834224 · Cited by 929
KROL, P. (2007) · Progress in Materials Science · doi:10.1016/j.pmatsci.2006.11.001 · Cited by 926
Mather, P. T., Luo, X., & Rousseau, I. A. (2009) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-082908-145419 · Cited by 911
Petrović, Z. S., & Ferguson, J. (1991) · Progress in Polymer Science · doi:10.1016/0079-6700(91)90011-9 · Cited by 895
Vegetable oil-based polymeric materials: synthesis, properties, and applications
Xia, Y., & Larock, R. C. (2010) · Green Chemistry · doi:10.1039/c0gc00264j · Cited by 864
Ju, K.-Y., Lee, Y., Lee, S., Park, S. B., & Lee, J.-K. (2011) · Biomacromolecules · doi:10.1021/bm101281b · Cited by 806
Comprehensive Organic Name Reactions and Reagents
Wang, Z. (2010) · Wiley eBooks · doi:10.1002/9780470638859 · Cited by 769
Bao, X., Zhao, J., Sun, J., Hu, M., & Yang, X. (2018) · ACS Nano · doi:10.1021/acsnano.8b04022 · Cited by 722
Santerre, J. P., Woodhouse, K., Laroche, G., & Labow, R. S. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2005.05.079 · Cited by 718
Biodegradation of polyurethane: a review
Howard, G. T. (2002) · International Biodeterioration & Biodegradation · doi:10.1016/s0964-8305(02)00051-3 · Cited by 711
Guan, J., Fujimoto, K. L., Sacks, M. S., & Wagner, W. R. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2004.10.018 · Cited by 703
95/04670 Carbon black science and technology
(1995) · Fuel and Energy Abstracts · doi:10.1016/0140-6701(95)96467-q · Cited by 650
Wilkes, R. A., & Aristilde, L. (2017) · Journal of Applied Microbiology · doi:10.1111/jam.13472 · Cited by 606
Synthetic biodegradable functional polymers for tissue engineering: a brief review
Guo, B., & Ma, P. X. (2014) · Science China Chemistry · doi:10.1007/s11426-014-5086-y · Cited by 592
Gardette, M., Perthue, A., Gardette, J.-L., Janecska, T., Földes, E., Pukánszky, B., & Therias, S. (2013) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2013.07.017 · Cited by 566
Elastomeric biomaterials for tissue engineering
Chen, Q., Liang, S., & Thouas, G. A. (2013) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2012.05.003 · Cited by 564
Review of electro-active shape-memory polymer composite
Liu, Y., Lv, H., Lan, X., Leng, J., & Du, S. (2009) · Composites Science and Technology · doi:10.1016/j.compscitech.2008.08.016 · Cited by 548
Zdrahala, R. J., & Zdrahala, I. J. (1999) · Journal of Biomaterials Applications · doi:10.1177/088532829901400104 · Cited by 540
A perspective approach to sustainable routes for non-isocyanate polyurethanes
Cornille, A., Auvergne, R., Figovsky, O., Boutevin, B., & Caillol, S. (2017) · European Polymer Journal · doi:10.1016/j.eurpolymj.2016.11.027 · Cited by 531
Characterization of polyurethane resins by FTIR, TGA, and XRD
Trovati, G., Sanches, E. A., Neto, S. C., Mascarenhas, Y. P., & Chierice, G. O. (2010) · Journal of Applied Polymer Science · doi:10.1002/app.31096 · Cited by 507
A literature survey on fatigue analysis approaches for rubber
MARS, W., & FATEMI, A. (2002) · International Journal of Fatigue · doi:10.1016/s0142-1123(02)00008-7 · Cited by 506
Yang, H., Zhu, S., & Pan, N. (2004) · Journal of Applied Polymer Science · doi:10.1002/app.20327 · Cited by 475
Polymer Photodegradation: Mechanisms and experimental methods
Rabek, J. F. (2012) · Cited by 455
González-Montelongo, R., Gloria Lobo, M., & González, M. (2010) · Food Chemistry · doi:10.1016/j.foodchem.2009.08.012 · Cited by 429
Sclafani, A., Palmisano, L., & Schiavello, M. (1990) · The Journal of Physical Chemistry · doi:10.1021/j100365a058 · Cited by 425
Non‐isocyanate polyurethanes: synthesis, properties, and applications
Rokicki, G., Parzuchowski, P. G., & Mazurek, M. (2015) · Polymers for Advanced Technologies · doi:10.1002/pat.3522 · Cited by 421
Onuki, Y., Bhardwaj, U., Papadimitrakopoulos, F., & Burgess, D. J. (2008) · Journal of Diabetes Science and Technology · doi:10.1177/193229680800200610 · Cited by 418
Non-isocyanate polyurethanes: from chemistry to applications
