The DOI matches its Crossref record; 429 of the 429 references it cites were found in a registry or an index.
Perfecting electrocatalysts via imperfections: towards the large-scale deployment of water electrolysis technology
Abstract
A tuned electronic structure favors the electrocatalytic water splitting reaction via accelerating the reaction kinetics, changing the rate-determining step, and optimizing the adsorption energy for intermediates; this is achieved via intentionally incorporating imperfections into the crystal lattices of electrocatalysts.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Double-slit photoelectron interference in strong-field ionization of the neon dimer
Kunitski, M., Eicke, N., Huber, P., Köhler, J., Zeller, S., Voigtsberger, J., Schlott, N., Henrichs, K., Sann, H., Trinter, F., et al. (2019) · Nature Communications · doi:10.1038/s41467-018-07882-8 · Cited by 8,162
Double-slit photoelectron interference in strong-field ionization of the neon dimer
Kunitski, M., Eicke, N., Huber, P., Köhler, J., Zeller, S., Voigtsberger, J., Schlott, N., Henrichs, K., Sann, H., Trinter, F., et al. (2019) · Institutional Repository of Leibniz Universität Hannover (Leibniz Universität Hannover) · doi:10.15488/5174 · Cited by 8,161
Structural absorption by barbule microstructures of super black bird of paradise feathers
McCoy, D. E., Feo, T., Harvey, T. A., & Prum, R. O. (2018) · Nature Communications · doi:10.1038/s41467-017-02088-w · Cited by 7,424
U1 snRNP regulates cancer cell migration and invasion in vitro
Oh, J.-M., Venters, C. C., Di, C., Pinto, A. M., Wan, L., Younis, I., Cai, Z., Arai, C., So, B. R., Duan, J., et al. (2020) · Nature Communications · doi:10.1038/s41467-019-13993-7 · Cited by 7,157
Electrocatalysis for the oxygen evolution reaction: recent development and future perspectives
Suen, N.-T., Hung, S.-F., Quan, Q., Zhang, N., Xu, Y.-J., & Chen, H. M. (2017) · Chemical Society Reviews · doi:10.1039/c6cs00328a · Cited by 6,307
Recent Advances in Electrocatalytic Hydrogen Evolution Using Nanoparticles
Zhu, J., Hu, L., Zhao, P., Lee, L. Y. S., & Wong, K.-Y. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00248 · Cited by 3,133
Efficient generation of mouse models of human diseases via ABE- and BE-mediated base editing
Liu, Z., Lu, Z., Yang, G., Huang, S., Li, G., Feng, S., Liu, Y., Li, J., Yu, W., Zhang, Y., et al. (2018) · Nature Communications · doi:10.1038/s41467-018-04768-7 · Cited by 2,074
Zhang, J., Zhao, Y., Guo, X., Chen, C., Dong, C.-L., Liu, R.-S., Han, C.-P., Li, Y., Gogotsi, Y., & Wang, G. (2018) · Nature Catalysis · doi:10.1038/s41929-018-0195-1 · Cited by 1,835
Self-citationSelf‐Supported Transition‐Metal‐Based Electrocatalysts for Hydrogen and Oxygen Evolution
Sun, H., Yan, Z., Liu, F., Xu, W., Cheng, F., & Chen, J. (2020) · Advanced Materials · doi:10.1002/adma.201806326 · Cited by 1,734
Hu, C., Zhang, L., & Gong, J. (2019) · Energy & Environmental Science · doi:10.1039/c9ee01202h · Cited by 1,690
Defect Chemistry of Nonprecious‐Metal Electrocatalysts for Oxygen Reactions
Yan, D., Li, Y., Huo, J., Chen, R., Dai, L., & Wang, S. (2017) · Advanced Materials · doi:10.1002/adma.201606459 · Cited by 1,600
Self-citationAtomic structure of sensitive battery materials and interfaces revealed by cryo–electron microscopy
Li, Y., Li, Y., Pei, A., Yan, K., Sun, Y., Wu, C.-L., Joubert, L.-M., Chin, R., Koh, A. L., Yu, Y., et al. (2017) · Science · doi:10.1126/science.aam6014 · Cited by 1,547
Zhuang, L., Ge, L., Yang, Y., Li, M., Jia, Y., Yao, X., & Zhu, Z. (2017) · Advanced Materials · doi:10.1002/adma.201606793 · Cited by 1,456
Xiao, Z., Huang, Y.-C., Dong, C.-L., Xie, C., Liu, Z., Du, S., Chen, W., Yan, D., Tao, L., Shu, Z., et al. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.0c00257 · Cited by 1,445
Self-citationChemical Synthesis of Single Atomic Site Catalysts
Ji, S., Chen, Y., Wang, X., Zhang, Z., Wang, D., & Li, Y. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00818 · Cited by 1,444
Zhang, J., Wang, T., Pohl, D., Rellinghaus, B., Dong, R., Liu, S., Zhuang, X., & Feng, X. (2016) · Angewandte Chemie International Edition · doi:10.1002/anie.201602237 · Cited by 1,412
Nanoarchitectonics for Transition‐Metal‐Sulfide‐Based Electrocatalysts for Water Splitting
Guo, Y., Park, T., Yi, J. W., Henzie, J., Kim, J., Wang, Z., Jiang, B., Bando, Y., Sugahara, Y., Tang, J., et al. (2019) · Advanced Materials · doi:10.1002/adma.201807134 · Cited by 1,402
Considerations for the scaling-up of water splitting catalysts
Kibsgaard, J., & Chorkendorff, I. (2019) · Nature Energy · doi:10.1038/s41560-019-0407-1 · Cited by 1,329
Direct Electrolytic Splitting of Seawater: Opportunities and Challenges
Dresp, S., Dionigi, F., Klingenhof, M., & Strasser, P. (2019) · ACS Energy Letters · doi:10.1021/acsenergylett.9b00220 · Cited by 1,272
Non‐Noble‐Metal‐Based Electrocatalysts toward the Oxygen Evolution Reaction
