Abstract

Oxide materials represent a versatile and fundamental platform for photonics, allowing the manipulation of light through optical property engineering. This review focuses mainly on the physics and applications of simple oxides, analysing their use in the realisation of dielectric mirrors, in particular of distributed Bragg reflectors, and planar microcavities. Critical aspects regarding the design of multilayer structures, the control of optical confinement and the improvement of the quality factor in passive devices are discussed. However, to provide a complete picture of the evolution of the field, the section dedicated to oxide materials anticipates future directions dominated by complex oxides such as lithium niobate, lithium tantalate and barium titanate required for active photonics. In this context, a necessary technological paradigm shift is highlighted: the transition from the current use of film-on-insulator platforms to the direct epitaxial growth of these functional materials, an essential step for the scalability and monolithic integration of future photonic devices.

Verified 2026-10-08 · 5 references not checked yet

Overview

CoChat Summary

TL;DR

This review surveys metal-oxide thin films for advanced photonics, focusing on dielectric mirrors, distributed Bragg reflectors (DBRs), and planar microcavities, while also previewing complex oxides for active photonics. It argues that material pair, deposition technique, and architecture govern mirror reflectivity and cavity quality factor, and that future scalability requires a shift toward direct epitaxial growth.

Key findings

  • DBR performance depends strongly on optical contrast and pair number: examples include SiO₂/ZrO₂ with R ≥ 95% at 366 nm and PBG 82 nm for an eight-pair structure; SiO₂/Al₂O₃ with R ≥ 97% at 290 nm; Al₂O₃/ZrO₂ with R = 99.8% at 377 nm for a 12.5-pair structure; Al₂O₃/YSZ with R = 99.7% for 10-period bilayer films; Al₂O₃/TiO₂ with R = 98.1% at 471 nm and PBG 79 nm for six-period bilayer films; and SiO₂/TiO₂ with 99.99% and tuneable PBG from visible to NIR via sol-gel spin coating.
  • Refractive indices vary by deposition method: SiO₂ shows n = 1.46–1.52 at 633 nm by PLD, 1.41–1.52 by RF magnetron sputtering, and 1.43–1.49 by e-beam evaporation; TiO₂ shows n = 2.6 at 550 nm by PLD, 2.57–2.74 by RF magnetron sputtering, and 2.06–2.08 by e-beam evaporation.
  • Planar microcavity quality factors in Table 8 range widely, e.g., SiO₂/HfO₂/Al with ZnO active layer Q = 4250; SiO₂/HfO₂ with HfO₂ Q = 3700; Al₂O₃/YSZ with ZnO Q = 1000; SiO₂/Ta₂O₅ with organics Q = 1000; SiO₂/TiO₂ with Er³⁺-doped SiO₂ Q = 890; and SiO₂/TiO₂ with TiO₂ Q = 35.
  • Complex oxides are highlighted for active photonics: LiNbO₃ has r₃₃ = 30.9 pm/V, d₃₃ = 27 pm/V, n ≈ 2.2 ordinary and 2.1 extraordinary, and transparency from 0.4 to 5.5 µm; LiTaO₃ has r₃₃ = 30.5 pm/V and bandgap 3.93 eV; BaTiO₃ has a Pockels coefficient larger than 1000 pm/V and transparency from 460 to 6300 nm.

Methods

  • This is a review article; the Data Availability Statement says “No new data were created or analysed in this study.”
  • It synthesizes literature on oxide thin-film processing, dielectric mirrors/DBRs, and planar optical microcavities, with tables comparing material pairs, refractive indices, deposition processes, and microcavity Q factors.
  • The main analysis is qualitative and comparative, discussing PVD, CVD, and solution-based routes, and linking deposition method to film density, refractive index, stress, optical losses, and device performance.

Limitations

  • The paper states that planar Fabry–Pérot cavities generally offer less spatial confinement (larger V_eff) and more modest temporal confinement (lower Q) than whispering gallery resonators and complex photonic structures, and that their architecture limits confinement effects.
  • It states that large-scale deposition studies are scarce because of challenges in obtaining uniform films on large surfaces, stress-induced defects, time and manufacturing cost, and difficult metrology on large surfaces.
  • Evident from the text: as a review, it provides no original experimental validation, and it notes method-specific drawbacks such as solution-based poor interface quality and porosity, CVD high temperatures, PVD higher cost, and MBE infrastructure/high-vacuum requirements with lower growth rates.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.3390/cryst16030164

Cites

301 of 306 references verified0 citation errors · 0 not checkable

Statistics

Nothing to recompute.

Verification

Claims the paper makes

29 Valid · 8 Not valid · 42 Not checked · 29 Own results and interpretations

27 more claims · 3 with their cited sources checked

Create a free account to see all 108 claims and every source verdict.

See all claims — free account
  • It may state two separate claims as one. 55
  • Probably not a substantial claim. 35
  • Borderline: one of the tests for a substantial claim is unclear. 1
  • The quote only partly states this claim. 2

Create a free account to see these claims.

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

Each contradiction between two passages listed here was confirmed by an independent check.

3 of 3

Cited works that were retracted

Works this paper cites that were later retracted, from the retraction notices publishers deposit. Major when the notice came out before this paper was published.

1 of 1

Citations

Cites

1 retracted

Metadata

Authors
Stîngescu, M.-L., Șopronyi, M.-A., Antohe, Ș., & Scărișoreanu, N.-D.
Affiliations
  • University of Bucharest (RO)
  • National Institute for Laser, Plasma and Radiation Physics (INFLPR), Atomiștilor Street 409, 077125 Măgurele, Romania
  • R&D Center for Materials and Electronic & Optoelectronic Devices (MDEO), Faculty of Physics, University of Bucharest, Atomiștilor Street 405, 077125 Măgurele, Romania
Venue
Crystals
Publisher
MDPI AG
Published
2026-02-27
Volume
16
Issue
3
Pages
164
ISSN
2073-4352 (ISSN-L)
OpenAlex
W7131786704
Cited by
2
References
295
Citations by year
2026: 2
FWCI
2.74
Type
journal article
Language
en
Open access
Locations
  • Crystals (publishedVersion, cc-by)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
Funders
Ministerul Cercetării și Inovării (Cod SMIS 351364, Contract nr. G 2024-85828/390008/27.11.2024, Program LAPLAS VII – contract no. 30N/2023.)
Topics
  • Physical Sciences › Materials Science › Surfaces, Coatings and Films › Optical Coatings and Gratings
  • Physical Sciences › Physics and Astronomy › Atomic and Molecular Physics, and Optics › Photorefractive and Nonlinear Optics
  • Physical Sciences › Materials Science › Materials Chemistry › Electronic and Structural Properties of Oxides
Keywords
metal oxide thin films, dielectric mirrors, distributed Bragg reflector, planar microcavities, light confinement, quality factor, passive optical components, complex oxides, lithium niobate, lithium tantalate, barium titanate, epitaxial growth, monolithic integration

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

The claim verdicts this report counts are experimental: their accuracy is not yet measured.

A language model drew the claims from the paper on 2026-10-08, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).

A second model labelled each claim on 2026-10-08 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Cited sources are checked with a language model’s help (gpt-6-sol).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.