Kathalewar, M. S., Joshi, P. B., Sabnis, A. S., & Malshe, V. C. (2013) · RSC Advances · doi:10.1039/c2ra21938g · Cited by 414
Thermal degradation of segmented polyurethanes
Petrović, Z. S., Zavargo, Z., Flyn, J. H., & Macknight, W. J. (1994) · Journal of Applied Polymer Science · doi:10.1002/app.1994.070510615 · Cited by 404
Progress in Study of Non-Isocyanate Polyurethane
Guan, J., Song, Y., Lin, Y., Yin, X., Zuo, M., Zhao, Y., Tao, X., & Zheng, Q. (2011) · Industrial & Engineering Chemistry Research · doi:10.1021/ie101995j · Cited by 389
Thermo-moisture responsive polyurethane shape-memory polymer and composites: a review
Huang, W. M., Yang, B., Zhao, Y., & Ding, Z. (2010) · Journal of Materials Chemistry · doi:10.1039/b922943d · Cited by 382
Properties of polyether-polyurethane block copolymers: effects of hard segment length distribution
Miller, J. A., Lin, S. B., Hwang, K. K. S., Wu, K. S., Gibson, P. E., & Cooper, S. L. (1985) · Macromolecules · doi:10.1021/ma00143a005 · Cited by 374
Polyurethane Elastomer Biostability
Stokes, K., McVenes, R., & Anderson, J. M. (1995) · Journal of Biomaterials Applications · doi:10.1177/088532829500900402 · Cited by 366
Microtubular architecture of biodegradable polymer scaffolds
Ma, P. X., & Zhang, R. (2001) · Journal of Biomedical Materials Research · doi:10.1002/1097-4636(20010915)56:4<516::aid-jbm1123>3.0.co;2-b · Cited by 342
Stabilization of Polymeric Materials
Zweifel, H. (1998) · Springer eBooks · doi:10.1007/978-3-642-80305-5 · Cited by 333
Chapter 4 Mechanisms of inflammation and infection with implanted devices
Anderson, J. M. (1993) · Cardiovascular Pathology · doi:10.1016/1054-8807(93)90045-4 · Cited by 331
Bio-based polyurethane: An efficient and environment friendly coating systems: A review
Noreen, A., Zia, K. M., Zuber, M., Tabasum, S., & Zahoor, A. F. (2016) · Progress in Organic Coatings · doi:10.1016/j.porgcoat.2015.11.018 · Cited by 331
IR-change and yellowing of polyurethane as a result of UV irradiation
Rosu, D., Rosu, L., & Cascaval, C. N. (2009) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.01.013 · Cited by 320
Zhao, Q., Topham, N., Anderson, J. M., Hiltner, A., Lodoen, G., & Payet, C. R. (1991) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820250205 · Cited by 318
Guan, J., Sacks, M. S., Beckman, E. J., & Wagner, W. R. (2002) · Journal of Biomedical Materials Research · doi:10.1002/jbm.10204 · Cited by 317
Polymer degradation and stabilization
(1989) · Additives for Polymers · doi:10.1016/0306-3747(89)90115-2 · Cited by 309
Enhanced photocatalytic activity of TiO2 powder (P25) by hydrothermal treatment
Yu, J., Yu, H., Cheng, B., Zhou, M., & Zhao, X. (2006) · Journal of Molecular Catalysis A: Chemical · doi:10.1016/j.molcata.2006.03.021 · Cited by 304
The Stability, Electronic Structure, and Optical Property of TiO2 Polymorphs
Zhu, T., & Gao, S.-P. (2014) · The Journal of Physical Chemistry C · doi:10.1021/jp412462m · Cited by 281
Eceiza, A., Martin, M. D., de la Caba, K., Kortaberria, G., Gabilondo, N., Corcuera, M. A., & Mondragon, I. (2008) · Polymer Engineering & Science · doi:10.1002/pen.20905 · Cited by 279
Yeh, F., Hsiao, B. S., Sauer, B. B., Michel, S., & Siesler, H. W. (2003) · Macromolecules · doi:10.1021/ma0214456 · Cited by 278
Hydrogen-bonding properties of hard-segment model compounds in polyurethane block copolymers
Brunette, C. M., Hsu, S. L., & MacKnight, W. J. (1982) · Macromolecules · doi:10.1021/ma00229a014 · Cited by 277
A study on the photo-degradation of zinc oxide (ZnO) filled polypropylene nanocomposites
Zhao, H., & Li, R. K. Y. (2006) · Polymer · doi:10.1016/j.polymer.2006.02.089 · Cited by 270
Degradation of polymer blends: A brief review
La Mantia, F. P., Morreale, M., Botta, L., Mistretta, M. C., Ceraulo, M., & Scaffaro, R. (2017) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2017.07.011 · Cited by 268