Wu, Z., Lu, X. F., Zang, S., & Lou, X. W. (. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201910274 · Cited by 1,230
Chandrasekaran, S., Yao, L., Deng, L., Bowen, C., Zhang, Y., Chen, S., Lin, Z., Peng, F., & Zhang, P. (2019) · Chemical Society Reviews · doi:10.1039/c8cs00664d · Cited by 1,199
Liu, D., Li, X., Chen, S., Yan, H., Wang, C., Wu, C., Haleem, Y. A., Duan, S., Lu, J., Ge, B., et al. (2019) · Nature Energy · doi:10.1038/s41560-019-0402-6 · Cited by 1,166
Burdyny, T., & Smith, W. A. (2019) · Energy & Environmental Science · doi:10.1039/c8ee03134g · Cited by 1,133
Chen, P., Zhou, T., Xing, L., Xu, K., Tong, Y., Xie, H., Zhang, L., Yan, W., Chu, W., Wu, C., et al. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201610119 · Cited by 1,085
Valsesia, A., Wang, Q.-P., Gheldof, N., Carayol, J., Ruffieux, H., Clark, T., Shenton, V., Oyston, L. J., Lefebvre, G., Metairon, S., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-08492-8 · Cited by 1,073
Xiao, Z., Wang, Y., Huang, Y.-C., Wei, Z., Dong, C.-L., Ma, J., Shen, S., Li, Y., & Wang, S. (2017) · Energy & Environmental Science · doi:10.1039/c7ee01917c · Cited by 1,063
Self-citationLi, Y., Sun, Y., Qin, Y., Zhang, W., Wang, L., Luo, M., Yang, H., & Guo, S. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201903120 · Cited by 1,054
Zhang, J., Liu, J., Xi, L., Yu, Y., Chen, N., Sun, S., Wang, W., Lange, K. M., & Zhang, B. (2018) · Journal of the American Chemical Society · doi:10.1021/jacs.8b00752 · Cited by 1,034
Jia, Y., Zhang, L., Gao, G., Chen, H., Wang, B., Zhou, J., Soo, M. T., Hong, M., Yan, X., Qian, G., et al. (2017) · Advanced Materials · doi:10.1002/adma.201700017 · Cited by 1,030
Zhao, S., Tan, C., He, C.-T., An, P., Xie, F., Jiang, S., Zhu, Y., Wu, K.-H., Zhang, B., Li, H., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-00709-1 · Cited by 1,028
Hannagan, R. T., Giannakakis, G., Flytzani-Stephanopoulos, M., & Sykes, E. C. H. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00078 · Cited by 1,017
Lattice-strained metal–organic-framework arrays for bifunctional oxygen electrocatalysis
Cheng, W., Zhao, X., Su, H., Tang, F., Che, W., Zhang, H., & Liu, Q. (2019) · Nature Energy · doi:10.1038/s41560-018-0308-8 · Cited by 1,016
Wang, Y., Zhang, Y., Liu, Z., Xie, C., Feng, S., Liu, D., Shao, M., & Wang, S. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201701477 · Cited by 1,005
Self-citationAdvanced Electrocatalysts with Single-Metal-Atom Active Sites
Wang, Y., Su, H., He, Y., Li, L., Zhu, S., Shen, H., Xie, P., Fu, X., Zhou, G., Feng, C., et al. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00594 · Cited by 1,005
Self-citationMoysiadou, A., Lee, S., Hsu, C.-S., Chen, H. M., & Hu, X. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.0c04867 · Cited by 987
Single-Atom Vacancy Defect to Trigger High-Efficiency Hydrogen Evolution of MoS2
Wang, X., Zhang, Y., Si, H., Zhang, Q., Wu, J., Gao, L., Wei, X., Sun, Y., Liao, Q., Zhang, Z., et al. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.9b12113 · Cited by 969
Chen, D., Chen, C., Baiyee, Z. M., Shao, Z., & Ciucci, F. (2015) · Chemical Reviews · doi:10.1021/acs.chemrev.5b00073 · Cited by 936
Chen, G., Wang, T., Zhang, J., Liu, P., Sun, H., Zhuang, X., Chen, M., & Feng, X. (2018) · Advanced Materials · doi:10.1002/adma.201706279 · Cited by 934
In Situ/Operando Electrocatalyst Characterization by X-ray Absorption Spectroscopy
Timoshenko, J., & Roldan Cuenya, B. (2021) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00396 · Cited by 931
Low, J., Dai, B., Tong, T., Jiang, C., & Yu, J. (2019) · Advanced Materials · doi:10.1002/adma.201802981 · Cited by 929
Support and Interface Effects in Water‐Splitting Electrocatalysts
Zhang, J., Zhang, Q., & Feng, X. (2019) · Advanced Materials · doi:10.1002/adma.201808167 · Cited by 916
MoS2 monolayer catalyst doped with isolated Co atoms for the hydrodeoxygenation reaction
Liu, G., Robertson, A. W., Li, M. M.-J., Kuo, W. C. H., Darby, M. T., Muhieddine, M. H., Lin, Y.-C., Suenaga, K., Stamatakis, M., Warner, J. H., et al. (2017) · Nature Chemistry · doi:10.1038/nchem.2740 · Cited by 914
Yang, Y., Yao, H., Yu, Z., Islam, S. M., He, H., Yuan, M., Yue, Y., Xu, K., Hao, W., Sun, G., et al. (2019) · Journal of the American Chemical Society · doi:10.1021/jacs.9b04492 · Cited by 911
Cao, L., Luo, Q., Liu, W., Lin, Y., Liu, X., Cao, Y., Zhang, W., Wu, Y., Yang, J., Yao, T., et al. (2018) · Nature Catalysis · doi:10.1038/s41929-018-0203-5 · Cited by 901
Energy system transformations for limiting end-of-century warming to below 1.5 °C
Rogelj, J., Luderer, G., Pietzcker, R. C., Kriegler, E., Schaeffer, M., Krey, V., & Riahi, K. (2015) · Nature Climate Change · doi:10.1038/nclimate2572 · Cited by 875
Cryo-STEM mapping of solid–liquid interfaces and dendrites in lithium-metal batteries
Zachman, M. J., Tu, Z., Choudhury, S., Archer, L. A., & Kourkoutis, L. F. (2018) · Nature · doi:10.1038/s41586-018-0397-3 · Cited by 823