Cregut, M., Bedas, M., Durand, M.-J., & Thouand, G. (2013) · Biotechnology Advances · doi:10.1016/j.biotechadv.2013.08.011 · Cited by 267
Tatai, L., Moore, T. G., Adhikari, R., Malherbe, F., Jayasekara, R., Griffiths, I., & Gunatillake, P. A. (2007) · Biomaterials · doi:10.1016/j.biomaterials.2007.08.035 · Cited by 267
Effect of particle size on the UV absorbance of zinc oxide nanoparticles
Goh, E. G., Xu, X., & McCormick, P. G. (2014) · Scripta Materialia · doi:10.1016/j.scriptamat.2014.01.033 · Cited by 265
Electroactive Polymers: Developments of and Perspectives for Dielectric Elastomers
Biggs, J., Danielmeier, K., Hitzbleck, J., Krause, J., Kridl, T., Nowak, S., Orselli, E., Quan, X., Schapeler, D., Sutherland, W., et al. (2013) · Angewandte Chemie International Edition · doi:10.1002/anie.201301918 · Cited by 264
Antioxidant activity of nanomaterials
Valgimigli, L., Baschieri, A., & Amorati, R. (2018) · Journal of Materials Chemistry B · doi:10.1039/c8tb00107c · Cited by 263
Wood plastic composites weathering: Visual appearance and chemical changes
Fabiyi, J. S., McDonald, A. G., Wolcott, M. P., & Griffiths, P. R. (2008) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2008.05.024 · Cited by 254
Pinchuk, L. (1995) · Journal of Biomaterials Science, Polymer Edition · doi:10.1163/156856294x00347 · Cited by 252
Guan, J., Sacks, M. S., Beckman, E. J., & Wagner, W. R. (2004) · Biomaterials · doi:10.1016/s0142-9612(03)00476-9 · Cited by 250
Accelerated aging for testing polymeric biomaterials and medical devices
Hukins, D. W. L., Mahomed, A., & Kukureka, S. N. (2008) · Medical Engineering & Physics · doi:10.1016/j.medengphy.2008.06.001 · Cited by 247
“Effect of nano-ZnO particles on the corrosion behavior of alkyd-based waterborne coatings”
Dhoke, S. K., Khanna, A. S., & Sinha, T. J. M. (2009) · Progress in Organic Coatings · doi:10.1016/j.porgcoat.2008.07.023 · Cited by 237
Polymer Degradation and Stabilization
Hawkins, W. L. (1984) · Polymers Properties and Applications · doi:10.1007/978-3-642-69376-2 · Cited by 235
Sterilization of implantable polymer-based medical devices: A review
Tipnis, N. P., & Burgess, D. J. (2018) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2017.12.003 · Cited by 233
Selected topics in biomedical polyurethanes. A review
Gogolewski, S. (1989) · Colloid & Polymer Science · doi:10.1007/bf01410115 · Cited by 230
Preparation and characterization of poly(styrene butylacrylate) latex/nano‐ZnO nanocomposites
Xiong, M., Gu, G., You, B., & Wu, L. (2003) · Journal of Applied Polymer Science · doi:10.1002/app.12869 · Cited by 228
Christenson, E. M., Anderson, J. M., & Hiltner, A. (2004) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.30067 · Cited by 219
Revising the mechanism of polymer autooxidation
Gryn'ova, G., Hodgson, J. L., & Coote, M. L. (2011) · Org. Biomol. Chem. · doi:10.1039/c0ob00596g · Cited by 217
Skarja, G. A., & Woodhouse, K. A. (2000) · Journal of Applied Polymer Science · doi:10.1002/(sici)1097-4628(20000321)75:12<1522::aid-app11>3.0.co;2-a · Cited by 216
Advances in Biomaterials Science and Biomedical Applications
(2013) · InTech eBooks · doi:10.5772/56420 · Cited by 216
Atmospheric and soil degradation of aliphatic–aromatic polyester films
Kijchavengkul, T., Auras, R., Rubino, M., Alvarado, E., Camacho Montero, J. R., & Rosales, J. M. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.11.048 · Cited by 209
Yeganeh, H., & Hojati-Talemi, P. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2006.10.011 · Cited by 209
Loh, X. J., Goh, S. H., & Li, J. (2007) · Biomaterials · doi:10.1016/j.biomaterials.2007.05.016 · Cited by 204
Gorna, K., & Gogolewski, S. (2003) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.10148 · Cited by 202
Photochemistry on TiO2: Mechanisms behind the surface chemistry
Yates, J. T. (2009) · Surface Science · doi:10.1016/j.susc.2008.11.052 · Cited by 202
Biomaterial-associated calcification: pathology, mechanisms, and strategies for prevention.
Schöen, F. J., Harasaki, H., Kim, K. M., Anderson, H. C., & Levy, R. J. (1988) · PubMed · Cited by 200
Usman, A., Zia, K. M., Zuber, M., Tabasum, S., Rehman, S., & Zia, F. (2016) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2016.02.004 · Cited by 198
New developments in polymer stabilization
Minagawa, M. (1989) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(89)81004-3 · Cited by 197
Enzyme-induced biodegradation of polycarbonate-polyurethanes: Dependence on hard-segment chemistry
Tang, Y. W., Labow, R. S., & Santerre, J. P. (2001) · Journal of Biomedical Materials Research · doi:10.1002/1097-4636(20011215)57:4<597::aid-jbm1207>3.0.co;2-t · Cited by 197
Ma, Z., Hong, Y., Nelson, D. M., Pichamuthu, J. E., Leeson, C. E., & Wagner, W. R. (2011) · Biomacromolecules · doi:10.1021/bm2007218 · Cited by 195
Funktionelle Gruppen an Festkörper‐Oberflächen
Boehm, H. ‐. (1966) · Angewandte Chemie · doi:10.1002/ange.19660781202 · Cited by 193
Biodegradation evaluation of polyether and polyester‐urethanes with oxidative and hydrolytic enzymes
Santerre, J. P., Labow, R. S., Duguay, D. G., Erfle, D., & Adams, G. A. (1994) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820281009 · Cited by 191
Barrioni, B. R., de Carvalho, S. M., Oréfice, R. L., de Oliveira, A. A. R., & Pereira, M. D. M. (2015) · Materials Science and Engineering: C · doi:10.1016/j.msec.2015.03.027 · Cited by 189
Simmons, A., Hyvarinen, J., Odell, R. A., Martin, D. J., Gunatillake, P. A., Noble, K. R., & Poole-Warren, L. A. (2004) · Biomaterials · doi:10.1016/j.biomaterials.2004.01.004 · Cited by 189
Hong, Y., Guan, J., Fujimoto, K. L., Hashizume, R., Pelinescu, A. L., & Wagner, W. R. (2010) · Biomaterials · doi:10.1016/j.biomaterials.2010.02.005 · Cited by 188
Kannan, R. Y., Salacinski, H. J., Odlyha, M., Butler, P. E., & Seifalian, A. M. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2005.10.006 · Cited by 187
Review on rubbers in medicine: natural, silicone and polyurethane rubbers
Rahimi, A., & Mashak, A. (2013) · Plastics, Rubber and Composites · doi:10.1179/1743289811y.0000000063 · Cited by 186
Poly(carbonate urethane) and poly(ether urethane) biodegradation: In vivo studies
Christenson, E. M., Dadsetan, M., Wiggins, M., Anderson, J. M., & Hiltner, A. (2004) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.30002 · Cited by 185
Alginate based polyurethanes: A review of recent advances and perspective
Zia, K. M., Zia, F., Zuber, M., Rehman, S., & Ahmad, M. N. (2015) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2015.04.076 · Cited by 184
Göçer, H., Akıncıoğlu, A., Öztaşkın, N., Göksu, S., & Gülçin, İ. (2013) · Archiv der Pharmazie · doi:10.1002/ardp.201300228 · Cited by 184
Hydrolytic degradation and functional stability of a segmented shape memory poly(ester urethane)
Pretsch, T., Jakob, I., & Müller, W. (2009) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2008.10.012 · Cited by 180
Mechanical characterisation of polyurethane elastomer for biomedical applications
Kanyanta, V., & Ivankovic, A. (2010) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2009.03.005 · Cited by 179
Skin Pigmentation‐Inspired Polydopamine Sunscreens
Wang, C., Wang, D., Dai, T., Xu, P., Wu, P., Zou, Y., Yang, P., Hu, J., Li, Y., & Cheng, Y. (2018) · Advanced Functional Materials · doi:10.1002/adfm.201802127 · Cited by 177
Polydimethylsiloxane/polyether-mixed macrodiol-based polyurethane elastomers: biostability
Martin, D. J., Poole Warren, L. A., Gunatillake, P. A., McCarthy, S. J., Meijs, G. F., & Schindhelm, K. (2000) · Biomaterials · doi:10.1016/s0142-9612(99)00271-9 · Cited by 176
Skarja, G. A., & Woodhouse, K. A. (1998) · Journal of Biomaterials Science, Polymer Edition · doi:10.1163/156856298x00659 · Cited by 173
Górna, K., & Gogolewski, S. (2002) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(01)00210-5 · Cited by 173
Liu, X., Hao, J., & Gaan, S. (2016) · RSC Advances · doi:10.1039/c6ra14345h · Cited by 173
Novel polycarbonate-based polyurethane elastomers: Composition–property relationship
Špírková, M., Pavličević, J., Strachota, A., Poreba, R., Bera, O., Kaprálková, L., Baldrian, J., Šlouf, M., Lazić, N., & Budinski-Simendić, J. (2011) · European Polymer Journal · doi:10.1016/j.eurpolymj.2011.01.001 · Cited by 172
Biodegradation of a polyurethane in vitro
Phua, S. K., Castillo, E., Anderson, J. M., & Hiltner, A. (1987) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820210207 · Cited by 172
Effects of crosslinking on thermal and mechanical properties of polyurethanes
Chiou, B., & Schoen, P. E. (2002) · Journal of Applied Polymer Science · doi:10.1002/app.10056 · Cited by 171