Sultan, S., Tiwari, J. N., Singh, A. N., Zhumagali, S., Ha, M., Myung, C. W., Thangavel, P., & Kim, K. S. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201900624 · Cited by 815
Enhancing Electrocatalytic Water Splitting by Strain Engineering
You, B., Tang, M. T., Tsai, C., Abild‐Pedersen, F., Zheng, X., & Li, H. (2019) · Advanced Materials · doi:10.1002/adma.201807001 · Cited by 793
Recent Advances and Prospective in Ruthenium-Based Materials for Electrochemical Water Splitting
Yu, J., He, Q., Yang, G., Zhou, W., Shao, Z., & Ni, M. (2019) · ACS Catalysis · doi:10.1021/acscatal.9b02457 · Cited by 789
Graphene Defects Trap Atomic Ni Species for Hydrogen and Oxygen Evolution Reactions
Zhang, L., Jia, Y., Gao, G., Yan, X., Chen, N., Chen, J., Soo, M. T., Wood, B., Yang, D., Du, A., et al. (2018) · Chem · doi:10.1016/j.chempr.2017.12.005 · Cited by 778
Han, N., Yang, K. R., Lu, Z., Li, Y., Xu, W., Gao, T., Cai, Z., Zhang, Y., Batista, V. S., Liu, W., et al. (2018) · Nature Communications · doi:10.1038/s41467-018-03429-z · Cited by 766
Hydrogen Evolution and Oxidation: Mechanistic Studies and Material Advances
Tian, X., Zhao, P., & Sheng, W. (2019) · Advanced Materials · doi:10.1002/adma.201808066 · Cited by 751
Gao, Q., Zhang, W., Shi, Z., Yang, L., & Tang, Y. (2019) · Advanced Materials · doi:10.1002/adma.201802880 · Cited by 734
Zhong, C., Liu, B., Ding, J., Liu, X., Zhong, Y., Li, Y., Sun, C., Han, X., Deng, Y., Zhao, N., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0584-y · Cited by 724
Zhu, K., Zhu, X., & Yang, W. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201802923 · Cited by 721
Dinh, C.-T., Jain, A., de Arquer, F. P. G., De Luna, P., Li, J., Wang, N., Zheng, X., Cai, J., Gregory, B. Z., Voznyy, O., et al. (2018) · Nature Energy · doi:10.1038/s41560-018-0296-8 · Cited by 717
Liu, R., Wang, Y., Liu, D., Zou, Y., & Wang, S. (2017) · Advanced Materials · doi:10.1002/adma.201701546 · Cited by 696
Self-citationCao, L., Luo, Q., Chen, J., Wang, L., Lin, Y., Wang, H., Liu, X., Shen, X., Zhang, W., Liu, W., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-12886-z · Cited by 687
Amorphous Catalysts and Electrochemical Water Splitting: An Untold Story of Harmony
Anantharaj, S., & Noda, S. (2020) · Small · doi:10.1002/smll.201905779 · Cited by 681
Li, M., Duanmu, K., Wan, C., Cheng, T., Zhang, L., Dai, S., Chen, W., Zhao, Z., Li, P., Fei, H., et al. (2019) · Nature Catalysis · doi:10.1038/s41929-019-0279-6 · Cited by 679
Jiang, K., Liu, B., Luo, M., Ning, S., Peng, M., Zhao, Y., Lu, Y.-R., Chan, T.-S., de Groot, F. M. F., & Tan, Y. (2019) · Nature Communications · doi:10.1038/s41467-019-09765-y · Cited by 670
Self-citationZhang, H., Maijenburg, A. W., Li, X., Schweizer, S. L., & Wehrspohn, R. B. (2020) · Advanced Functional Materials · doi:10.1002/adfm.202003261 · Cited by 666
Zheng, X., Zhang, B., De Luna, P., Liang, Y., Comin, R., Voznyy, O., Han, L., García de Arquer, F. P., Liu, M., Dinh, C. T., et al. (2018) · Nature Chemistry · doi:10.1038/nchem.2886 · Cited by 657
Ultrahigh-Loading of Ir Single Atoms on NiO Matrix to Dramatically Enhance Oxygen Evolution Reaction
Wang, Q., Huang, X., Zhao, Z. L., Wang, M., Xiang, B., Li, J., Feng, Z., Xu, H., & Gu, M. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.9b12642 · Cited by 657
Wastewater treatment for carbon capture and utilization
Lu, L., Guest, J. S., Peters, C. A., Zhu, X., Rau, G. H., & Ren, Z. J. (2018) · Nature Sustainability · doi:10.1038/s41893-018-0187-9 · Cited by 653
3D Nitrogen‐Anion‐Decorated Nickel Sulfides for Highly Efficient Overall Water Splitting
Chen, P., Zhou, T., Zhang, M., Tong, Y., Zhong, C., Zhang, N., Zhang, L., Wu, C., & Xie, Y. (2017) · Advanced Materials · doi:10.1002/adma.201701584 · Cited by 643
Shan, J., Ling, T., Davey, K., Zheng, Y., & Qiao, S. (2019) · Advanced Materials · doi:10.1002/adma.201900510 · Cited by 642
Yan, H., Xie, Y., Wu, A., Cai, Z., Wang, L., Tian, C., Zhang, X., & Fu, H. (2019) · Advanced Materials · doi:10.1002/adma.201901174 · Cited by 640
Wang, X., Liu, J., Liu, Z., Wang, W., Luo, J., Han, X., Du, X., Qiao, S., & Yang, J. (2018) · Advanced Materials · doi:10.1002/adma.201800005 · Cited by 640
Se-Doping Activates FeOOH for Cost-Effective and Efficient Electrochemical Water Oxidation
Niu, S., Jiang, W.-J., Wei, Z., Tang, T., Ma, J., Hu, J.-S., & Wan, L.-J. (2019) · Journal of the American Chemical Society · doi:10.1021/jacs.9b01214 · Cited by 638
Luo, Z., Ouyang, Y., Zhang, H., Xiao, M., Ge, J., Jiang, Z., Wang, J., Tang, D., Cao, X., Liu, C., et al. (2018) · Nature Communications · doi:10.1038/s41467-018-04501-4 · Cited by 637
Luo, X., Ji, P., Wang, P., Cheng, R., Chen, D., Lin, C., Zhang, J., He, J., Shi, Z., Li, N., et al. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201903891 · Cited by 636