Properties of lignin–polyurethane films prepared by casting method
Ciobanu, C., Ungureanu, M. I., Ignat, M.-E., Ungureanu, D., & Popa, V. (2004) · Industrial Crops and Products · doi:10.1016/j.indcrop.2004.04.024 · Cited by 170
Fourier Transform Infrared Thermal Analysis of a Segmented Polyurethane
Senich, G. A., & MacKnight, W. J. (1980) · Macromolecules · doi:10.1021/ma60073a021 · Cited by 169
Hyperbranched polyurethane as novel solid–solid phase change material for thermal energy storage
Cao, Q., & Liu, P. (2006) · European Polymer Journal · doi:10.1016/j.eurpolymj.2006.07.020 · Cited by 167
Improvement of UV resistance of wood surfaces by using ZnO nanoparticles
Salla, J., Pandey, K. K., & Srinivas, K. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.01.013 · Cited by 167
Gao, Z., Peng, J., Zhong, T., Sun, J., Wang, X., & Yue, C. (2012) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2011.10.027 · Cited by 166
New insights into the microbial degradation of polyurethanes
Mahajan, N., & Gupta, P. K. (2015) · RSC Advances · doi:10.1039/c5ra04589d · Cited by 165
Accelerated ageing of polyurethanes for marine applications
Davies, P., & Evrard, G. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.05.016 · Cited by 163
Biodegradable Water-Based Polyurethane Shape Memory Elastomers for Bone Tissue Engineering
Wang, Y.-J., Jeng, U.-S., & Hsu, S.-H. (2018) · ACS Biomaterials Science & Engineering · doi:10.1021/acsbiomaterials.8b00091 · Cited by 163
Biodegradation mechanisms of polyurethane elastomers
Christenson, E. M., Anderson, J. M., & Hiltner, A. (2007) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1179/174327807x238909 · Cited by 161
Zhou, L., Yu, L., Ding, M., Li, J., Tan, H. S., Wang, Z., & Fu, Q. (2011) · Macromolecules · doi:10.1021/ma102346a · Cited by 161
Chen, J., Dong, R., Ge, J., Guo, B., & Ma, P. X. (2015) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.5b10829 · Cited by 160
Designing Biostable Polyurethane Elastomers for Biomedical Implants
Gunatillake, P. A., Martin, D. J., Meijs, G. F., McCarthy, S. J., & Adhikari, R. (2003) · Australian Journal of Chemistry · doi:10.1071/ch02168 · Cited by 159
Cellular interactions with biomaterials: In vivo cracking of pre‐stressed pellethane 2363‐80A
Zhao, Q., Agger, M. P., Fitzpatrick, M. N., Anderson, J. M., Hiltner, A., Stokes, K., & Urbanski, P. (1990) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820240508 · Cited by 158
Degradation studies on segmented polyurethanes prepared with HMDI, PCL and different chain extenders
Chan‐Chan, L. H., Solís-Correa, R. E., Vargas‐Coronado, R. F., Cervantes‐Uc, J. M., Cauich-Rodríguez, J. V., Quintana, P., & Bartolo-Pérez, P. (2009) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.12.010 · Cited by 158
Napper, I. E., & Thompson, R. C. (2023) · Annual Review of Environment and Resources · doi:10.1146/annurev-environ-112522-072642 · Cited by 158
Cristea, M. V., Riedl, B., & Blanchet, P. (2010) · Progress in Organic Coatings · doi:10.1016/j.porgcoat.2010.08.006 · Cited by 157
McCarthy, S. J., Meijs, G. F., Mitchell, N., Gunatillake, P. A., Heath, G., Brandwood, A., & Schindhelm, K. (1997) · Biomaterials · doi:10.1016/s0142-9612(97)00083-5 · Cited by 157
Synthesis and Characterization of a Biodegradable Thermoplastic Poly(ester−urethane) Elastomer
Kylmä, J., & Seppälä, J. V. (1997) · Macromolecules · doi:10.1021/ma961569g · Cited by 155
Górna, K., & Gogolewski, S. (2002) · Journal of Biomedical Materials Research · doi:10.1002/jbm.10100 · Cited by 154
Zhou, L., Liang, D., He, X., Li, J., Tan, H. S., Li, J., Fu, Q., & Gu, Q. (2012) · Biomaterials · doi:10.1016/j.biomaterials.2011.11.009 · Cited by 153
Tien, Y. I., & Wei, K. (2002) · Journal of Applied Polymer Science · doi:10.1002/app.11086 · Cited by 149
Roles of anatase and rutile TiO2 nanoparticles in photooxidation of polyurethane
Chen, X., Wang, Z., Liao, Z. F., Mai, Y. L., & Zhang, M. Q. (2006) · Polymer Testing · doi:10.1016/j.polymertesting.2006.10.002 · Cited by 149
Takahara, A., Coury, A. J., Hergenrother, R. W., & Cooper, S. L. (1991) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820250306 · Cited by 149
Bruin, P., Veenstra, G. J., Nijenhuis, A. J., & Pennings, A. J. (1988) · Die Makromolekulare Chemie, Rapid Communications · doi:10.1002/marc.1988.030090814 · Cited by 148
Degradation of Implant Materials
Eliaz, N. (2012) · Springer eBooks · doi:10.1007/978-1-4614-3942-4 · Cited by 146
Jiang, X., Li, J., Ding, M., Tan, H. S., Ling, Q., Zhong, Y., & Fu, Q. (2007) · European Polymer Journal · doi:10.1016/j.eurpolymj.2007.02.029 · Cited by 146