Zhang, G., Feng, Y.-S., Lu, W.-T., He, D., Wang, C.-Y., Li, Y.-K., Wang, X.-Y., & Cao, F.-F. (2018) · ACS Catalysis · doi:10.1021/acscatal.8b00413 · Cited by 633
Yang, G., Jiao, Y., Yan, H., Xie, Y., Wu, A., Dong, X., Guo, D., Tian, C., & Fu, H. (2020) · Advanced Materials · doi:10.1002/adma.202000455 · Cited by 633
Lu, B., Guo, L., Wu, F., Peng, Y., Lu, J. E., Smart, T. J., Wang, N., Finfrock, Y. Z., Morris, D., Zhang, P., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-08419-3 · Cited by 629
Li, L., Qin, Z., Ries, L., Hong, S., Michel, T., Yang, J., Salameh, C., Bechelany, M., Miele, P., Kaplan, D., et al. (2019) · ACS Nano · doi:10.1021/acsnano.9b01583 · Cited by 626
Duan, Y., Yu, Z., Hu, S., Zheng, X., Zhang, C., Ding, H., Hu, B., Fu, Q., Yu, Z., Zheng, X., et al. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201909939 · Cited by 625
Effect of interlayer anions on [NiFe]-LDH nanosheet water oxidation activity
Hunter, B. M., Hieringer, W., Winkler, J. R., Gray, H. B., & Müller, A. M. (2016) · Energy & Environmental Science · doi:10.1039/c6ee00377j · Cited by 616
Chen, W., Pei, J., He, C., Wan, J., Ren, H., Wang, Y., Dong, J., Wu, K., Cheong, W., Mao, J., et al. (2018) · Advanced Materials · doi:10.1002/adma.201800396 · Cited by 613
Direct human health risks of increased atmospheric carbon dioxide
Jacobson, T. A., Kler, J. S., Hernke, M. T., Braun, R. K., Meyer, K. C., & Funk, W. E. (2019) · Nature Sustainability · doi:10.1038/s41893-019-0323-1 · Cited by 609
Chen, J., Zheng, F., Zhang, S.-J., Fisher, A., Zhou, Y., Wang, Z., Li, Y., Xu, B.-B., Li, J.-T., & Sun, S.-G. (2018) · ACS Catalysis · doi:10.1021/acscatal.8b03489 · Cited by 608
CoP‐Doped MOF‐Based Electrocatalyst for pH‐Universal Hydrogen Evolution Reaction
Liu, T., Li, P., Yao, N., Cheng, G., Chen, S., Luo, W., & Yin, Y. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201901409 · Cited by 606
Zhang, J., & Dai, L. (2016) · Angewandte Chemie International Edition · doi:10.1002/anie.201607405 · Cited by 603
Zhang, L., Si, R., Liu, H., Chen, N., Wang, Q., Adair, K., Wang, Z., Chen, J., Song, Z., Li, J., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-12887-y · Cited by 600
Engineering Cobalt Defects in Cobalt Oxide for Highly Efficient Electrocatalytic Oxygen Evolution
Zhang, R., Zhang, Y.-C., Pan, L., Shen, G.-Q., Mahmood, N., Ma, Y.-H., Shi, Y., Jia, W., Wang, L., Zhang, X., et al. (2018) · ACS Catalysis · doi:10.1021/acscatal.8b01046 · Cited by 599
Yin, X., Wang, H., Tang, S., Lu, X., Shu, M., Si, R., & Lu, T. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201804817 · Cited by 594
Zou, X., Liu, Y., Li, G., Wu, Y., Liu, D., Li, W., Li, H., Wang, D., Zhang, Y., & Zou, X. (2017) · Advanced Materials · doi:10.1002/adma.201700404 · Cited by 589
A General Method to Probe Oxygen Evolution Intermediates at Operating Conditions
Tao, H. B., Xu, Y., Huang, X., Chen, J., Pei, L., Zhang, J., Chen, J. G., & Liu, B. (2019) · Joule · doi:10.1016/j.joule.2019.03.012 · Cited by 587
Fang, S., Zhu, X., Liu, X., Gu, J., Liu, W., Wang, D., Zhang, W., Lin, Y., Lu, J., Wei, S., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-14848-2 · Cited by 585
Pan, Y., Liu, S., Sun, K., Chen, X., Wang, B., Wu, K., Cao, X., Cheong, W., Shen, R., Han, A., et al. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201804349 · Cited by 584
Hu, F., Zhu, S., Chen, S., Li, Y., Ma, L., Wu, T., Zhang, Y., Wang, C., Liu, C., Yang, X., et al. (2017) · Advanced Materials · doi:10.1002/adma.201606570 · Cited by 576
Residual fossil CO2 emissions in 1.5–2 °C pathways
Luderer, G., Vrontisi, Z., Bertram, C., Edelenbosch, O. Y., Pietzcker, R. C., Rogelj, J., De Boer, H. S., Drouet, L., Emmerling, J., Fricko, O., et al. (2018) · Nature Climate Change · doi:10.1038/s41558-018-0198-6 · Cited by 575
Anantharaj, S., & Kundu, S. (2019) · ACS Energy Letters · doi:10.1021/acsenergylett.9b00686 · Cited by 565
Ye, S., Shi, Z., Feng, J., Tong, Y., & Li, G. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201712549 · Cited by 561
Wang, D., Li, Q., Han, C., Lu, Q., Xing, Z., & Yang, X. (2019) · Nature Communications · doi:10.1038/s41467-019-11765-x · Cited by 557
Qi, K., Cui, X., Gu, L., Yu, S., Fan, X., Luo, M., Xu, S., Li, N., Zheng, L., Zhang, Q., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-12997-7 · Cited by 554
Chai, G.-L., Qiu, K., Qiao, M., Titirici, M.-M., Shang, C., & Guo, Z. (2017) · Energy & Environmental Science · doi:10.1039/c6ee03446b · Cited by 544
Su, J., Ge, R., Jiang, K., Dong, Y., Hao, F., Tian, Z., Chen, G., & Chen, L. (2018) · Advanced Materials · doi:10.1002/adma.201801351 · Cited by 544
Ramalingam, V., Varadhan, P., Fu, H., Kim, H., Zhang, D., Chen, S., Song, L., Ma, D., Wang, Y., Alshareef, H. N., et al. (2019) · Advanced Materials · doi:10.1002/adma.201903841 · Cited by 536
Drivers of declining CO2 emissions in 18 developed economies
Le Quéré, C., Korsbakken, J. I., Wilson, C., Tosun, J., Andrew, R., Andres, R. J., Canadell, J. G., Jordan, A., Peters, G. P., & van Vuuren, D. P. (2019) · Nature Climate Change · doi:10.1038/s41558-019-0419-7 · Cited by 534
Ye, S., Luo, F., Zhang, Q., Zhang, P., Xu, T., Wang, Q., He, D., Guo, L., Zhang, Y., He, C., et al. (2019) · Energy & Environmental Science · doi:10.1039/c8ee02888e · Cited by 530
Tong, Y., Chen, P., Zhou, T., Xu, K., Chu, W., Wu, C., & Xie, Y. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201702430 · Cited by 523
Cai, P., Huang, J., Chen, J., & Wen, Z. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201701280 · Cited by 521
Chen, W., Pei, J., He, C., Wan, J., Ren, H., Zhu, Y., Wang, Y., Dong, J., Tian, S., Cheong, W., et al. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201710599 · Cited by 519
Huang, Y., Sun, Y., Zheng, X., Aoki, T., Pattengale, B., Huang, J., He, X., Bian, W., Younan, S., Williams, N., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-08877-9 · Cited by 519
Cobalt Covalent Doping in MoS2 to Induce Bifunctionality of Overall Water Splitting
Xiong, Q., Wang, Y., Liu, P., Zheng, L., Wang, G., Yang, H., Wong, P., Zhang, H., & Zhao, H. (2018) · Advanced Materials · doi:10.1002/adma.201801450 · Cited by 509
An, L., Feng, J., Zhang, Y., Wang, R., Liu, H., Wang, G., Cheng, F., & Xi, P. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201805298 · Cited by 506
Zhang, X., Zhao, Y., Zhao, Y., Shi, R., Waterhouse, G. I. N., & Zhang, T. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201900881 · Cited by 480
Self-citationWu, Y., Liu, X., Han, D., Song, X., Shi, L., Song, Y., Niu, S., Xie, Y., Cai, J., Wu, S., et al. (2018) · Nature Communications · doi:10.1038/s41467-018-03858-w · Cited by 477
Li, J., Liu, H.-X., Gou, W., Zhang, M., Xia, Z., Zhang, S., Chang, C.-R., Ma, Y., & Qu, Y. (2019) · Energy & Environmental Science · doi:10.1039/c9ee00752k · Cited by 473
Sun, Y., Xu, K., Wei, Z., Li, H., Zhang, T., Li, X., Cai, W., Ma, J., Fan, H. J., & Li, Y. (2018) · Advanced Materials · doi:10.1002/adma.201802121 · Cited by 473
In Situ/Operando Techniques for Characterization of Single-Atom Catalysts
Li, X., Yang, X., Zhang, J., Huang, Y., & Liu, B. (2019) · ACS Catalysis · doi:10.1021/acscatal.8b04937 · Cited by 471
Jia, J., Xiong, T., Zhao, L., Wang, F., Liu, H., Hu, R., Zhou, J., Zhou, W., & Chen, S. (2017) · ACS Nano · doi:10.1021/acsnano.7b06607 · Cited by 470
Heteroatom-doped transition metal electrocatalysts for hydrogen evolution reaction
Jin, H., Liu, X., Chen, S., Vasileff, A., Li, L., Jiao, Y., Song, L., Zheng, Y., & Qiao, S.-Z. (2019) · ACS Energy Letters · doi:10.1021/acsenergylett.9b00348 · Cited by 469
Zhu, Y., Chen, H.-C., Hsu, C.-S., Lin, T.-S., Chang, C.-J., Chang, S.-C., Tsai, L.-D., & Chen, H. M. (2019) · ACS Energy Letters · doi:10.1021/acsenergylett.9b00382 · Cited by 465
Metal Boride‐Based Catalysts for Electrochemical Water‐Splitting: A Review
Gupta, S., Patel, M. K., Miotello, A., & Patel, N. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201906481 · Cited by 464
Zheng, Y.-R., Wu, P., Gao, M.-R., Zhang, X.-L., Gao, F.-Y., Ju, H.-X., Wu, R., Gao, Q., You, R., Huang, W.-X., et al. (2018) · Nature Communications · doi:10.1038/s41467-018-04954-7 · Cited by 460
Huang, H., Yan, M., Yang, C., He, H., Jiang, Q., Yang, L., Lu, Z., Sun, Z., Xu, X., Bando, Y., et al. (2019) · Advanced Materials · doi:10.1002/adma.201903415 · Cited by 454
Metal Atom‐Doped Co 3 O 4 Hierarchical Nanoplates for Electrocatalytic Oxygen Evolution
Zhang, S. L., Guan, B. Y., Lu, X. F., Xi, S., Du, Y., & Lou, X. W. (. (2020) · Advanced Materials · doi:10.1002/adma.202002235 · Cited by 454
In Situ/Operando Studies for Designing Next-Generation Electrocatalysts
Zhu, Y., Wang, J., Chu, H., Chu, Y.-C., & Chen, H. M. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c00305 · Cited by 450
Huang, J., Li, Y., Zhang, Y., Rao, G., Wu, C., Hu, Y., Wang, X., Lu, R., Li, Y., & Xiong, J. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201910716 · Cited by 444
O-coordinated W-Mo dual-atom catalyst for pH-universal electrocatalytic hydrogen evolution
Yang, Y., Qian, Y., Li, H., Zhang, Z., Mu, Y., Do, D., Zhou, B., Dong, J., Yan, W., Qin, Y., et al. (2020) · Science Advances · doi:10.1126/sciadv.aba6586 · Cited by 442
Shan, X., Liu, J., Mu, H., Xiao, Y., Mei, B., Liu, W., Lin, G., Jiang, Z., Wen, L., & Jiang, L. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.201911617 · Cited by 437
Lu, X. F., Yu, L., Zhang, J., & Lou, X. W. (. (2019) · Advanced Materials · doi:10.1002/adma.201900699 · Cited by 435
Rational Design of Graphene‐Supported Single Atom Catalysts for Hydrogen Evolution Reaction
Hossain, M. D., Liu, Z., Zhuang, M., Yan, X., Xu, G., Gadre, C. A., Tyagi, A., Abidi, I. H., Sun, C., Wong, H., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803689 · Cited by 434
Single-Atom Catalysts for Electrochemical Water Splitting
Zhu, C., Shi, Q., Feng, S., Du, D., & Lin, Y. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b00640 · Cited by 430