Gryn’ova, G., Ingold, K. U., & Coote, M. L. (2012) · Journal of the American Chemical Society · doi:10.1021/ja3006379 · Cited by 145
Wang, T.-L., & Hsieh, T. (1997) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(96)00130-9 · Cited by 145
Schimpf, V., Ritter, B. S., Weis, P., Parison, K., & Mülhaupt, R. (2017) · Macromolecules · doi:10.1021/acs.macromol.6b02460 · Cited by 141
Zhao, Q. H., McNally, A. K., Rubin, K. R., Renier, M., Wu, Y., Rose‐Caprara, V., Anderson, J. M., Hiltner, A., Urbanski, P., & Stokes, K. (1993) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820270311 · Cited by 140
Degradation of polyester polyurethane by Aspergillus sp. strain S45 isolated from soil
Osman, M., Satti, S. M., Luqman, A., Hasan, F., Shah, Z., & Shah, A. A. (2018) · Journal of Polymers and the Environment · doi:10.1007/s10924-017-0954-0 · Cited by 140
Enzymatic degradation of poly(ether urethane) and poly(carbonate urethane) by cholesterol esterase
Christenson, E. M., Patel, S. R., Anderson, J. M., & Hiltner, A. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2006.03.012 · Cited by 139
Martin, D. J., Meijs, G. F., Renwick, G. M., Gunatillake, P. A., & McCarthy, S. J. (1996) · Journal of Applied Polymer Science · doi:10.1002/(sici)1097-4628(19960425)60:4<557::aid-app9>3.0.co;2-n · Cited by 135
Doley, S., & Dolui, S. K. (2018) · European Polymer Journal · doi:10.1016/j.eurpolymj.2018.03.030 · Cited by 135
Small-angle X-Ray scattering from polyurethane elastomers
Clough, S. B., Schneider, N. S., & King, A. O. (1968) · Journal of Macromolecular Science Part B · doi:10.1080/00222346808212463 · Cited by 133
Clear castable polyurethane elastomer for fabrication of microfluidic devices
Domanský, K., Leslie, D. C., McKinney, J., Fraser, J. P., Sliz, J. D., Hamkins-Indik, T., Hamilton, G. A., Bahinski, A., & Ingber, D. E. (2013) · Lab on a Chip · doi:10.1039/c3lc50558h · Cited by 132
Elastomeric biodegradable polyurethane blends for soft tissue applications
Fromstein, J. D., & Woodhouse, K. A. (2002) · Journal of Biomaterials Science Polymer Edition · doi:10.1163/156856202320253929 · Cited by 132
Wilhelm, C., & Gardette, J. (1998) · Polymer · doi:10.1016/s0032-3861(97)10065-9 · Cited by 132
Chien, Y.-C., Chuang, W., Jeng, U., & Hsu, S.-H. (2017) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b11993 · Cited by 131
Studies on the photo-oxidative degradation of LDPE films in the presence of oxidised polyethylene
Roy, P. K., Surekha, P., Rajagopal, C., Chatterjee, S. N., & Choudhary, V. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.01.010 · Cited by 130
Beniah, G., Fortman, D. J., Heath, W. H., Dichtel, W. R., & Torkelson, J. M. (2017) · Macromolecules · doi:10.1021/acs.macromol.7b00765 · Cited by 130
Abraham, F., Alshuth, T., & Jerrams, S. (2004) · Materials & Design (1980-2015) · doi:10.1016/j.matdes.2004.02.020 · Cited by 129
Degradation of a poly(ether urethane urea) elastomer: infra-red and XPS studies
Marchant, R. E., Zhao, Q., Anderson, J. M., & Hiltner, A. (1987) · Polymer · doi:10.1016/0032-3861(87)90037-1 · Cited by 128
Thermooxidative Stabilization of Polymers Using Natural and Synthetic Melanins
Shanmuganathan, K., Cho, J. H., Iyer, P., Baranowitz, S. A., & Ellison, C. J. (2011) · Macromolecules · doi:10.1021/ma202170n · Cited by 127
Hydrolytic degradation of segmented polyurethane copolymers for biomedical applications
Mondal, S., & Martin, D. J. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.04.008 · Cited by 125
A new innovative stabilization method for the protection of natural wood
Hayoz, P., Peter, W., & Rogez, D. (2003) · Progress in Organic Coatings · doi:10.1016/s0300-9440(03)00102-4 · Cited by 124
Li, S., Xu, S., He, L., Xu, F., Wang, Y., & Zhang, L. (2010) · Polymer-Plastics Technology and Engineering · doi:10.1080/03602550903532166 · Cited by 123
Molecular engineering of chitin based polyurethane elastomers
Zia, K. M., Barikani, M., Zuber, M., Bhatti, I. A., & Sheikh, M. A. (2008) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2008.03.013 · Cited by 123
Fernando, S. S., Christensen, P. A., Egerton, T. A., & White, J. R. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.01.032 · Cited by 122
Decomposition behavior of polyurethanes via mathematical simulation
Chang, W. L. (1994) · Journal of Applied Polymer Science · doi:10.1002/app.1994.070531306 · Cited by 122
Polyurethane conductive blends and composites: synthesis and applications perspective
Thangavel, G., Rao, C. R. K., Narayan, R., & Raju, K. V. S. N. (2012) · Journal of Materials Science · doi:10.1007/s10853-012-6658-x · Cited by 121