Pető, J., Ollár, T., Vancsó, P., Popov, Z. I., Magda, G. Z., Dobrik, G., Hwang, C., Sorokin, P. B., & Tapasztó, L. (2018) · Nature Chemistry · doi:10.1038/s41557-018-0136-2 · Cited by 422
Cao, L., Hu, Y., Tang, S., Iljin, A., Wang, J., Zhang, Z., & Lu, T. (2018) · Advanced Science · doi:10.1002/advs.201800949 · Cited by 416
Huang, L., Chen, D., Luo, G., Lu, Y., Chen, C., Zou, Y., Dong, C., Li, Y., & Wang, S. (2019) · Advanced Materials · doi:10.1002/adma.201901439 · Cited by 414
Self-citationAnjum, M. A. R., Jeong, H. Y., Lee, M. H., Shin, H. S., & Lee, J. S. (2018) · Advanced Materials · doi:10.1002/adma.201707105 · Cited by 409
Preferential Cation Vacancies in Perovskite Hydroxide for the Oxygen Evolution Reaction
Chen, D., Qiao, M., Lu, Y., Hao, L., Liu, D., Dong, C., Li, Y., & Wang, S. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201805520 · Cited by 409
Self-citationXu, Q., Jiang, H., Zhang, H., Hu, Y., & Li, C. (2019) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2018.09.064 · Cited by 408
Li, M., Zhu, Y., Wang, H., Wang, C., Pinna, N., & Lu, X. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803185 · Cited by 406
Boundary activated hydrogen evolution reaction on monolayer MoS2
Zhu, J., Wang, Z.-C., Dai, H., Wang, Q., Yang, R., Yu, H., Liao, M., Zhang, J., Chen, W., Wei, Z., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-09269-9 · Cited by 406
Yang, L., Liu, R., & Jiao, L. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201909618 · Cited by 402
Operando Spectroscopic Analysis of an Amorphous Cobalt Sulfide Hydrogen Evolution Electrocatalyst
Kornienko, N., Resasco, J., Becknell, N., Jiang, C.-M., Liu, Y.-S., Nie, K., Sun, X., Guo, J., Leone, S. R., & Yang, P. (2015) · Journal of the American Chemical Society · doi:10.1021/jacs.5b03545 · Cited by 396
Environmental variability supports chimpanzee behavioural diversity
Kalan, A. K., Kulik, L., Arandjelovic, M., Boesch, C., Haas, F., Dieguez, P., Barratt, C. D., Abwe, E. E., Agbor, A., Angedakin, S., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-18176-3 · Cited by 396
Lin, Y., Sun, K., Liu, S., Chen, X., Cheng, Y., Cheong, W., Chen, Z., Zheng, L., Zhang, J., Li, X., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201901213 · Cited by 393
Boosting hydrogen evolution on MoS2 via co-confining selenium in surface and cobalt in inner layer
Zheng, Z., Yu, L., Gao, M., Chen, X., Zhou, W., Ma, C., Wu, L., Zhu, J., Meng, X., Hu, J., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-17199-0 · Cited by 393
Zhu, Y., Sokolowski, J., Song, X., He, Y., Mei, Y., & Wu, G. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201902844 · Cited by 392
He, Q., Tian, D., Jiang, H., Cao, D., Wei, S., Liu, D., Song, P., Lin, Y., & Song, L. (2020) · Advanced Materials · doi:10.1002/adma.201906972 · Cited by 388
Fan, H., Yu, H., Zhang, Y., Zheng, Y., Luo, Y., Dai, Z., Li, B., Zong, Y., & Yan, Q. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201706610 · Cited by 387
Liu, H., He, Q., Jiang, H., Lin, Y., Zhang, Y., Habib, M., Chen, S., & Song, L. (2017) · ACS Nano · doi:10.1021/acsnano.7b06501 · Cited by 385
Ruthenium‐Based Single‐Atom Alloy with High Electrocatalytic Activity for Hydrogen Evolution
Chen, C., Wu, D., Li, Z., Zhang, R., Kuai, C., Zhao, X., Dong, C., Qiao, S., Liu, H., & Du, X. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803913 · Cited by 384
Structural and Electronic Optimization of MoS 2 Edges for Hydrogen Evolution
Wang, H., Xiao, X., Liu, S., Chiang, C.-L., Kuai, X., Peng, C.-K., Lin, Y.-C., Meng, X., Zhao, J., Choi, J., et al. (2019) · Journal of the American Chemical Society · doi:10.1021/jacs.9b09932 · Cited by 383
Chen, G., Zhu, Y., Chen, H. M., Hu, Z., Hung, S., Ma, N., Dai, J., Lin, H., Chen, C., Zhou, W., et al. (2019) · Advanced Materials · doi:10.1002/adma.201900883 · Cited by 378
Zhang, Y., Wu, C., Jiang, H., Lin, Y., Liu, H., He, Q., Chen, S., Duan, T., & Song, L. (2018) · Advanced Materials · doi:10.1002/adma.201707522 · Cited by 377
Hui, L., Xue, Y., Huang, B., Yu, H., Zhang, C., Zhang, D., Jia, D., Zhao, Y., Li, Y., Liu, H., et al. (2018) · Nature Communications · doi:10.1038/s41467-018-07790-x · Cited by 377
Self-citationHan, X., Wu, X., Deng, Y., Liu, J., Lu, J., Zhong, C., & Hu, W. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201800935 · Cited by 375
Dai, L., Chen, Z., Li, L., Yin, P., Liu, Z., & Zhang, H. (2020) · Advanced Materials · doi:10.1002/adma.201906915 · Cited by 375
Bai, L., Lee, S., & Hu, X. (2021) · Angewandte Chemie International Edition · doi:10.1002/anie.202011388 · Cited by 373
FeS2/CoS2 Interface Nanosheets as Efficient Bifunctional Electrocatalyst for Overall Water Splitting
Li, Y., Yin, J., An, L., Lu, M., Sun, K., Zhao, Y., Gao, D., Cheng, F., & Xi, P. (2018) · Small · doi:10.1002/smll.201801070 · Cited by 365