An FTIR–ATR investigation of in vivo poly(ether urethane) degradation
Wu, Y., Sellitti, C., Anderson, J. M., Hiltner, A., Lodoen, G. A., & Payet, C. R. (1992) · Journal of Applied Polymer Science · doi:10.1002/app.1992.070460202 · Cited by 120
Oxidative biodegradation mechanisms of biaxially strained poly(etherurethane urea) elastomers
Schubert, M. A., Wiggins, M. J., Schaefer, M. P., Hiltner, A., & Anderson, J. M. (1995) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820290309 · Cited by 120
Role of oxygen in biodegradation of poly(etherurethane urea) elastomers
Schubert, M. A., Wiggins, M. J., Anderson, J. M., & Hiltner, A. (1997) · Journal of Biomedical Materials Research · Cited by 119
Thermoplastic Polyurethane Hydrolysis Stability
Schollenberger, C. S., & Stewart, F. D. (1971) · Journal of Elastomers & Plastics · doi:10.1177/009524437100300103 · Cited by 117
Bioinspired Polydopamine-Coated Hemoglobin as Potential Oxygen Carrier with Antioxidant Properties
Wang, Q., Zhang, R., Lu, M., You, G., Wang, Y., Chen, G., Zhao, C., Wang, Z., Song, X. R., Wu, Y. F., et al. (2017) · Biomacromolecules · doi:10.1021/acs.biomac.7b00077 · Cited by 117
Handbook of UV Degradation and Stabilization
Wypych, G. (2015) · Elsevier eBooks · doi:10.1016/c2014-0-01351-2 · Cited by 117
A damage model for the fatigue life of elastomeric materials
Wang, B., Lu, H., & Kim, G.-H. (2002) · Mechanics of Materials · doi:10.1016/s0167-6636(02)00175-8 · Cited by 116
Environmental stress cracking: A review
Robeson, L. M. (2012) · Polymer Engineering and Science · doi:10.1002/pen.23284 · Cited by 114
Polymer/carbon nanotube nanocomposites: Influence of carbon nanotubes on EVA photodegradation
Thérias, S., Fanton, E., Gardette, J., Peeterbroeck, S., Alexandre, M., & Dúbois, P. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.06.021 · Cited by 112
Effect of chemical structure on the biodegradation of polyurethanes under composting conditions
Kim, Y. D., & Kim, S. C. (1998) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(98)00017-2 · Cited by 111
Reinforcement of Elastomers by Particulate Fillers
Donnet, J., & Custodéro, E. (2013) · Elsevier eBooks · doi:10.1016/b978-0-12-394584-6.00008-x · Cited by 111
Degradation of polyurethanes in sea water
Rutkowska, M., Krasowska, K., Heimowska, A., Steinka, I., & Janik, H. (2002) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(02)00019-8 · Cited by 110
Hydrolytic degradation of poly(carbonate)-urethanes by monocyte-derived macrophages
Labow, R. S., Meek, E., & Santerre, J. P. (2001) · Biomaterials · doi:10.1016/s0142-9612(01)00049-7 · Cited by 108
Luo, X., Xiao, Y., Wu, Q., & Zeng, J. (2018) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2018.04.126 · Cited by 107
The in vivo auto-oxidation of polyether polyurethane by metal ions
Stokes, K., Urbanski, P., & UPTON, J. E. (1989) · Journal of Biomaterials Science Polymer Edition · doi:10.1163/156856290x00062 · Cited by 106
Autooxidative Degradation of Implanted Polyether Polyurethane Devices
Stokes, K., Coury, A. J., & Urbanski, P. (1986) · Journal of Biomaterials Applications · doi:10.1177/088532828600100302 · Cited by 106
Effect of silane modified nano ZnO on UV degradation of polyurethane coatings
Hằng, T. T. X., Dung, N. T., Trúc, T. A., Dương, N. T., Truoc, B. V., Vũ, P. G., Hoàng, T., Thanh, Đ. T. M., & Olivier, M. (2014) · Progress in Organic Coatings · doi:10.1016/j.porgcoat.2014.11.008 · Cited by 106
Soybean oil‐based polyurethane networks as candidate biomaterials: Synthesis and biocompatibility
Miao, S., Sun, L., Wang, P., Liu, R., Su, Z., & Zhang, S. (2012) · European Journal of Lipid Science and Technology · doi:10.1002/ejlt.201200050 · Cited by 103
Chemical and physical changes occurring in polyester polyurethane during biodegradation
Kay, M. J., McCabe, R. W., & Morton, L. H. G. (1993) · International Biodeterioration & Biodegradation · doi:10.1016/0964-8305(93)90006-n · Cited by 102
Solubility product of OH-carbonated hydroxyapatite
Ito, A., Maekawa, K., Tsutsumi, S., Ikazaki, F., & Tateishi, T. (1997) · Journal of Biomedical Materials Research · doi:10.1002/(sici)1097-4636(19970915)36:4<550::aid-jbm14>3.0.co;2-e · Cited by 101
Deka, H., Karak, N., Kalita, R. D., & Buragohain, A. K. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.06.017 · Cited by 101
Gac, P. L., Choqueuse, D., & Mélot, D. (2013) · Polymer Testing · doi:10.1016/j.polymertesting.2013.10.009 · Cited by 101
On the ozone protection of polymers having non-conjugated unsaturation
Cataldo, F. (2001) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(01)00017-9 · Cited by 99