Self-citationAsnavandi, M., Yin, Y., Li, Y., Sun, C., & Zhao, C. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b00696 · Cited by 365
Shin, H., Xiao, H., & Goddard, W. A. (2018) · Journal of the American Chemical Society · doi:10.1021/jacs.8b02225 · Cited by 364
Guo, C., Zheng, Y., Ran, J., Xie, F., Jaroniec, M., & Qiao, S. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201701531 · Cited by 363
Anantharaj, S., & Aravindan, V. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201902666 · Cited by 361
Shi, Q., Liu, Q., Ma, Y., Fang, Z., Liang, Z., Shao, G., Tang, B., Yang, W., Qin, L., & Fang, X. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201903854 · Cited by 361
Zheng, X., Han, X., Cao, Y., Zhang, Y., Nordlund, D., Wang, J., Chou, S., Liu, H., Li, L., Zhong, C., et al. (2020) · Advanced Materials · doi:10.1002/adma.202000607 · Cited by 354
Huang, X., Xu, X., Li, C., Wu, D., Cheng, D., & Cao, D. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803970 · Cited by 353
Zhang, J., Shang, X., Ren, H., Chi, J., Fu, H., Dong, B., Liu, C., & Chai, Y. (2019) · Advanced Materials · doi:10.1002/adma.201905107 · Cited by 352
Zou, X., Wu, Y., Liu, Y., Liu, D., Li, W., Gu, L., Liu, H., Wang, P., Sun, L., & Zhang, Y. (2018) · Chem · doi:10.1016/j.chempr.2018.02.023 · Cited by 351
Wu, Y., Tao, X., Qing, Y., Xu, H., Yang, F., Luo, S., Tian, C., Liu, M., & Lu, X. (2019) · Advanced Materials · doi:10.1002/adma.201900178 · Cited by 351
Capturing the active sites of multimetallic (oxy)hydroxides for the oxygen evolution reaction
Bo, X., Hocking, R. K., Zhou, S., Li, Y., Chen, X., Zhuang, J., Du, Y., & Zhao, C. (2020) · Energy & Environmental Science · doi:10.1039/d0ee01609h · Cited by 351
Sun, J., Lowe, S. E., Zhang, L., Wang, Y., Pang, K., Wang, Y., Zhong, Y., Liu, P., Zhao, K., Tang, Z., et al. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201811573 · Cited by 349
Zhou, G., Li, M., Li, Y., Dong, H., Sun, D., Liu, X., Xu, L., Tian, Z., & Tang, Y. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201905252 · Cited by 348
Wang, X., Vasileff, A., Jiao, Y., Zheng, Y., & Qiao, S. (2019) · Advanced Materials · doi:10.1002/adma.201803625 · Cited by 346
Cao, E., Chen, Z., Wu, H., Yu, P., Wang, Y., Xiao, F., Chen, S., Du, S., Xie, Y., Wu, Y., et al. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.201915254 · Cited by 337
Liu, Y., Ma, C., Zhang, Q., Wang, W., Pan, P., Gu, L., Xu, D., Bao, J., & Dai, Z. (2019) · Advanced Materials · doi:10.1002/adma.201900062 · Cited by 330
Lai, W., Zhang, L., Hua, W., Indris, S., Yan, Z., Hu, Z., Zhang, B., Liu, Y., Wang, L., Liu, M., et al. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201904614 · Cited by 330
Favaro, M., Yang, J., Nappini, S., Magnano, E., Toma, F. M., Crumlin, E. J., Yano, J., & Sharp, I. D. (2017) · Journal of the American Chemical Society · doi:10.1021/jacs.7b03211 · Cited by 323
Sun, H., Min, Y., Yang, W., Lian, Y., Lin, L., Feng, K., Deng, Z., Chen, M., Zhong, J., Xu, L., et al. (2019) · ACS Catalysis · doi:10.1021/acscatal.9b02264 · Cited by 323
Tiwari, J. N., Harzandi, A. M., Ha, M., Sultan, S., Myung, C. W., Park, H. J., Kim, D. Y., Thangavel, P., Singh, A. N., Sharma, P., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201900931 · Cited by 322
Yuan, Z., Li, J., Yang, M., Fang, Z., Jian, J., Yu, D., Chen, X., & Dai, L. (2019) · Journal of the American Chemical Society · doi:10.1021/jacs.9b00154 · Cited by 309
Cai, J., Song, Y., Zang, Y., Niu, S., Wu, Y., Xie, Y., Zheng, X., Liu, Y., Lin, Y., Liu, X., et al. (2020) · Science Advances · doi:10.1126/sciadv.aaw8113 · Cited by 309
Shang, H., Sun, W., Sui, R., Pei, J., Zheng, L., Dong, J., Jiang, Z., Zhou, D., Zhuang, Z., Chen, W., et al. (2020) · Nano Letters · doi:10.1021/acs.nanolett.0c01925 · Cited by 309
Chao, T., Luo, X., Chen, W., Jiang, B., Ge, J., Lin, Y., Wu, G., Wang, X., Hu, Y., Zhuang, Z., et al. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201709803 · Cited by 308
Liu, B., Wang, Y., Peng, H., Yang, R., Jiang, Z., Zhou, X., Lee, C., Zhao, H., & Zhang, W. (2018) · Advanced Materials · doi:10.1002/adma.201803144 · Cited by 308
Nickel Vacancies Boost Reconstruction in Nickel Hydroxide Electrocatalyst
He, Q., Wan, Y., Jiang, H., Pan, Z., Wu, C., Wang, M., Wu, X., Ye, B., Ajayan, P. M., & Song, L. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b00515 · Cited by 306
Wu, X., Zhou, S., Wang, Z., Liu, J., Pei, W., Yang, P., Zhao, J., & Qiu, J. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201901333 · Cited by 302
Wang, C., & Qi, L. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.202005436 · Cited by 302
Ultrathin two-dimensional materials for photo- and electrocatalytic hydrogen evolution
Di, J., Yan, C., Handoko, A. D., Seh, Z. W., Li, H., & Liu, Z. (2018) · Materials Today · doi:10.1016/j.mattod.2018.01.034 · Cited by 300
Liu, T., Li, P., Yao, N., Kong, T., Cheng, G., Chen, S., & Luo, W. (2019) · Advanced Materials · doi:10.1002/adma.201806672 · Cited by 300