Ng, W. S., Lee, C. S., Chuah, C. H., & Cheng, S. F. (2016) · Industrial Crops and Products · doi:10.1016/j.indcrop.2016.11.066 · Cited by 99
Horrocks, A. R., Mwila, J., Miraftab, M., Liu, M., & Chohan, S. (1999) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(98)00213-4 · Cited by 98
Schmidt, S., Gatti, F. J., Luitz, M., Ritter, B. S., Bruchmann, B., & Mülhaupt, R. (2017) · Macromolecules · doi:10.1021/acs.macromol.6b02787 · Cited by 95
Phua, S. L., Yang, L., Toh, C. L., Guoqiang, D., Lau, S. K., Dasari, A., & Lu, X. (2013) · ACS Applied Materials & Interfaces · doi:10.1021/am3024405 · Cited by 94
Simmons, A., Hyvarinen, J., & Poole-Warren, L. A. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2006.04.017 · Cited by 94
Effect of soft‐segment chemistry on polyurethane biostability during in vitro fatigue loading
Wiggins, M. J., MacEwan, M., Anderson, J. M., & Hiltner, A. (2004) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.20081 · Cited by 94
Low-Initial-Modulus Biodegradable Polyurethane Elastomers for Soft Tissue Regeneration
Xu, C., Huang, Y., Tang, L., & Hong, Y. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b15009 · Cited by 94
Wavelength sensitivity of unstabilized and UV stabilized polycarbonate to solar simulated radiation
Andrady, A. L., Searle, N. D., & Crewdson, L. (1992) · Polymer Degradation and Stability · doi:10.1016/0141-3910(92)90031-y · Cited by 93
Siddiquey, I. A., Furusawa, T., Sato, M., Honda, K., & Suzuki, N. (2007) · Dyes and Pigments · doi:10.1016/j.dyepig.2007.01.020 · Cited by 93
Santerre, J. P., & Labow, R. S. (1997) · Journal of Biomedical Materials Research · doi:10.1002/(sici)1097-4636(199708)36:2<223::aid-jbm11>3.0.co;2-h · Cited by 91
Takahara, A., Hergenrother, R. W., Coury, A. J., & Cooper, S. L. (1992) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820260609 · Cited by 91
Development of a new in vitro model for studying implantable polyurethane calcification
Golomb, G., & Wagner, D. K. (1991) · Biomaterials · doi:10.1016/0142-9612(91)90008-x · Cited by 91
Huang, Y.-J., Hung, K.-C., Hung, H.-S., & Hsu, S.-H. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b04718 · Cited by 89
Thermal stability of segmented polyurethanes
Ferguson, J. W., & Petrovìć, Z. S. (1976) · European Polymer Journal · doi:10.1016/0014-3057(76)90050-1 · Cited by 89
Enzyme–biomaterial interactions: Effect of biosystems on degradation of polyurethanes
Santerre, J. P., Labow, R. S., & Adams, G. A. (1993) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820270113 · Cited by 89
Hindered Amine Mechanisms: Part III—Investigations using isotopic labelling
Klemchuk, P. P., Gande, M. E., & Cordola, E. (1990) · Polymer Degradation and Stability · doi:10.1016/0141-3910(90)90097-q · Cited by 89
Synthesis and characterization of L ‐tyrosine based polyurethanes for biomaterial applications
Sarkar, D., Yang, J., Gupta, A. S., & Lopina, S. T. (2008) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.32095 · Cited by 88
Study of electroactive shape memory polyurethane–carbon nanotube hybrids
Lee, H.-F., & Yu, H. H. (2011) · Soft Matter · doi:10.1039/c0sm01101k · Cited by 88
Cited by
Design of biodegradable, implantable devices towards clinical translation
Li, C., Guo, C., Fitzpatrick, V., Ibrahim, A., Zwierstra, M. J., Hanna, P., Lechtig, A., Nazarian, A., Lin, S. J., & Kaplan, D. L. (2019) · Nature Reviews Materials · doi:10.1038/s41578-019-0150-z · Cited by 808
Stretchable Electronics Based on PDMS Substrates
Qi, D., Zhang, K., Tian, G., Jiang, B., & Huang, Y. (2021) · Advanced Materials · doi:10.1002/adma.202003155 · Cited by 663
Yao, Y., Xu, Z., Liu, B., Xiao, M., Yang, J., & Liu, W. (2021) · Advanced Functional Materials · doi:10.1002/adfm.202006944 · Cited by 335
Plastic pollutants: effective waste management for pollution control and abatement
Rajmohan, K. V. S., Ramya, C., Raja Viswanathan, M., & Varjani, S. (2019) · Current Opinion in Environmental Science & Health · doi:10.1016/j.coesh.2019.08.006 · Cited by 326
Thermochromic smart windows with highly regulated radiative cooling and solar transmission
Wang, S., Zhou, Y., Jiang, T., Yang, R., Tan, G., & Long, Y. (2021) · Nano Energy · doi:10.1016/j.nanoen.2021.106440 · Cited by 326
Metadata
- Authors
- Xie, F., Zhang, T., Bryant, P., Kurusingal, V., Colwell, J. M., & Laycock, B.
- Venue
- Progress in Polymer Science
- Publisher
- Elsevier BV
- Published
- 2019-03
- Volume
- 90
- Pages
- 211-268
- ISSN
- 0079-6700 (ISSN-L)
- OpenAlex
- W2906851405
- Cited by
- 722
- References
- 353
- FWCI
- 23.00
- Type
- journal article
- Language
- en
- Open access
- bronze
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.