Activation of MoS2 Basal Planes for Hydrogen Evolution by Zinc
Wu, W., Niu, C., Wei, C., Jia, Y., Li, C., & Xu, Q. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201812475 · Cited by 297
Robust and Stable Acidic Overall Water Splitting on Ir Single Atoms
Luo, F., Hu, H., Zhao, X., Yang, Z., Zhang, Q., Xu, J., Kaneko, T., Yoshida, Y., Zhu, C., & Cai, W. (2020) · Nano Letters · doi:10.1021/acs.nanolett.0c00127 · Cited by 297
Xu, K., Cheng, H., Lv, H., Wang, J., Liu, L., Liu, S., Wu, X., Chu, W., Wu, C., & Xie, Y. (2018) · Advanced Materials · doi:10.1002/adma.201703322 · Cited by 292
Accelerated Hydrogen Evolution Reaction in CoS2 by Transition-Metal Doping
Zhang, J., Liu, Y., Sun, C., Xi, P., Peng, S., Gao, D., & Xue, D. (2018) · ACS Energy Letters · doi:10.1021/acsenergylett.8b00066 · Cited by 292
Optimized Metal Chalcogenides for Boosting Water Splitting
Yin, J., Jin, J., Lin, H., Yin, Z., Li, J., Lu, M., Guo, L., Xi, P., Tang, Y., & Yan, C. (2020) · Advanced Science · doi:10.1002/advs.201903070 · Cited by 292
The Comprehensive Understanding of as an Evaluation Parameter for Electrochemical Water Splitting
Wei, C., & Xu, Z. J. (2018) · Small Methods · doi:10.1002/smtd.201800168 · Cited by 290
Chen, J., Liu, G., Zhu, Y.-Z., Su, M., Yin, P., Wu, X.-J., Lu, Q., Tan, C., Zhao, M., Liu, Z., et al. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.0c01649 · Cited by 289
Fe‐Ni‐Mo Nitride Porous Nanotubes for Full Water Splitting and Zn‐Air Batteries
Zhu, C., Yin, Z., Lai, W., Sun, Y., Liu, L., Zhang, X., Chen, Y., & Chou, S. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201802327 · Cited by 288
Liu, Y., Xiao, C., Huang, P., Cheng, M., & Xie, Y. (2018) · Chem · doi:10.1016/j.chempr.2018.02.006 · Cited by 282
Yao, N., Li, P., Zhou, Z., Zhao, Y., Cheng, G., Chen, S., & Luo, W. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201902449 · Cited by 280
Self-citationCarbon doping switching on the hydrogen adsorption activity of NiO for hydrogen evolution reaction
Kou, T., Chen, M., Wu, F., Smart, T. J., Wang, S., Wu, Y., Zhang, Y., Li, S., Lall, S., Zhang, Z., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-14462-2 · Cited by 280
Self-citationHighly efficient hydrogen evolution triggered by a multi-interfacial Ni/WC hybrid electrocatalyst
Ma, Y.-Y., Lang, Z.-L., Yan, L.-K., Wang, Y.-H., Tan, H.-Q., Feng, K., Xia, Y.-J., Zhong, J., Liu, Y., Kang, Z.-H., et al. (2018) · Energy & Environmental Science · doi:10.1039/c8ee01129j · Cited by 279
Wu, Y., Li, F., Chen, W., Xiang, Q., Ma, Y., Zhu, H., Tao, P., Song, C., Shang, W., Deng, T., et al. (2018) · Advanced Materials · doi:10.1002/adma.201803151 · Cited by 276
Jayaramulu, K., Masa, J., Tomanec, O., Peeters, D., Ranc, V., Schneemann, A., Zboril, R., Schuhmann, W., & Fischer, R. A. (2017) · Advanced Functional Materials · doi:10.1002/adfm.201700451 · Cited by 271
Qin, Q., Jang, H., Li, P., Yuan, B., Liu, X., & Cho, J. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803312 · Cited by 269
Phosphorus Vacancies that Boost Electrocatalytic Hydrogen Evolution by Two Orders of Magnitude
Duan, J., Chen, S., Ortíz‐Ledón, C. A., Jaroniec, M., & Qiao, S. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.201914967 · Cited by 268
He, T., Matta, S. K., Will, G., & Du, A. (2019) · Small Methods · doi:10.1002/smtd.201800419 · Cited by 267
Engineering grain boundaries at the 2D limit for the hydrogen evolution reaction
He, Y., Tang, P., Hu, Z., He, Q., Zhu, C., Wang, L., Zeng, Q., Golani, P., Gao, G., Fu, W., et al. (2020) · Nature Communications · doi:10.1038/s41467-019-13631-2 · Cited by 267
Cited by
Descriptors for the Evaluation of Electrocatalytic Reactions: d‐Band Theory and Beyond
Jiao, S., Fu, X., & Huang, H. (2022) · Advanced Functional Materials · doi:10.1002/adfm.202107651 · Cited by 719
Self-citationRecent advances in proton exchange membrane water electrolysis
Liu, R.-T., Xu, Z.-L., Li, F.-M., Chen, F.-Y., Yu, J.-Y., Yan, Y., Chen, Y., & Xia, B. Y. (2023) · Chemical Society Reviews · doi:10.1039/d2cs00681b · Cited by 701
Sun, H., Xu, X., Kim, H., Jung, W., Zhou, W., & Shao, Z. (2023) · ENERGY & ENVIRONMENTAL MATERIALS · doi:10.1002/eem2.12441 · Cited by 601
Anantharaj, S., Noda, S., Driess, M., & Menezes, P. W. (2021) · ACS Energy Letters · doi:10.1021/acsenergylett.1c00608 · Cited by 597
Stability of electrocatalytic OER: from principle to application
Li, H., Lin, Y., Duan, J., Wen, Q., Liu, Y., & Zhai, T. (2024) · Chemical Society Reviews · doi:10.1039/d3cs00010a · Cited by 540
Metadata
- Authors
- Jiao, S., Fu, X., Wang, S., & Zhao, Y.
- Venue
- Energy & Environmental Science
- Publisher
- Royal Society of Chemistry (RSC)
- Published
- 2021
- Volume
- 14
- Issue
- 4
- Pages
- 1722-1770
- ISSN
- 1754-5692 (ISSN-L)
- 1754-5706
- OpenAlex
- W3135581272
- Cited by
- 399
- References
- 429
- FWCI
- 12.30
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.